JPH0572685B2 - - Google Patents
Info
- Publication number
- JPH0572685B2 JPH0572685B2 JP60136371A JP13637185A JPH0572685B2 JP H0572685 B2 JPH0572685 B2 JP H0572685B2 JP 60136371 A JP60136371 A JP 60136371A JP 13637185 A JP13637185 A JP 13637185A JP H0572685 B2 JPH0572685 B2 JP H0572685B2
- Authority
- JP
- Japan
- Prior art keywords
- cadmium
- thin film
- cto
- compound
- film
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Landscapes
- Liquid Crystal (AREA)
- Electrochromic Elements, Electrophoresis, Or Variable Reflection Or Absorption Elements (AREA)
- Surface Treatment Of Glass (AREA)
- Chemically Coating (AREA)
- Non-Insulated Conductors (AREA)
- Manufacturing Of Electric Cables (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP13637185A JPS6290809A (ja) | 1985-06-21 | 1985-06-21 | 酸化物透明導電性薄膜の製法 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP13637185A JPS6290809A (ja) | 1985-06-21 | 1985-06-21 | 酸化物透明導電性薄膜の製法 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS6290809A JPS6290809A (ja) | 1987-04-25 |
JPH0572685B2 true JPH0572685B2 (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html) | 1993-10-12 |
Family
ID=15173599
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP13637185A Granted JPS6290809A (ja) | 1985-06-21 | 1985-06-21 | 酸化物透明導電性薄膜の製法 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS6290809A (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html) |
Families Citing this family (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JP2838111B2 (ja) * | 1988-12-02 | 1998-12-16 | 横河電機株式会社 | 薄膜el素子およびその製造方法 |
JP3660372B2 (ja) * | 1994-06-29 | 2005-06-15 | セイコーインスツル株式会社 | 透明導電性薄膜の製造方法 |
CN104086087A (zh) * | 2014-06-19 | 2014-10-08 | 东华大学 | 一种自晶种生长的鸟巢状水合氧化钨纳米结构电致变色薄膜的制备方法 |
Family Cites Families (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS61273807A (ja) * | 1985-05-28 | 1986-12-04 | 鐘淵化学工業株式会社 | 酸化物透明導電性薄膜 |
-
1985
- 1985-06-21 JP JP13637185A patent/JPS6290809A/ja active Granted
Also Published As
Publication number | Publication date |
---|---|
JPS6290809A (ja) | 1987-04-25 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JP3616128B2 (ja) | 透明導電膜の製造方法 | |
US3759743A (en) | Method of applying coarings of tin oxide upon transparent substrates | |
JP2013541442A (ja) | 光電池のガラスがコーティングされた可撓性ポリマー基材 | |
KR910000408B1 (ko) | 투명도전막의 제조방법 | |
CN1280960A (zh) | 铟锡氧化物薄膜溶胶-凝胶制备方法 | |
WO2004094328A1 (en) | Coating compositions | |
JPH08264022A (ja) | 透明導電膜 | |
JPH0572685B2 (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html) | ||
JP4377003B2 (ja) | 透明導電膜のシート抵抗値の調整方法及び透明導電膜の形成方法 | |
JP2011108637A (ja) | 低屈折率透明導電膜の製造方法及び低屈折率透明導電膜、低屈折率透明導電基板並びにそれを用いたデバイス | |
JPH0467285B2 (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html) | ||
GB2428689A (en) | Process for preparing transparent conducting metal oxides | |
JP4522566B2 (ja) | 透明導電膜のシート抵抗値の調整方法 | |
JPH01132004A (ja) | 透光性導基板およびその製造方法 | |
JPS639018B2 (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html) | ||
JPH06234521A (ja) | 透明導電膜およびその製造方法 | |
JPS60135576A (ja) | カドミウム−スズ複合酸化物薄膜の製法 | |
JP2004026554A (ja) | 透明導電膜形成液及びそれを用いた透明導電膜付基体の製法 | |
JP2561680B2 (ja) | 透明酸化物薄膜被着ガラスの製造方法 | |
JP2526632B2 (ja) | 透明導電性酸化亜鉛膜の製造方法 | |
JP4365918B2 (ja) | 透明導電膜形成用塗布液およびこれを使用した透明導電膜形成方法 | |
KR100378019B1 (ko) | 투명 도전막의 보호막 형성용 조성물 및 이로부터 투명도전막을 제조하는 방법 | |
JPS61261235A (ja) | 透明導電膜の形成法 | |
JPH07122359A (ja) | 電子レンジオーブンの窓部 | |
JPS62267476A (ja) | 透明導電性被膜形成組成物 |