JPH0582355B2 - - Google Patents
Info
- Publication number
- JPH0582355B2 JPH0582355B2 JP3777588A JP3777588A JPH0582355B2 JP H0582355 B2 JPH0582355 B2 JP H0582355B2 JP 3777588 A JP3777588 A JP 3777588A JP 3777588 A JP3777588 A JP 3777588A JP H0582355 B2 JPH0582355 B2 JP H0582355B2
- Authority
- JP
- Japan
- Prior art keywords
- oxygen concentration
- crucible
- crystal
- layer
- single crystal
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Landscapes
- Crystals, And After-Treatments Of Crystals (AREA)
- Liquid Deposition Of Substances Of Which Semiconductor Devices Are Composed (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP3777588A JPH01212292A (ja) | 1988-02-19 | 1988-02-19 | 結晶成長方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP3777588A JPH01212292A (ja) | 1988-02-19 | 1988-02-19 | 結晶成長方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPH01212292A JPH01212292A (ja) | 1989-08-25 |
| JPH0582355B2 true JPH0582355B2 (enEXAMPLES) | 1993-11-18 |
Family
ID=12506858
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP3777588A Granted JPH01212292A (ja) | 1988-02-19 | 1988-02-19 | 結晶成長方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPH01212292A (enEXAMPLES) |
-
1988
- 1988-02-19 JP JP3777588A patent/JPH01212292A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPH01212292A (ja) | 1989-08-25 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| KR930003044B1 (ko) | 실리콘 단결정의 제조방법 및 장치 | |
| JPH01215788A (ja) | 結晶引上げ方法 | |
| JP2813592B2 (ja) | 単結晶製造方法 | |
| JPH07267776A (ja) | 結晶成長方法 | |
| JPH0379320B2 (enEXAMPLES) | ||
| JPH0582355B2 (enEXAMPLES) | ||
| JP2640315B2 (ja) | シリコン単結晶の製造方法 | |
| JPH0524969A (ja) | 結晶成長装置 | |
| JPH034517B2 (enEXAMPLES) | ||
| JP2550740B2 (ja) | 結晶成長装置 | |
| JPH07277875A (ja) | 結晶成長方法 | |
| JPS61261288A (ja) | シリコン単結晶引上装置 | |
| JPH037405Y2 (enEXAMPLES) | ||
| JPH01197392A (ja) | 結晶成長方法 | |
| JPH0769778A (ja) | 単結晶成長装置 | |
| JPH09255475A (ja) | 単結晶成長装置 | |
| JP3011085B2 (ja) | 単結晶の成長方法 | |
| JPH0259494A (ja) | シリコン単結晶の製造方法及び装置 | |
| JP2539336Y2 (ja) | 結晶成長装置 | |
| JPH02172885A (ja) | シリコン単結晶の製造方法 | |
| JPH09208360A (ja) | 単結晶の成長方法 | |
| JPH08259371A (ja) | Srの均一化に優れる単結晶成長方法 | |
| JPH07267775A (ja) | 単結晶引上げ方法 | |
| JPH09315892A (ja) | 単結晶成長方法 | |
| JPH101394A (ja) | アンチモン添加シリコン単結晶の成長方法 |