JPH0517303B2 - - Google Patents
Info
- Publication number
- JPH0517303B2 JPH0517303B2 JP62150392A JP15039287A JPH0517303B2 JP H0517303 B2 JPH0517303 B2 JP H0517303B2 JP 62150392 A JP62150392 A JP 62150392A JP 15039287 A JP15039287 A JP 15039287A JP H0517303 B2 JPH0517303 B2 JP H0517303B2
- Authority
- JP
- Japan
- Prior art keywords
- less
- temperature
- stress corrosion
- treatment
- corrosion cracking
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Landscapes
- Heat Treatment Of Nonferrous Metals Or Alloys (AREA)
- Heat Treatment Of Articles (AREA)
- Heat Treatment Of Steel (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP15039287A JPS62297446A (ja) | 1987-06-17 | 1987-06-17 | Ni基合金の熱処理法 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP15039287A JPS62297446A (ja) | 1987-06-17 | 1987-06-17 | Ni基合金の熱処理法 |
Related Parent Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP186980A Division JPS5698464A (en) | 1980-01-11 | 1980-01-11 | Treating method for improving resistance to stress and corrosion cracking of ni-based alloy |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS62297446A JPS62297446A (ja) | 1987-12-24 |
JPH0517303B2 true JPH0517303B2 (enrdf_load_stackoverflow) | 1993-03-08 |
Family
ID=15495988
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP15039287A Granted JPS62297446A (ja) | 1987-06-17 | 1987-06-17 | Ni基合金の熱処理法 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS62297446A (enrdf_load_stackoverflow) |
Family Cites Families (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5035023A (enrdf_load_stackoverflow) * | 1973-07-14 | 1975-04-03 |
-
1987
- 1987-06-17 JP JP15039287A patent/JPS62297446A/ja active Granted
Also Published As
Publication number | Publication date |
---|---|
JPS62297446A (ja) | 1987-12-24 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
US8470106B2 (en) | Method of heat treatment for desensitizing a nickel-based alloy relative to environmentally-assisted cracking, in particular for a nuclear reactor fuel assembly and for a nuclear reactor, and a part made of the alloy and subjected to the treatment | |
Staehle et al. | Effect of alloy composition on stress corrosion cracking of Fe-Cr-Ni base alloys | |
JPS59159958A (ja) | 析出硬化性銅合金及びその処理方法 | |
JPS58153751A (ja) | 耐酸化性ニツケル合金 | |
SU649329A3 (ru) | Способ термической обработки алюминиевых сплавов | |
JPH0517303B2 (enrdf_load_stackoverflow) | ||
JPS6358220B2 (enrdf_load_stackoverflow) | ||
Andrieu et al. | Influence of compositional modifications on thermal stability of alloy 718 | |
JPS58123857A (ja) | 耐焼戻し脆性に優れた圧力容器用鋼材 | |
JPS6277448A (ja) | 耐SCC性に優れた高強度Ni基合金部材の製造方法 | |
JPS62250136A (ja) | Cu合金製端子 | |
JPS59208066A (ja) | 内部窒化モリブデン−ジルコニウム合金の加工法 | |
JPH02247358A (ja) | 原子炉部材用Fe基合金及びその製造法 | |
JPH079048B2 (ja) | 高強度および高硬度を有する耐食性Ni基合金線材 | |
JPS60100629A (ja) | オ−ステナイトステンレス鋼の製造方法 | |
JPS5817823B2 (ja) | Crを含有するNi基合金の熱処理方法 | |
JPS5985850A (ja) | Ni基合金の熱処理法 | |
SU1601146A1 (ru) | Способ термообработки сплава системы F @ - N @ - Со - Т @ с эффектом пам ти формы | |
SU1168610A1 (ru) | Способ обработки магнитотвердых сплавов на основе системы железо-молибден-никель | |
JPS59200747A (ja) | Cu−Zn−Al系形状記憶合金の熱処理方法 | |
JPH06271939A (ja) | 高強度2相ステンレス鋼線材の製造方法 | |
JPS62177155A (ja) | 耐応力腐食割れ性に優れたFe基合金及びその製造方法 | |
SU1668467A1 (ru) | Способ химико-термической обработки | |
JPS6128021B2 (enrdf_load_stackoverflow) | ||
JPS63241150A (ja) | チタン合金の熱処理方法 |