JPH0555982B2 - - Google Patents
Info
- Publication number
- JPH0555982B2 JPH0555982B2 JP61144648A JP14464886A JPH0555982B2 JP H0555982 B2 JPH0555982 B2 JP H0555982B2 JP 61144648 A JP61144648 A JP 61144648A JP 14464886 A JP14464886 A JP 14464886A JP H0555982 B2 JPH0555982 B2 JP H0555982B2
- Authority
- JP
- Japan
- Prior art keywords
- active material
- negative electrode
- cadmium
- paste
- material paste
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Links
Classifications
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M4/00—Electrodes
- H01M4/02—Electrodes composed of, or comprising, active material
- H01M4/24—Electrodes for alkaline accumulators
- H01M4/26—Processes of manufacture
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M4/00—Electrodes
- H01M4/02—Electrodes composed of, or comprising, active material
- H01M4/62—Selection of inactive substances as ingredients for active masses, e.g. binders, fillers
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02E—REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02E60/00—Enabling technologies; Technologies with a potential or indirect contribution to GHG emissions mitigation
- Y02E60/10—Energy storage using batteries
Landscapes
- Chemical & Material Sciences (AREA)
- Chemical Kinetics & Catalysis (AREA)
- Electrochemistry (AREA)
- General Chemical & Material Sciences (AREA)
- Engineering & Computer Science (AREA)
- Manufacturing & Machinery (AREA)
- Battery Electrode And Active Subsutance (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP61144648A JPS63965A (ja) | 1986-06-19 | 1986-06-19 | アルカリ蓄電池用カドミウム負極板の製造法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP61144648A JPS63965A (ja) | 1986-06-19 | 1986-06-19 | アルカリ蓄電池用カドミウム負極板の製造法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS63965A JPS63965A (ja) | 1988-01-05 |
| JPH0555982B2 true JPH0555982B2 (enExample) | 1993-08-18 |
Family
ID=15366963
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP61144648A Granted JPS63965A (ja) | 1986-06-19 | 1986-06-19 | アルカリ蓄電池用カドミウム負極板の製造法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS63965A (enExample) |
Families Citing this family (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US5208122A (en) * | 1991-03-26 | 1993-05-04 | Sanyo Electric Co., Ltd. | Enclosed alkaline storage cell |
| KR20170042281A (ko) * | 2014-08-08 | 2017-04-18 | 스미토모덴키고교가부시키가이샤 | 나트륨 이온 2차 전지용 양극 및 나트륨 이온 2차 전지 |
-
1986
- 1986-06-19 JP JP61144648A patent/JPS63965A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS63965A (ja) | 1988-01-05 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| CN113644260A (zh) | 一种CuCo-BDC超薄纳米片及其制备方法和用途 | |
| KR20210122281A (ko) | 고접착성 및 고이온전도도의 코팅 슬러리 및 제조 방법, 리튬 배터리 분리막 | |
| JPH0555982B2 (enExample) | ||
| JPS6313270A (ja) | アルカリ蓄電池用カドミウム負極板の製造法 | |
| JPS6313269A (ja) | アルカリ蓄電池用カドミウム負極板の製造法 | |
| JPS6313271A (ja) | アルカリ蓄電池用カドミウム負極板の製造法 | |
| CN110993897A (zh) | 一种提高阀控式密封铅酸电池使用寿命的正极添加剂及其应用 | |
| JPH02253557A (ja) | 水素吸蔵電極の製造法 | |
| JP2000160118A (ja) | 結着剤および粉体の結着方法 | |
| CN118702078B (zh) | 一种磷酸铁和磷酸铁锂材料的制备方法及应用 | |
| JPS60170167A (ja) | アルカリ電池用電極の製造方法 | |
| JPH0355030B2 (enExample) | ||
| JPS62113360A (ja) | スラリ−式カドミウム極板の製造法 | |
| CN115275146A (zh) | 一种钠离子电池正极浆料及其制备方法 | |
| JPS6134861A (ja) | アルカリ蓄電池用焼結基板の製造方法 | |
| JPS636743A (ja) | 鉛蓄電池極板の製造法 | |
| JPS5945186B2 (ja) | 鉛蓄電池用陰極板の製造法 | |
| JPH03184261A (ja) | アルカリ蓄電池用陰極板の製造法 | |
| JP3540558B2 (ja) | アルカリ蓄電池用水酸化ニッケル電極の製造方法とこの製造方法で得られた水酸化ニッケル電極 | |
| JPH0424823B2 (enExample) | ||
| JPS6273566A (ja) | 密閉形アルカリ蓄電池用陰極板の製造方法 | |
| JPH0426184B2 (enExample) | ||
| JP2989001B2 (ja) | アルカリ蓄電池用カドミウム負極の製造方法 | |
| JPH0711955B2 (ja) | アルカリ蓄電池用非焼結式カドミウム陰極 | |
| JPH09147849A (ja) | ペースト式アルカリ蓄電池用負極とその製造方法 |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| LAPS | Cancellation because of no payment of annual fees |