JPH0546859B2 - - Google Patents
Info
- Publication number
- JPH0546859B2 JPH0546859B2 JP8891985A JP8891985A JPH0546859B2 JP H0546859 B2 JPH0546859 B2 JP H0546859B2 JP 8891985 A JP8891985 A JP 8891985A JP 8891985 A JP8891985 A JP 8891985A JP H0546859 B2 JPH0546859 B2 JP H0546859B2
- Authority
- JP
- Japan
- Prior art keywords
- acrylamide
- meth
- weight
- temperature
- substituted
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Links
Landscapes
- Compositions Of Macromolecular Compounds (AREA)
- Addition Polymer Or Copolymer, Post-Treatments, Or Chemical Modifications (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP8891985A JPS61247716A (ja) | 1985-04-26 | 1985-04-26 | 感温性重合体エマルシヨン |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP8891985A JPS61247716A (ja) | 1985-04-26 | 1985-04-26 | 感温性重合体エマルシヨン |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS61247716A JPS61247716A (ja) | 1986-11-05 |
| JPH0546859B2 true JPH0546859B2 (index.php) | 1993-07-15 |
Family
ID=13956324
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP8891985A Granted JPS61247716A (ja) | 1985-04-26 | 1985-04-26 | 感温性重合体エマルシヨン |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS61247716A (index.php) |
Families Citing this family (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| ES2118563T3 (es) * | 1994-02-10 | 1998-09-16 | Kohjin Co | Mezcla de polimeros que absorbe/desabsorbe agua sensible a la temperatura. |
| JP4874572B2 (ja) * | 2000-02-29 | 2012-02-15 | 三洋化成工業株式会社 | 原油増産用添加剤 |
| JP5521189B2 (ja) * | 2008-05-07 | 2014-06-11 | 国立大学法人東北大学 | フィルム及びフィルム製造方法 |
| CN107406555B (zh) * | 2015-04-28 | 2020-02-14 | 深圳大学 | 一种形状记忆聚合物及其制备方法和应用 |
-
1985
- 1985-04-26 JP JP8891985A patent/JPS61247716A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS61247716A (ja) | 1986-11-05 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| CA1286823C (en) | Aqueous fluorinated acrylate resin emulsions | |
| AU719694B2 (en) | Aqueous stable dispersions based on water-soluble polymers containing a cationic dispersant comprising hydrophobic units | |
| US6221957B1 (en) | Aqueous saline dispersions of water-soluble polymers containing an amphiphilic dispersant based on a cationic polymer containing hydrophobic units | |
| US4098987A (en) | Non-ionic surfactants from water soluble copolymers of acrylamide with hydrophobic monomers | |
| CN101792496A (zh) | 梯度共聚物的制备方法 | |
| JP5554428B2 (ja) | 塩素化ビニルポリマーからラテックスを調製するための方法 | |
| JPH0546859B2 (index.php) | ||
| US3512985A (en) | Direct positive photographic silver halide emulsions and elements containing water insoluble polymers | |
| JP3513479B2 (ja) | 高温低粘度低温高粘度型感温性高分子材料 | |
| JPH11100404A (ja) | 水性乳化重合のための保護コロイドとしての新規コロイド分散系混合物、それの製造方法及び使用法 | |
| JP3101714B1 (ja) | 可逆的な親水性−疎水性変化を示す共重合体及びその製造方法 | |
| JP2991241B2 (ja) | 超高分子量の感熱性ポリアクリルアミド系誘導体の製造方法 | |
| JP3587267B2 (ja) | 耐塩水性ラテックス | |
| JP2884069B2 (ja) | pH感応性、感熱性マイクロビーズ及びその製造方法 | |
| JPH0586409B2 (index.php) | ||
| JP2004217724A (ja) | 水性エマルジョンの製造方法 | |
| JP2945966B2 (ja) | pH感応性、感熱性マイクロビーズの製造方法 | |
| JPS61210A (ja) | 水性組成物の製造方法 | |
| JP3747249B2 (ja) | 高分子乳化剤、その製造法及びそれを用いる乳化重合法 | |
| JPH07258342A (ja) | 耐塩水性ラテックス | |
| JPS6312611A (ja) | 銅キレ−ト能をもつ感熱高分子 | |
| JP3538632B2 (ja) | 感熱性離水剤及びその製造方法 | |
| JP2001019938A (ja) | 感熱性ゲルマイクロビーズ及びその製造方法 | |
| JPS6187717A (ja) | 重合体エマルシヨン | |
| US4528322A (en) | Aqueous cationic dispersions of synthetic polymers |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| LAPS | Cancellation because of no payment of annual fees |