JPH0437544B2 - - Google Patents
Info
- Publication number
- JPH0437544B2 JPH0437544B2 JP60207370A JP20737085A JPH0437544B2 JP H0437544 B2 JPH0437544 B2 JP H0437544B2 JP 60207370 A JP60207370 A JP 60207370A JP 20737085 A JP20737085 A JP 20737085A JP H0437544 B2 JPH0437544 B2 JP H0437544B2
- Authority
- JP
- Japan
- Prior art keywords
- electrode plate
- nickel
- hydroxide
- cycle
- capacity
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Classifications
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M4/00—Electrodes
- H01M4/02—Electrodes composed of, or comprising, active material
- H01M4/24—Electrodes for alkaline accumulators
- H01M4/32—Nickel oxide or hydroxide electrodes
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02E—REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02E60/00—Enabling technologies; Technologies with a potential or indirect contribution to GHG emissions mitigation
- Y02E60/10—Energy storage using batteries
Landscapes
- Chemical & Material Sciences (AREA)
- Chemical Kinetics & Catalysis (AREA)
- Electrochemistry (AREA)
- General Chemical & Material Sciences (AREA)
- Battery Electrode And Active Subsutance (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP60207370A JPS6266569A (ja) | 1985-09-19 | 1985-09-19 | アルカリ蓄電池用陽極板 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP60207370A JPS6266569A (ja) | 1985-09-19 | 1985-09-19 | アルカリ蓄電池用陽極板 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS6266569A JPS6266569A (ja) | 1987-03-26 |
JPH0437544B2 true JPH0437544B2 (enrdf_load_stackoverflow) | 1992-06-19 |
Family
ID=16538603
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP60207370A Granted JPS6266569A (ja) | 1985-09-19 | 1985-09-19 | アルカリ蓄電池用陽極板 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS6266569A (enrdf_load_stackoverflow) |
Families Citing this family (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH04137368A (ja) * | 1990-09-26 | 1992-05-12 | Matsushita Electric Ind Co Ltd | ニッケル/水素蓄電池とその製造法 |
JP3717786B2 (ja) * | 1998-02-20 | 2005-11-16 | 三洋電機株式会社 | アルカリ蓄電池用ニッケル極、アルカリ蓄電池用ニッケル極の製造方法及びアルカリ蓄電池 |
EP1901373A1 (en) | 1998-11-30 | 2008-03-19 | Sanyo Electric Co., Ltd. | Nickel electrodes for alkaline secondary battery and alkaline secondary batteries |
Family Cites Families (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5319086A (en) * | 1976-08-04 | 1978-02-21 | Jiyuuzou Maekawa | Compound stress load universal tester |
JPS54129331A (en) * | 1978-03-29 | 1979-10-06 | Sanyo Electric Co | Alkaliizinc storage battery |
-
1985
- 1985-09-19 JP JP60207370A patent/JPS6266569A/ja active Granted
Also Published As
Publication number | Publication date |
---|---|
JPS6266569A (ja) | 1987-03-26 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
US4084047A (en) | Stable alkaline zinc electrode | |
US6348284B1 (en) | Non-sintered nickel electrode for a secondary electro-chemical cell having an alkaline electrolyte | |
JPH02112165A (ja) | アルカリ蓄電池 | |
JPH0437544B2 (enrdf_load_stackoverflow) | ||
WO1998031063A1 (fr) | Accumulateur alcalin et procede de charge d'accumulateur | |
JPS5983347A (ja) | 密閉形ニツケル−カドミウム蓄電池 | |
JP3204275B2 (ja) | アルカリ蓄電池用ニッケル電極 | |
JP2591988B2 (ja) | カドミウム負極板およびその負極板を用いたアルカリ二次電池 | |
JPS61233967A (ja) | 密閉形ニツケル−水素蓄電池の製造法 | |
JPS63158749A (ja) | アルカリ蓄電池用亜鉛極 | |
JPS5910538B2 (ja) | ニツケル−カドミウムアルカリ蓄電池 | |
JP2858855B2 (ja) | アルカリ蓄電池用水酸化ニッケル電極及びその製造方法 | |
JP2810460B2 (ja) | アルカリ蓄電池用正極板 | |
JP2975673B2 (ja) | カドミウム負極板の製造方法 | |
JPH10172559A (ja) | アルカリ蓄電池用ニッケル活物質およびその製造方法 | |
JP2865397B2 (ja) | アルカリ蓄電池の製造方法 | |
JPS6188453A (ja) | アルカリ蓄電池用ニツケル正極 | |
JPH0239063B2 (enrdf_load_stackoverflow) | ||
JPH0430145B2 (enrdf_load_stackoverflow) | ||
JPH01117273A (ja) | 鉛蓄電池 | |
JPS58672B2 (ja) | 密閉式アルカリ蓄電池の製造法 | |
JPS632266A (ja) | ニツケル亜鉛蓄電池 | |
JPS58119159A (ja) | アルカリ蓄電池用亜鉛極 | |
JPH071695B2 (ja) | アルカリ亜鉛蓄電池 | |
JPH03744B2 (enrdf_load_stackoverflow) |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
EXPY | Cancellation because of completion of term |