JPH0455415Y2 - - Google Patents
Info
- Publication number
- JPH0455415Y2 JPH0455415Y2 JP1985102584U JP10258485U JPH0455415Y2 JP H0455415 Y2 JPH0455415 Y2 JP H0455415Y2 JP 1985102584 U JP1985102584 U JP 1985102584U JP 10258485 U JP10258485 U JP 10258485U JP H0455415 Y2 JPH0455415 Y2 JP H0455415Y2
- Authority
- JP
- Japan
- Prior art keywords
- substrate
- active material
- sintered substrate
- liquid
- electrolytic
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Classifications
-
- Y02E60/124—
Landscapes
- Battery Electrode And Active Subsutance (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP1985102584U JPH0455415Y2 (enrdf_load_html_response) | 1985-07-05 | 1985-07-05 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP1985102584U JPH0455415Y2 (enrdf_load_html_response) | 1985-07-05 | 1985-07-05 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS6210364U JPS6210364U (enrdf_load_html_response) | 1987-01-22 |
| JPH0455415Y2 true JPH0455415Y2 (enrdf_load_html_response) | 1992-12-25 |
Family
ID=30974364
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP1985102584U Expired JPH0455415Y2 (enrdf_load_html_response) | 1985-07-05 | 1985-07-05 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPH0455415Y2 (enrdf_load_html_response) |
Families Citing this family (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| AT394225B (de) * | 1988-10-05 | 1992-02-25 | Meru Horst Mag | Baukoerper |
Family Cites Families (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5372137A (en) * | 1976-12-08 | 1978-06-27 | Furukawa Battery Co Ltd | Method of manufacturing electrode plate for storage battery |
| JPS5482631A (en) * | 1977-12-14 | 1979-07-02 | Matsushita Electric Industrial Co Ltd | Method of producing anode plate for alkaline storage battery |
| JPS5546480A (en) * | 1978-09-30 | 1980-04-01 | Shin Kobe Electric Mach Co Ltd | Manufacturing method of electrode board for nickel- cadmium cell |
-
1985
- 1985-07-05 JP JP1985102584U patent/JPH0455415Y2/ja not_active Expired
Also Published As
| Publication number | Publication date |
|---|---|
| JPS6210364U (enrdf_load_html_response) | 1987-01-22 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| CN210059085U (zh) | 一种铜箔加工用清洗装置 | |
| JPS59114812A (ja) | エツチングされた陰極アルミニウムコンデンサフオイルの清浄化及び処理並びにそれにより製造されたフオイル | |
| CN204589336U (zh) | 一种具有清理装置的电解铜箔制箔机 | |
| JPH0455415Y2 (enrdf_load_html_response) | ||
| JP3916526B2 (ja) | シリコン基板のエッチング方法 | |
| JP3009006B2 (ja) | 半導体基板の乾燥装置 | |
| JPS61133633A (ja) | 半導体ウエ−ハの洗浄装置 | |
| CN110021683A (zh) | 一种碲化镉太阳能电池基板处理工艺 | |
| CN109801789A (zh) | 一种利用二段直流电发孔制备中压腐蚀箔的方法 | |
| US3489612A (en) | Method of impregnating sintered matrixes for negative electrodes for alkaline storage batteries with active material | |
| JPH0215577A (ja) | 固体電解質管の洗浄方法 | |
| JPS6130060Y2 (enrdf_load_html_response) | ||
| CN209101675U (zh) | 锂电池用铝箔的生产装置 | |
| JPH1059747A (ja) | ガラス板の洗滌乾燥方法及びその装置 | |
| JPH0112717Y2 (enrdf_load_html_response) | ||
| JPH02270978A (ja) | 鋼板の連続酸洗処理方法 | |
| SU435574A1 (ru) | Способ продления срока службб1 щелочного никель-железного аккумулятора | |
| JPH11162907A (ja) | 洗浄方法 | |
| JPS5546480A (en) | Manufacturing method of electrode board for nickel- cadmium cell | |
| US6428674B1 (en) | Process for the removal of galvanic electrolytic residues from electrode frames or electrode frame webs with fiber structure | |
| JPH0734932Y2 (ja) | ラジアルセル型電解処理装置 | |
| JPH0353497Y2 (enrdf_load_html_response) | ||
| JPS6336533A (ja) | ウエツト洗浄処理方法 | |
| JPH06104148A (ja) | 電解コンデンサ用Al電極箔の交流エッチング方法 | |
| JPS6345276Y2 (enrdf_load_html_response) |