JPH02290947A - 耐サワー性の優れた高靭性電縫鋼管用鋼板 - Google Patents
耐サワー性の優れた高靭性電縫鋼管用鋼板Info
- Publication number
- JPH02290947A JPH02290947A JP11257889A JP11257889A JPH02290947A JP H02290947 A JPH02290947 A JP H02290947A JP 11257889 A JP11257889 A JP 11257889A JP 11257889 A JP11257889 A JP 11257889A JP H02290947 A JPH02290947 A JP H02290947A
- Authority
- JP
- Japan
- Prior art keywords
- toughness
- steel
- sour resistance
- steel plate
- content
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Treatment Of Steel In Its Molten State (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP11257889A JPH02290947A (ja) | 1989-05-01 | 1989-05-01 | 耐サワー性の優れた高靭性電縫鋼管用鋼板 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP11257889A JPH02290947A (ja) | 1989-05-01 | 1989-05-01 | 耐サワー性の優れた高靭性電縫鋼管用鋼板 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPH02290947A true JPH02290947A (ja) | 1990-11-30 |
JPH0587582B2 JPH0587582B2 (enrdf_load_stackoverflow) | 1993-12-17 |
Family
ID=14590229
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP11257889A Granted JPH02290947A (ja) | 1989-05-01 | 1989-05-01 | 耐サワー性の優れた高靭性電縫鋼管用鋼板 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPH02290947A (enrdf_load_stackoverflow) |
Cited By (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH0593243A (ja) * | 1991-07-02 | 1993-04-16 | Kawasaki Steel Corp | 炭酸ガスおよび硫化水素ガスに対する耐食性にすぐれたラインパイプ用鋼 |
US7074283B2 (en) * | 2002-03-29 | 2006-07-11 | Sumitomo Metal Industries, Ltd. | Low alloy steel |
EP2412839A4 (en) * | 2009-03-25 | 2017-03-01 | Nippon Steel & Sumitomo Metal Corporation | Electric resistance welded steel pipe having excellent workability and excellent post-quenching fatigue properties |
Citations (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS56112440A (en) * | 1980-02-06 | 1981-09-04 | Nippon Kokan Kk <Nkk> | Steel for pipeline with superior sulfide stress corrosion crack resistance |
JPS5887221A (ja) * | 1981-11-20 | 1983-05-25 | Nippon Kokan Kk <Nkk> | 耐硫化物腐食割れ性に優れた高張力鋼の製造方法 |
JPS5976818A (ja) * | 1982-10-22 | 1984-05-02 | Nippon Steel Corp | 耐水素誘起割れ性の優れた鋼材の製造方法 |
-
1989
- 1989-05-01 JP JP11257889A patent/JPH02290947A/ja active Granted
Patent Citations (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS56112440A (en) * | 1980-02-06 | 1981-09-04 | Nippon Kokan Kk <Nkk> | Steel for pipeline with superior sulfide stress corrosion crack resistance |
JPS5887221A (ja) * | 1981-11-20 | 1983-05-25 | Nippon Kokan Kk <Nkk> | 耐硫化物腐食割れ性に優れた高張力鋼の製造方法 |
JPS5976818A (ja) * | 1982-10-22 | 1984-05-02 | Nippon Steel Corp | 耐水素誘起割れ性の優れた鋼材の製造方法 |
Cited By (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH0593243A (ja) * | 1991-07-02 | 1993-04-16 | Kawasaki Steel Corp | 炭酸ガスおよび硫化水素ガスに対する耐食性にすぐれたラインパイプ用鋼 |
US7074283B2 (en) * | 2002-03-29 | 2006-07-11 | Sumitomo Metal Industries, Ltd. | Low alloy steel |
EP2412839A4 (en) * | 2009-03-25 | 2017-03-01 | Nippon Steel & Sumitomo Metal Corporation | Electric resistance welded steel pipe having excellent workability and excellent post-quenching fatigue properties |
US9757780B2 (en) | 2009-03-25 | 2017-09-12 | Nippon Steel & Sumitomo Metal Corporation | Electric resistance welded steel pipe excellent in deformability and fatigue properties after quenching |
Also Published As
Publication number | Publication date |
---|---|
JPH0587582B2 (enrdf_load_stackoverflow) | 1993-12-17 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JP3116156B2 (ja) | 耐食性および溶接性に優れた鋼管の製造方法 | |
JPH10503809A (ja) | 熱間加工性に優れた耐硫化物応力割れ性を有するマルテンサイト系ステンレス鋼 | |
JP3379355B2 (ja) | 耐硫化物応力割れ性を必要とする環境で使用される高強度鋼材およびその製造方法 | |
CN113166827A (zh) | 热轧钢及其制造方法 | |
JP3879723B2 (ja) | 耐水素誘起割れ性に優れた高強度継目無鋼管およびその製造方法 | |
JPH0375337A (ja) | 高強度かつ耐食性の優れたマルテンサイト系ステンレス鋼 | |
CN100420758C (zh) | 具有优异抗氢致开裂性的高强度无缝钢管及其制备方法 | |
EP0774519A1 (en) | Process for producing steel material and steel pipe excellent in corrosion resistance and weldability | |
JP2711163B2 (ja) | 耐co▲下2▼腐食性の優れた高耐食性低合金ラインパイプ用鋼の製造法 | |
JPH05271766A (ja) | 耐水素誘起割れ性の優れた高強度鋼板の製造方法 | |
JP2620809B2 (ja) | 耐高温高塩化物イオン濃度湿潤高圧炭酸ガス環境腐食性、耐応力腐食割れ性の優れた高強度マルテンサイト系ステンレス鋼およびその製造方法 | |
EP0738784A1 (en) | High chromium martensitic steel pipe having excellent pitting resistance and method of manufacturing | |
JP2742948B2 (ja) | 耐食性の優れたマルテンサイト系ステンレス鋼およびその製造方法 | |
JPH08104922A (ja) | 低温靱性の優れた高強度鋼管の製造方法 | |
AU758316B2 (en) | High Cr steel pipe for line pipe | |
JPS647138B2 (enrdf_load_stackoverflow) | ||
JPH02290947A (ja) | 耐サワー性の優れた高靭性電縫鋼管用鋼板 | |
JP2742949B2 (ja) | 耐食性の優れたマルテンサイト系ステンレス鋼およびその製造方法 | |
JP2602319B2 (ja) | 高強度かつ耐高温高塩化物イオン濃度湿潤炭酸ガス環境腐食性、耐応力腐食割れ別の優れたマルテンサイト系ステンレス鋼およびその製造方法 | |
JPH0553855B2 (enrdf_load_stackoverflow) | ||
JPH08209289A (ja) | 耐遅れ破壊性に優れた機械構造用鋼 | |
JPS61201759A (ja) | ラインパイプ用高強度高靭性溶接クラツド鋼管 | |
JPS61104054A (ja) | ラインパイプ用高強度高靭性溶接クラツド鋼管 | |
JP3085253B2 (ja) | 湿潤硫化水素環境で疲労亀裂進展特性に優れる原油タンカー用鋼板の製造方法 | |
JPS6199661A (ja) | ラインパイプ用高強度高靭性溶接クラツド鋼管 |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
FPAY | Renewal fee payment (event date is renewal date of database) |
Free format text: PAYMENT UNTIL: 20081217 Year of fee payment: 15 |
|
FPAY | Renewal fee payment (event date is renewal date of database) |
Free format text: PAYMENT UNTIL: 20081217 Year of fee payment: 15 |
|
FPAY | Renewal fee payment (event date is renewal date of database) |
Free format text: PAYMENT UNTIL: 20091217 Year of fee payment: 16 |
|
EXPY | Cancellation because of completion of term | ||
FPAY | Renewal fee payment (event date is renewal date of database) |
Free format text: PAYMENT UNTIL: 20091217 Year of fee payment: 16 |