JP2512763B2 - ろう付け用ストップオフ剤 - Google Patents

ろう付け用ストップオフ剤

Info

Publication number
JP2512763B2
JP2512763B2 JP21416287A JP21416287A JP2512763B2 JP 2512763 B2 JP2512763 B2 JP 2512763B2 JP 21416287 A JP21416287 A JP 21416287A JP 21416287 A JP21416287 A JP 21416287A JP 2512763 B2 JP2512763 B2 JP 2512763B2
Authority
JP
Japan
Prior art keywords
stop
brazing
agent
effect
flow
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Lifetime
Application number
JP21416287A
Other languages
English (en)
Other versions
JPS6462266A (en
Inventor
道彦 西島
隆司 醍醐
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Tokuriki Honten Co Ltd
Original Assignee
Tokuriki Honten Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Tokuriki Honten Co Ltd filed Critical Tokuriki Honten Co Ltd
Priority to JP21416287A priority Critical patent/JP2512763B2/ja
Publication of JPS6462266A publication Critical patent/JPS6462266A/ja
Application granted granted Critical
Publication of JP2512763B2 publication Critical patent/JP2512763B2/ja
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Description

【発明の詳細な説明】 〔産業上の利用分野〕 本発明は、高温時においても酸化防止効果のあるろう
付け用ストップオフ剤に関する。
〔従来の技術〕
従来、ろう付け時の流れ止め(ストップオフ)用とし
て用いられているものに、酸化物、黒鉛、との粉等の粉
末と水あるいはアルコールとを混合したペースト剤が用
いられていた。
〔発明が解決しようとする問題点〕
しかし、このようなストップオフ剤は、ろう付け面に
塗布しておくことにより酸化防止の効果がないことはな
いが、高温時における酸化防止効果は必ずしも充分では
なく、ろう付け用として特に硬ろうのろう付け時のよう
に比較的高温で用いられるストップオフ剤には、流れ止
めの効果と酸化防止の効果とを兼ね備えたものがないと
いう問題があった。
〔問題点を解決する為の手段〕
本発明は、C1〜C4のアルコール65〜85Wt%、酸化ほう
素10〜30Wt%および四ほう酸ナトリウム5Wt%以下より
なる酸化防止液と、ろう付け時において流れ止めする材
料すなわちマグネシア、アルミナ、チタニア、酸化クロ
ムもしくはカルシア等の安定な酸化物粉末とを、重量比
で1:0.3〜1:1の割合で混合することによりペースト化し
てろう付け用ストップオフ剤としたことを特徴とする。
なお、上記組成成分において、酸化防止液中の酸化ほ
う素は10Wt%未満では酸化防止の効果は弱く、30Wt%を
越えると溶媒中への溶解度限を越えてしまうことにな
る。
四ほう酸ナトリウムは5Wt%を越えると溶媒中への溶
解度限を越えてしまうことになる。
〔作用〕
以上の本発明によると、酸化防止液の溶媒としてC1〜
C4のアルコールを用いたことにより有機溶剤の性質およ
び揮発性を有し、金属材料表面に多少の油脂類があって
もその表面にむらなく塗布することができ、かつすばや
く蒸発して直ちに一様なストップオフ剤の層を形成する
ことできる。
また、流れ止め材として酸化物粉末を用いたことによ
り比較的高温時においても酸化防止の作用があると共に
流れ止めの作用がある。
〔実 施 例〕
以下に本発明の実施例を第1表に示す。
以上のストップオフ剤の酸化の有無と流れ止め効果の
実験結果を以下の第2表に示す。なを、比較のために従
来例としてマグネシアとエタノールを混合してペース
ト化したもの、アルミナと水を混合してペースト化し
たものを用いた。
実験は、それぞれのペーストを銅の基材に塗布後、硬
ろうであるBAG−8からなるろう材をもちい、大気中800
℃で2分〜5分加熱後、塗布部分の酸化の有無と流れ止
め効果の有無をもって比較した。
〔発明の効果〕 以上説明した本発明によると、C1〜C4のアルコール、
酸化ほう素および四ほう酸ナトリウムからなる酸化防止
液と酸化物粉末とを混合してペースト状にしたことによ
り、酸化防止液の溶媒としてC1〜C4のアルコールを用い
ているために有機溶剤の性質および揮発性を有し、金属
材料表面に多少の油脂類があってもその表面にむらなく
塗布することができ、しかもすばやく蒸発して直ちに一
様なストップオフ剤の層を形成することができる効果を
有する。
また、流れ止め材として酸化物粉末を用いたことによ
り比較的高温時においても酸化防止の効果があると共に
流れ止めの効果があり、すぐれたろう付け用ストップオ
フ剤となる。

Claims (1)

    (57)【特許請求の範囲】
  1. 【請求項1】C1〜C4のアルコール65〜85Wt%、酸化ほう
    素10〜30Wt%および四ほう酸ナトリウム5Wt%以下より
    なる酸化防止液と、ろう付け時において流れ止めする材
    料すなわちマグネシア、アルミナ、チタニア、酸化クロ
    ムもしくはカルシア等の安定な酸化物粉末とを、重量比
    で1:0.3〜1:1の割合で混合してペースト化したことを特
    徴とするろう付け用ストップオフ剤。
JP21416287A 1987-08-29 1987-08-29 ろう付け用ストップオフ剤 Expired - Lifetime JP2512763B2 (ja)