- JPH0545664B2 JPH0545664B2 JP57215563A JP21556382A JPH0545664B2 JP H0545664 B2 JPH0545664 B2 JP H0545664B2 JP 57215563 A JP57215563 A JP 57215563A JP 21556382 A JP21556382 A JP 21556382A JP H0545664 B2 JPH0545664 B2 JP H0545664B2
- Authority
- JP
- Japan
- Prior art keywords
- heating
- based alloy
- nickel
- corrosion resistance
- treating
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Landscapes
- Arc Welding In General (AREA)
- Heat Treatment Of Nonferrous Metals Or Alloys (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP21556382A JPS59107068A (ja) | 1982-12-10 | 1982-12-10 | ニツケル基合金溶接部の処理法 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP21556382A JPS59107068A (ja) | 1982-12-10 | 1982-12-10 | ニツケル基合金溶接部の処理法 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS59107068A JPS59107068A (ja) | 1984-06-21 |
JPH0545664B2 true JPH0545664B2 (enrdf_load_stackoverflow) | 1993-07-09 |
Family
ID=16674496
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP21556382A Granted JPS59107068A (ja) | 1982-12-10 | 1982-12-10 | ニツケル基合金溶接部の処理法 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS59107068A (enrdf_load_stackoverflow) |
Families Citing this family (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US6344097B1 (en) * | 2000-05-26 | 2002-02-05 | Integran Technologies Inc. | Surface treatment of austenitic Ni-Fe-Cr-based alloys for improved resistance to intergranular-corrosion and-cracking |
US6589298B1 (en) | 2000-05-26 | 2003-07-08 | Integran Technologies, Inc. | Surface treatment of metallic components of electrochemical cells for improved adhesion and corrosion resistance |
EP1456430A1 (en) * | 2001-11-23 | 2004-09-15 | Integran Technologies Inc. | Surface treatment of austenitic ni-fe-cr based alloys |
WO2020111017A1 (ja) * | 2018-11-30 | 2020-06-04 | Jfeスチール株式会社 | 溶接継手の耐疲労特性向上方法 |
Family Cites Families (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5469517A (en) * | 1977-11-16 | 1979-06-04 | Hitachi Ltd | Improving method for intergranular corrosion resistance of ni alloy |
-
1982
- 1982-12-10 JP JP21556382A patent/JPS59107068A/ja active Granted
Also Published As
Publication number | Publication date |
---|---|
JPS59107068A (ja) | 1984-06-21 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS6254022A (ja) | 酸性ガスおよび/または油の輸送用に使用可能の溶接鋼管の製造方法 | |
Ramkumar et al. | Effect of low energy laser shock peening on the mechanical integrity of Hastelloy C-276 welds | |
KR20010022644A (ko) | 니켈 및 철기 수퍼합금을 처리하기 위한 야금학적 방법 | |
JP2007284704A (ja) | 含Crニッケル基合金管の製造方法および含Crニッケル基合金管 | |
Chandrasekar et al. | Investigation on un-peened and laser shock peened weldment of Inconel 600 fabricated by ATIG welding process | |
Roshith et al. | Investigations on induced residual stresses, mechanical and metallurgical properties of CO2 laser beam and pulse current gas tungsten arc welded SMO 254 | |
JP3428175B2 (ja) | 表面処理層を有する構造物および表面処理層の形成方法 | |
CN119609359A (zh) | 一种通过飞秒激光处理镍基高温合金获得高强韧接头的制备方法 | |
JPH0545664B2 (enrdf_load_stackoverflow) | ||
JP4176546B2 (ja) | 原子炉構成材料 | |
JP3077576B2 (ja) | 低炭素マルテンサイト系ステンレス鋼溶接管の製造方法 | |
JP4196755B2 (ja) | 低炭素ステンレス鋼管の配管溶接継手とその製造方法 | |
JP3319358B2 (ja) | 耐水素誘起割れ性、耐硫化物応力割れ性および低温靭性に優れたラインパイプ用溶接鋼管の製造方法 | |
JP2000254776A (ja) | 原子炉内部配管溶接部の応力腐食割れ防止方法 | |
Sorokin et al. | Weldability of cast creep-resisting nickel alloys of the ZhS6 type | |
JP3674085B2 (ja) | 原子炉圧力容器ノズルの熱処理方法 | |
JP2005510627A (ja) | ニッケル・鉄・クロムを主成分とするオーステナイト系合金の表面処理 | |
Kumar et al. | Influence of laser power and welding speed on dendrite structure growth of low power pulsed laser welded super alloy | |
JPS60238423A (ja) | 二相系ステンレス鋼の溶接部の耐食性改善方法 | |
JP3064851B2 (ja) | マルテンサイト系ステンレス鋼溶接管の製造方法 | |
JP3146918B2 (ja) | オーステナイト系ステンレス鋼溶接管の製造方法 | |
Yu et al. | The influence of laser welding process parameters on welding joint of TA15 titanium alloy sheets | |
JPH07188737A (ja) | 核燃料再処理プラント用耐食機器の耐食処理方法 | |
Yu et al. | Effects of Thermal Ageing on Microstructure and Hardness of Ni Cladding on Austenitic Stainless Steel by GTAW | |
JPH11241146A (ja) | 耐食性に優れた構造物およびその製造方法、ならびに、構造物の改修方法 |