JPH0549419B2 - - Google Patents
Info
- Publication number
- JPH0549419B2 JPH0549419B2 JP60152851A JP15285185A JPH0549419B2 JP H0549419 B2 JPH0549419 B2 JP H0549419B2 JP 60152851 A JP60152851 A JP 60152851A JP 15285185 A JP15285185 A JP 15285185A JP H0549419 B2 JPH0549419 B2 JP H0549419B2
- Authority
- JP
- Japan
- Prior art keywords
- residual stress
- shot
- hole
- internal defect
- internal
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Landscapes
- Application Of Or Painting With Fluid Materials (AREA)
- Pressure Vessels And Lids Thereof (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP15285185A JPS6215025A (ja) | 1985-07-11 | 1985-07-11 | 鋳造部品の流体漏れ補修方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP15285185A JPS6215025A (ja) | 1985-07-11 | 1985-07-11 | 鋳造部品の流体漏れ補修方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS6215025A JPS6215025A (ja) | 1987-01-23 |
| JPH0549419B2 true JPH0549419B2 (cg-RX-API-DMAC7.html) | 1993-07-26 |
Family
ID=15549514
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP15285185A Granted JPS6215025A (ja) | 1985-07-11 | 1985-07-11 | 鋳造部品の流体漏れ補修方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS6215025A (cg-RX-API-DMAC7.html) |
Families Citing this family (9)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP2637443B2 (ja) * | 1987-12-07 | 1997-08-06 | トピー工業株式会社 | 鋳造アルミホイールの加工方法 |
| JPH0655449A (ja) * | 1992-08-03 | 1994-03-01 | Hino Motors Ltd | ショットブラスト加工を利用したワークの表面仕上げ方法 |
| JPH10166271A (ja) * | 1996-12-09 | 1998-06-23 | Sinto Brator Co Ltd | 軽合金製品のショットピーニング方法 |
| JP4706948B2 (ja) * | 2001-04-05 | 2011-06-22 | 新東工業株式会社 | 軽合金鋳造製品の表面処理方法 |
| JP5059385B2 (ja) * | 2006-11-29 | 2012-10-24 | 旭テック株式会社 | 軽合金鋳造製車両用ホイール |
| AU2009329094B2 (en) * | 2008-12-18 | 2013-09-12 | Csir | Method of repairing a metallic artefact |
| HUE031748T2 (en) * | 2012-09-10 | 2017-07-28 | Vulkan Inox Gmbh | Method and Spray for Creating an Aluminum Satin Surface |
| CN106737212A (zh) * | 2016-12-02 | 2017-05-31 | 江苏毅合捷汽车科技股份有限公司 | 一种高效环保的汽车涡轮增压器再制造喷砂工艺 |
| CN109676317B (zh) * | 2018-11-10 | 2021-03-16 | 芜湖天航装备技术有限公司 | 一种用于组合传动发电机壳体再修复方法 |
Family Cites Families (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5970447A (ja) * | 1982-10-12 | 1984-04-20 | Nippon Kokan Kk <Nkk> | 連続鋳造鋳片の表面疵除去方法 |
-
1985
- 1985-07-11 JP JP15285185A patent/JPS6215025A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS6215025A (ja) | 1987-01-23 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US6289705B1 (en) | Method for the ultrasonic peening of large sized annular surfaces of thin parts | |
| US4233720A (en) | Method of forming and ultrasonic testing articles of near net shape from powder metal | |
| CN104001752B (zh) | 一种钢制管件生产工艺 | |
| JP3974385B2 (ja) | ロータへの羽根の固定部の寿命を延ばすための方法 | |
| RU2407620C2 (ru) | Металлическая деталь, обрабатываемая методом компрессии ее подповерхностных слоев, и способ ее изготовления | |
| CN102123828B (zh) | 涡轮机部件的超声波喷丸处理方法 | |
| JPH0549419B2 (cg-RX-API-DMAC7.html) | ||
| JPH06297331A (ja) | 金属表面にブラストする装置と方法 | |
| US20090094829A1 (en) | Method for ultrasonic peening of gas turbine engine components without engine disassembly | |
| CN106078525A (zh) | 大型热浸锌工件表面涂装前处理工艺 | |
| KR20250019722A (ko) | 강교의 예방 보전 공법 | |
| TWI619123B (zh) | 儲存桶之應力腐蝕破裂防止方法以及儲存桶 | |
| JP2024038318A (ja) | 鋼橋の予防保全工法、及びこれに用いられる循環式ブラスト装置 | |
| CN105862028A (zh) | 一种汽车发动机曲轴的激光修复再制造方法 | |
| Kinoshita et al. | Fatigue strength improvement of welded joints of existing steel bridges by shot-peening | |
| CN109487183B (zh) | 一种适用于铝锂合金的湿喷丸表面改性方法 | |
| JPH07314170A (ja) | 原子炉容器ノズルの溶接引張り応力低減方法 | |
| US20110308290A1 (en) | Method for ultrasonic peening of gas turbine engine components without engine disassembly | |
| JP6644334B2 (ja) | 金型冷却孔の表面処理方法及び金型 | |
| JPH08267400A (ja) | ウォータージェットによる表面異質層を有する材料表面の処理方法 | |
| JP2018196927A (ja) | サンドブラスト装置セットおよび鉄塔の素地調整方法 | |
| RU2757881C1 (ru) | Способ виброударной обработки деталей из титановых сплавов | |
| JPS61126368A (ja) | デイ−ゼル機関用燃料高圧管およびその製造方法 | |
| JP2024010583A (ja) | 鋼橋の予防保全工法 | |
| Patil | Repairing casting defects by high pressure cold spraying method |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| EXPY | Cancellation because of completion of term |