JPH0222125B2 - - Google Patents

Info

Publication number
JPH0222125B2
JPH0222125B2 JP57014720A JP1472082A JPH0222125B2 JP H0222125 B2 JPH0222125 B2 JP H0222125B2 JP 57014720 A JP57014720 A JP 57014720A JP 1472082 A JP1472082 A JP 1472082A JP H0222125 B2 JPH0222125 B2 JP H0222125B2
Authority
JP
Japan
Prior art keywords
steel pipe
temperature
grain size
treatment
fine
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Lifetime
Application number
JP57014720A
Other languages
English (en)
Japanese (ja)
Other versions
JPS58133352A (ja
Inventor
Kazuhiro Kanero
Takashi Shiraishi
Isao Minegishi
Jusuke Minami
Shunei Kodera
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
JFE Engineering Corp
Original Assignee
Nippon Kokan Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Nippon Kokan Ltd filed Critical Nippon Kokan Ltd
Priority to JP1472082A priority Critical patent/JPS58133352A/ja
Publication of JPS58133352A publication Critical patent/JPS58133352A/ja
Publication of JPH0222125B2 publication Critical patent/JPH0222125B2/ja
Granted legal-status Critical Current

Links

Landscapes

  • Solid-Phase Diffusion Into Metallic Material Surfaces (AREA)
  • Heat Treatment Of Articles (AREA)
JP1472082A 1982-02-03 1982-02-03 オーステナイトステンレス鋼管の製造法 Granted JPS58133352A (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP1472082A JPS58133352A (ja) 1982-02-03 1982-02-03 オーステナイトステンレス鋼管の製造法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP1472082A JPS58133352A (ja) 1982-02-03 1982-02-03 オーステナイトステンレス鋼管の製造法

Related Child Applications (1)

Application Number Title Priority Date Filing Date
JP32798488A Division JPH01287249A (ja) 1988-12-27 1988-12-27 オーステナイトステンレス鋼管およびその製造法

Publications (2)

Publication Number Publication Date
JPS58133352A JPS58133352A (ja) 1983-08-09
JPH0222125B2 true JPH0222125B2 (enrdf_load_stackoverflow) 1990-05-17

Family

ID=11868965

Family Applications (1)

Application Number Title Priority Date Filing Date
JP1472082A Granted JPS58133352A (ja) 1982-02-03 1982-02-03 オーステナイトステンレス鋼管の製造法

Country Status (1)

Country Link
JP (1) JPS58133352A (enrdf_load_stackoverflow)

Families Citing this family (7)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPH04110456A (ja) * 1990-08-30 1992-04-10 Natl Res Inst For Metals 合金とその製造方法
JPH09249946A (ja) * 1996-03-14 1997-09-22 Nkk Corp 加圧流動床燃焼型火力発電プラント用鋼
JP3632672B2 (ja) * 2002-03-08 2005-03-23 住友金属工業株式会社 耐水蒸気酸化性に優れたオーステナイト系ステンレス鋼管およびその製造方法
WO2011096592A1 (ja) * 2010-02-04 2011-08-11 小田産業株式会社 高強度・高延性で優れた耐食性・耐熱性を有する高窒素ステンレス鋼管及びそれらの製造方法
RU2511158C2 (ru) 2010-06-09 2014-04-10 Сумитомо Метал Индастриз, Лтд. Труба из нержавеющей аустенитной стали с отличной стойкостью к окислению паром и способ ее получения
ES2712806T3 (es) 2011-06-28 2019-05-14 Nippon Steel & Sumitomo Metal Corp Tubo de acero inoxidable austenítico
CN104907351B (zh) * 2015-04-22 2017-01-18 苏州劲元油压机械有限公司 一种滤油网用强韧不锈钢丝及其制造工艺

Family Cites Families (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS5558329A (en) * 1978-10-21 1980-05-01 Nippon Kokan Kk <Nkk> Production of iron base alloy pipe of superior oxidation resistance to high temperature steam
JPS5681658A (en) * 1979-12-05 1981-07-03 Nippon Kokan Kk <Nkk> Austenitic alloy pipe with superior hot steam oxidation resistance

Also Published As

Publication number Publication date
JPS58133352A (ja) 1983-08-09

Similar Documents

Publication Publication Date Title
JP4135691B2 (ja) 窒化物系介在物形態制御鋼
JP2009280836A (ja) 耐遅れ破壊特性に優れた高強度pc鋼線及びその製造方法
WO2015004906A1 (ja) 高炭素熱延鋼板およびその製造方法
CN113166894B (zh) 具有改善的耐腐蚀性的铁素体不锈钢及其制造方法
JP2011214058A (ja) 高強度ステンレス鋼線及びその製造方法
JPH0421718A (ja) 耐硫化物応力割れ性に優れた高強度鋼の製造法
EP1170391B1 (en) High strength steel plate having improved workability and plating adhesion and process for producing the same
JPH0222125B2 (enrdf_load_stackoverflow)
JP4374196B2 (ja) 加工性、めっき性および靱性に優れた微細組織を有する高強度鋼板及びその製造方法
JPH0453943B2 (enrdf_load_stackoverflow)
JP2001140041A (ja) ばね用複層組織クロム系ステンレス鋼およびその製造方法
EP3971307A1 (en) Electric-resistance-welded steel pipe for hollow stabilizer
JP2756534B2 (ja) 高延性棒鋼の製造方法
JPH0250916A (ja) 細粒化組織の低合金高張力シームレス鋼管の製造法
CN112063932B (zh) 深冲用热轧搪瓷钢及其制造方法
JPH07207337A (ja) 高強度2相ステンレス鋼材の製造方法
JPS5811492B2 (ja) 高力ボルト用高張力高延性線材及び棒鋼の製造法
JP3201081B2 (ja) 油井用ステンレス鋼およびその製造方法
TW202210642A (zh) 沃斯田鐵系不鏽鋼板及其製造方法
JPH0254403B2 (enrdf_load_stackoverflow)
JPH07179943A (ja) 耐食性に優れた高靭性マルテンサイト系ステンレス鋼継目無鋼管の製造法
JP3620099B2 (ja) 強度と靱性に優れるCr−Mo鋼の製造方法
JPS5940220B2 (ja) 耐硫化物腐食割れ性の優れた低合金鋼
JPS5910415B2 (ja) 耐応力腐食割れ性の優れた高張力線材及び棒鋼の製造法
KR0143476B1 (ko) 열간가공성이 우수한 질소첨가 오스테나이트계 스테인레스강