JP4486085B2 - 金属ストリップを溶融浸漬被覆する方法 - Google Patents
金属ストリップを溶融浸漬被覆する方法 Download PDFInfo
- Publication number
- JP4486085B2 JP4486085B2 JP2006518003A JP2006518003A JP4486085B2 JP 4486085 B2 JP4486085 B2 JP 4486085B2 JP 2006518003 A JP2006518003 A JP 2006518003A JP 2006518003 A JP2006518003 A JP 2006518003A JP 4486085 B2 JP4486085 B2 JP 4486085B2
- Authority
- JP
- Japan
- Prior art keywords
- guide passage
- container
- metal
- metal strip
- coating
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Description
特開平11−193451号による解決手段は、同様に底領域内の電磁弁によって容器内の被覆金属を保持する。
ドイツ連邦共和国特許出願公開第195 35 854号明細書及びドイツ連邦共和国特許出願公開第100 14 867号明細書は、ガイド通路内の金属ストリップの位置を精確に制御する特別な解決手段を提唱する。ここで開示された概念によれば、移動磁場を生成するコイルに加えて、さらなる補正コイルが設けられている。これらの補正コイルは、制御システムに接続していて、金属板が中心の位置からずれた時にこの中心の位置に再び戻される作用をする。
したがって、ガイド通路の有効幅が、このガイド通路の垂線延長部分にわたって変化する。この場合、ガイド通路の下面と容器の底との間の検討すべき高さは重要である。1つの区域が、ガイド通路の設けられている横断面の変化によってガイド通路の垂線延長部分内に提供される。被覆金属中の流れが、この区域内で鎮静できる。これによって、金属浴の表面も鎮静する。
狭隘部又は拡大部の横断面が、主に円の一部の形を有する。
この代わりの又は追加の構成は、ガイド通路を仕切る壁が狭隘部を有することを提唱する。またこの代わりに又はこれに追加して、ガイド通路を仕切る壁が拡大部を有することが提唱され得る。この狭隘部又は拡大部の横断面が、主に円の切片の形を有してもよい。少なくとも1つの流れ誘導要素が、容器内に及び/又はガイド通路内に配置されていることがその他の構成にしたがって提唱される場合、別の流れの鎮静が実現され得る。この流れ誘導要素は、平坦で幅の狭い板として効果的に形成されている。この板の長手軸線は、金属ストリップの送り方向に対して垂直にかつ金属ストリップの表面の法線方向に対して垂直に延在している。さらに、少なくとも1つの流れ誘導要素を拡張部の領域内のガイド通路内に配置してもよい。
本発明の実施の形態を図面に基づいて説明する。
コイル5の磁場が、制御部に応じて補正コイルによって増幅又は減衰され得る(磁場の重ね合わせ原理)。こうして、ガイドチャネル4内の金属ストリップ1の位置が制御され得る。
図2の狭隘部10を上方に延長して拡大部11につなげてもよいことは、図示されていない。
2 被覆金属
3 容器
4 ガイド通路
5 コイル
6 仕切壁
7 ガイド通路の下面
8 容器の底領域
9 漏斗状部分
10 狭隘部
11 拡大部
12,12′,12″流れ誘導要素
13,13′ 流れ誘導要素
14 流れ誘導要素の長手軸線
15 被覆金属の表面
16 浴鎮静板
17 アクチュエータ
d ガイド通路を仕切る壁の距離
N 金属ストリップの表面に対する法線方向
H ガイド通路の垂線延長部分の範囲
h 漏斗状部分の垂線延長部分
R 送り方向
Claims (8)
- 金属ストリップ(1)を溶融浸漬被覆する装置にあって、この装置内では、金属ストリップ(1)が、溶融されている被覆金属(2)を収容している容器(3)及びこの容器(3)に直列に連結されているガイド通路(4)を貫通し、当該装置は、前記ガイド通路(4)の領域内の金属ストリップ(1)の両側に配置された少なくとも2つのコイル(5)を有し、これらのコイル(5)は、前記被覆金属(2)を前記容器(3)内に保持する電磁場を生成する当該装置において、
前記ガイド通路(4)の下面(7)と前記容器(3)の底領域(8)との間にある前記ガイド通路(4)の垂線延長部分の範囲(H)内で、前記ガイド通路(4)を仕切る壁(6)の距離(d)が、前記金属ストリップ(1)の表面に対する法線(N)の方向に一定でなく設定されていて、
前記ガイド通路(4)を仕切る前記壁(6)が、狭隘部(10)を有するか又は狭隘部(10)及び拡大部(11)を有することを特徴とする装置。 - 前記狭隘部(10)又は前記拡大部(11)の横断面が、円の一部の形を有することを特徴とする請求項1に記載の装置。
- 少なくとも1つの流れ誘導要素(12,12′,12″,13,13′)が、前記容器(3)及び/又は前記ガイド通路(4)内に配置されていることを特徴とする請求項1又は2に記載の装置。
- 前記流れ誘導要素(12,12′,12″,13,13′)は、平坦な板として形成されていて、この平坦な板の長手軸線(14)が、前記金属ストリップ(1)の送り方向(R)に対して垂直にかつこの金属ストリップ(1)の表面の法線方向(N)に対して垂直に延在していることを特徴とする請求項3に記載の装置。
- 前記ガイド通路(4)内の前記少なくとも1つの流れ誘導要素(13,13′)は、前記拡大部(11)の領域内に配置されていることを特徴とする請求項3又は4に記載の装置。
- 少なくとも1つの浴鎮静板(16)が、前記容器(3)内の前記被覆金属(2)の表面(15)の領域内に配置されていることを特徴とする請求項1〜5のいずれか1項に記載の装置。
- 前記浴鎮静板(16)の位置の高さが、アクチュエータ(17)によって調整可能であることを特徴とする請求項6に記載の装置。
- 前記浴鎮静板(16)は、セラミック材料製であることを特徴とする請求項6又は7に記載の装置。