JPH0335399B2 - - Google Patents
Info
- Publication number
- JPH0335399B2 JPH0335399B2 JP58139266A JP13926683A JPH0335399B2 JP H0335399 B2 JPH0335399 B2 JP H0335399B2 JP 58139266 A JP58139266 A JP 58139266A JP 13926683 A JP13926683 A JP 13926683A JP H0335399 B2 JPH0335399 B2 JP H0335399B2
- Authority
- JP
- Japan
- Prior art keywords
- type
- chromium
- auxiliary agent
- electrolytic
- molar ratio
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Landscapes
- Electrochemical Coating By Surface Reaction (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP13926683A JPS6029494A (ja) | 1983-07-29 | 1983-07-29 | 塗料密着性にすぐれたティンフリ−スチ−ルの製造方法 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP13926683A JPS6029494A (ja) | 1983-07-29 | 1983-07-29 | 塗料密着性にすぐれたティンフリ−スチ−ルの製造方法 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS6029494A JPS6029494A (ja) | 1985-02-14 |
JPH0335399B2 true JPH0335399B2 (enrdf_load_stackoverflow) | 1991-05-28 |
Family
ID=15241277
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP13926683A Granted JPS6029494A (ja) | 1983-07-29 | 1983-07-29 | 塗料密着性にすぐれたティンフリ−スチ−ルの製造方法 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS6029494A (enrdf_load_stackoverflow) |
Family Cites Families (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS6040519B2 (ja) * | 1981-04-25 | 1985-09-11 | 川崎製鉄株式会社 | テインフリ−鋼板の製造方法 |
-
1983
- 1983-07-29 JP JP13926683A patent/JPS6029494A/ja active Granted
Also Published As
Publication number | Publication date |
---|---|
JPS6029494A (ja) | 1985-02-14 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
EP2143822B1 (en) | Plated steel sheet for cans and process for producing the same | |
TWI424098B (zh) | 具優異耐蝕性之罐用鋼板 | |
EP0101871B1 (en) | Method of producing tin-free steel sheets having improved resistance to retorting treatment | |
JPS6363640B2 (enrdf_load_stackoverflow) | ||
JPS59170298A (ja) | 塗料密着性にすぐれたテインフリ−鋼板の製造方法 | |
JPH0335399B2 (enrdf_load_stackoverflow) | ||
JPS6254096A (ja) | 溶接性に優れた電解クロメ−ト処理鋼板及びその製造方法 | |
JPS58210197A (ja) | 耐レトルト処理性にすぐれたテインフリ−鋼の製造方法 | |
JP2576570B2 (ja) | 電解クロメート処理鋼板の前処理方法 | |
JPH0366397B2 (enrdf_load_stackoverflow) | ||
JPH0246678B2 (enrdf_load_stackoverflow) | ||
JPH01219195A (ja) | 電解クロメート処理鋼板の製造方法 | |
JP3093917B2 (ja) | ラミネート鋼板およびその原板 | |
JPH0215640B2 (enrdf_load_stackoverflow) | ||
CA1238293A (en) | Method for producing tin-free steel strips having improved lacquer adhesion | |
JPS5974296A (ja) | 耐レトルト処理性のすぐれたテインフリ−スチ−ルの製造方法 | |
JPS6116434B2 (enrdf_load_stackoverflow) | ||
JPS631397B2 (enrdf_load_stackoverflow) | ||
JPS6056098A (ja) | 塗料密着性の優れたティンフリ−スチ−ルの製造方法 | |
JPS60114595A (ja) | 接着性のすぐれたティンフリ−スチ−ル | |
JPS6310237B2 (enrdf_load_stackoverflow) | ||
JPS5927400B2 (ja) | 湿滑接着性にすぐれた電解クロメ−ト処理鋼板の製造法 | |
JPH0225593A (ja) | 均一なクロム酸化膜を有するティンフリー鋼板の製造方法 | |
JPS6123795A (ja) | 塗料2次密着性のすぐれたテインフリ−スチ−ルの製造方法 | |
JPS634090A (ja) | 製缶用表面処理鋼板 |