JP2524286Y2 - マイクロ波加熱溶融炉のルツボ構造 - Google Patents
マイクロ波加熱溶融炉のルツボ構造Info
- Publication number
- JP2524286Y2 JP2524286Y2 JP13291U JP13291U JP2524286Y2 JP 2524286 Y2 JP2524286 Y2 JP 2524286Y2 JP 13291 U JP13291 U JP 13291U JP 13291 U JP13291 U JP 13291U JP 2524286 Y2 JP2524286 Y2 JP 2524286Y2
- Authority
- JP
- Japan
- Prior art keywords
- crucible
- hole
- pipe
- peripheral wall
- melting furnace
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
- 238000002844 melting Methods 0.000 title claims description 19
- 230000008018 melting Effects 0.000 title claims description 19
- 238000010438 heat treatment Methods 0.000 claims description 13
- 239000002184 metal Substances 0.000 claims description 13
- 230000002093 peripheral effect Effects 0.000 claims description 13
- 238000013022 venting Methods 0.000 claims description 8
- 239000007788 liquid Substances 0.000 description 16
- 239000000155 melt Substances 0.000 description 11
- 238000007872 degassing Methods 0.000 description 6
- 239000000463 material Substances 0.000 description 6
- 239000012768 molten material Substances 0.000 description 6
- 239000012466 permeate Substances 0.000 description 4
- 239000000047 product Substances 0.000 description 4
- 238000000034 method Methods 0.000 description 3
- 230000001681 protective effect Effects 0.000 description 3
- 239000010802 sludge Substances 0.000 description 3
- 230000004907 flux Effects 0.000 description 2
- 239000011521 glass Substances 0.000 description 2
- 238000010309 melting process Methods 0.000 description 2
- 239000000126 substance Substances 0.000 description 2
- 239000002699 waste material Substances 0.000 description 2
- 238000007792 addition Methods 0.000 description 1
- 238000010276 construction Methods 0.000 description 1
- 238000001816 cooling Methods 0.000 description 1
- 238000010586 diagram Methods 0.000 description 1
- 238000011038 discontinuous diafiltration by volume reduction Methods 0.000 description 1
- 238000001035 drying Methods 0.000 description 1
- 238000001704 evaporation Methods 0.000 description 1
- 230000008020 evaporation Effects 0.000 description 1
- 230000004927 fusion Effects 0.000 description 1
- 239000007769 metal material Substances 0.000 description 1
- 239000002901 radioactive waste Substances 0.000 description 1
- 238000011084 recovery Methods 0.000 description 1
- 150000003839 salts Chemical class 0.000 description 1
- 239000007787 solid Substances 0.000 description 1
- 230000008646 thermal stress Effects 0.000 description 1
- XLYOFNOQVPJJNP-UHFFFAOYSA-N water Substances O XLYOFNOQVPJJNP-UHFFFAOYSA-N 0.000 description 1
Landscapes
- Crucibles And Fluidized-Bed Furnaces (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP13291U JP2524286Y2 (ja) | 1991-01-08 | 1991-01-08 | マイクロ波加熱溶融炉のルツボ構造 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP13291U JP2524286Y2 (ja) | 1991-01-08 | 1991-01-08 | マイクロ波加熱溶融炉のルツボ構造 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPH0495295U JPH0495295U (enrdf_load_stackoverflow) | 1992-08-18 |
| JP2524286Y2 true JP2524286Y2 (ja) | 1997-01-29 |
Family
ID=33524086
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP13291U Expired - Lifetime JP2524286Y2 (ja) | 1991-01-08 | 1991-01-08 | マイクロ波加熱溶融炉のルツボ構造 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JP2524286Y2 (enrdf_load_stackoverflow) |
-
1991
- 1991-01-08 JP JP13291U patent/JP2524286Y2/ja not_active Expired - Lifetime
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0495295U (enrdf_load_stackoverflow) | 1992-08-18 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US6283908B1 (en) | Vitrification of waste with conitnuous filling and sequential melting | |
| DE60129376T3 (de) | Verfahren und Vorrichtung zur Herstellung von Quarzglaskörpern | |
| US5168918A (en) | Casting of dental metals | |
| JP6052805B2 (ja) | チタン鋳塊の製造方法 | |
| JP2524286Y2 (ja) | マイクロ波加熱溶融炉のルツボ構造 | |
| CN213996312U (zh) | 一种废旧沥青路面材料分离装置 | |
| JP3015423B2 (ja) | 素電池の処理方法 | |
| ZA85865B (en) | A closure cap and method of making the same | |
| US3934107A (en) | Process for repairing slag ladles | |
| JPH0376880B2 (enrdf_load_stackoverflow) | ||
| JPS61180646A (ja) | 密封空間内で金属又は合金を処理および鋳造する方法および装置 | |
| US6562245B2 (en) | Crushed foam glass filter aid and method of use | |
| US4460524A (en) | Method for heating a riser of molten refractory material | |
| JPS61168719A (ja) | 廃棄物溶融炉の出滓設備 | |
| RU2209842C2 (ru) | Способ плавки и литья металла | |
| CN112267129A (zh) | 一种用于铝制品回收过滤的电解槽 | |
| US4686025A (en) | Apparatus for the production of a metal by electrolyzing halides in a molten salt bath, by a simultaneous continuous double deposit | |
| JPH01320074A (ja) | 放射性又は有害廃棄物の燃焼装置から生じる灰分又は燃焼残分をガラス様の耐浸出性の最終貯蔵に好適な生成物に変換する方法 | |
| JP4274475B2 (ja) | 溶融用キャニスタ | |
| JPH0421727A (ja) | チタン鋳塊の製造方法および装置 | |
| US2104530A (en) | Electric furnace process | |
| DE1533120A1 (de) | Verfahren und Vorrichtung zur Reinigung von Kupfer | |
| JPS631512B2 (enrdf_load_stackoverflow) | ||
| RU2168226C1 (ru) | Способ остекловывания радиоактивных отходов в охлаждаемом металлическом индукционном плавителе | |
| JPH05126997A (ja) | ガラス固化体の製造方法 |