JPH0260796B2 - - Google Patents
Info
- Publication number
- JPH0260796B2 JPH0260796B2 JP57092153A JP9215382A JPH0260796B2 JP H0260796 B2 JPH0260796 B2 JP H0260796B2 JP 57092153 A JP57092153 A JP 57092153A JP 9215382 A JP9215382 A JP 9215382A JP H0260796 B2 JPH0260796 B2 JP H0260796B2
- Authority
- JP
- Japan
- Prior art keywords
- paper
- paper strength
- polymer
- monomer
- acrylamide
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Landscapes
- Paper (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP9215382A JPS58214597A (ja) | 1982-06-01 | 1982-06-01 | 紙の製造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP9215382A JPS58214597A (ja) | 1982-06-01 | 1982-06-01 | 紙の製造方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS58214597A JPS58214597A (ja) | 1983-12-13 |
| JPH0260796B2 true JPH0260796B2 (enrdf_load_html_response) | 1990-12-18 |
Family
ID=14046472
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP9215382A Granted JPS58214597A (ja) | 1982-06-01 | 1982-06-01 | 紙の製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS58214597A (enrdf_load_html_response) |
Families Citing this family (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP2575692B2 (ja) * | 1987-03-20 | 1997-01-29 | 三井サイテック株式会社 | 紙の製造法 |
| JP3291665B2 (ja) * | 1993-12-24 | 2002-06-10 | 荒川化学工業株式会社 | 抄き合わせ紙の製造方法 |
| KR101506920B1 (ko) * | 2006-10-25 | 2015-03-30 | 시바 홀딩 인크 | 종이 강도를 향상시키는 방법 |
Family Cites Families (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS56107099A (en) * | 1980-01-21 | 1981-08-25 | Kyowa Sangyo | Paper strength increasing method |
| JPH0685495A (ja) * | 1992-04-17 | 1994-03-25 | Apollo Hokuriku:Kk | 電子部品搭載装置と、それにおける部品位置決め方法 |
-
1982
- 1982-06-01 JP JP9215382A patent/JPS58214597A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS58214597A (ja) | 1983-12-13 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US4051086A (en) | Absorption rate of absorbent polymers by treating with glyoxal | |
| JP3014695B2 (ja) | ポリマー組成物 | |
| US4798861A (en) | Surface treatment of polymers | |
| CA1238132A (en) | Aqueous polymer dispersions | |
| US5032628A (en) | Process for the preparation of a highly water absorptive resin from acrylic resin, epoxy crosslinker and hydrophilic silicate | |
| JP3926852B2 (ja) | 紙を製造する方法、及びそれに用いるための材料 | |
| FI105567B (fi) | Menetelmä hienojen superimukykyisten polymeeripartikkeleiden muuttamiseksi suuremmiksi partikkeleiksi | |
| EP3420005B1 (en) | Glyoxalated polyacrylamide terpolymer, base copolymer thereof, compositions containing same, uses in papermaking and products thereof | |
| EP0233014A2 (en) | Polymers and processes for their production from water soluble monomers | |
| US4759856A (en) | Flocculation processes | |
| AU2015370830B2 (en) | A method for producing interpenetrating polymer network material, a product thereof and use of the product | |
| KR20070100240A (ko) | 제지방법 | |
| JPH11315112A (ja) | ポリアクリロニトリルエマルジョンを基とする改質超吸収材 | |
| US4511477A (en) | Process of using water-absorbent agents for low pH applications | |
| JPH0260796B2 (enrdf_load_html_response) | ||
| US7740743B2 (en) | Fine particle size lime slurries and their production | |
| RU2003121405A (ru) | Агломерат связующих средств, способ его получения и его применение | |
| JPS58154710A (ja) | 両性高吸水性樹脂の製法 | |
| US5435834A (en) | Ore pelletization | |
| JPS58127714A (ja) | 高吸水性ポリマ−の製造法 | |
| JP2907476B2 (ja) | 製紙用添加剤 | |
| JPH0841103A (ja) | 吸水性セルロース材料の製造方法 | |
| JP5311360B2 (ja) | 水溶性重合体の製造方法 | |
| JPH0229084B2 (ja) | Kokyusuiseijushinoseiho | |
| KR950013063B1 (ko) | 고 흡수성 수지 유화액을 포함하는 조성물 |