JP5623329B2 - 流動性改善型セメントクリンカー - Google Patents
流動性改善型セメントクリンカー Download PDFInfo
- Publication number
- JP5623329B2 JP5623329B2 JP2011093395A JP2011093395A JP5623329B2 JP 5623329 B2 JP5623329 B2 JP 5623329B2 JP 2011093395 A JP2011093395 A JP 2011093395A JP 2011093395 A JP2011093395 A JP 2011093395A JP 5623329 B2 JP5623329 B2 JP 5623329B2
- Authority
- JP
- Japan
- Prior art keywords
- cement
- cement clinker
- clinker
- ratio
- tio
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Description
ケイ酸率(SM)= SiO2/(Al2O3+Fe2O3)
後述する実施例、比較例に具体的に結果を示すように、クリンカー中のTiO2含有量が1質量%の場合には、通常の普通ポルトランドセメントと同等な鉄率やケイ酸率とした場合、即ち鉄率が1.8程度、ケイ酸率が2.4程度ではペーストフローの値が低下する。換言すれば、本発明のクリンカーは従来のセメントクリンカーに比べて鉄率が大幅に低く、ケイ酸率も低めのものである。
(1)セメントクリンカーの化学組成の測定:JIS R 5204に準拠する蛍光X線分析法により測定した。
(2)セメントペーストフローの測定:JAS 15 M−103に準拠して測定し、練り混ぜ時間を3分、水/セメント比0.50、混和剤添加なし、試験温度を20℃とし、練り上がり直後のフローを測定した。
クリンカー中のTi含有量が、TiO2換算で0.5質量%、鉄率、ケイ酸率が所定の値となるように各原料の配合比を調整し、これを焼成してセメントクリンカーを得た。得られたセメントクリンカーの化学組成及び三率を表1に示す。
焼成後のセメントクリンカーの組成が表1に示す値になるようにTiO2含有量および原料組成を変化させた以外は、実施例1と同様にしてセメントを製造し、セメントペーストフローの測定を行なった。
Claims (3)
- TiO2を0.5〜1.0質量%含むポルトランドセメントクリンカーであって、鉄率(IM)が1.0〜1.3、ケイ酸率(SM)が2.2〜2.32の範囲にあることを特徴とするポルトランドセメントクリンカー。
- 請求項1記載のポルトランドセメントクリンカーと、石膏とを含むポルトランドセメント。
- 更に、高炉スラグ、シリカ質混合材、フライアッシュ及び石灰石からなる群から選ばれるいずれか1種以上の混合材を含む請求項2記載のポルトランドセメント。