JP2013214005A5 - - Google Patents

Download PDF

Info

Publication number
JP2013214005A5
JP2013214005A5 JP2012085208A JP2012085208A JP2013214005A5 JP 2013214005 A5 JP2013214005 A5 JP 2013214005A5 JP 2012085208 A JP2012085208 A JP 2012085208A JP 2012085208 A JP2012085208 A JP 2012085208A JP 2013214005 A5 JP2013214005 A5 JP 2013214005A5
Authority
JP
Japan
Prior art keywords
toner
styrene
adhesive tape
sulfonic acid
glass
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP2012085208A
Other languages
English (en)
Japanese (ja)
Other versions
JP2013214005A (ja
Filing date
Publication date
Application filed filed Critical
Priority to JP2012085208A priority Critical patent/JP2013214005A/ja
Priority claimed from JP2012085208A external-priority patent/JP2013214005A/ja
Publication of JP2013214005A publication Critical patent/JP2013214005A/ja
Publication of JP2013214005A5 publication Critical patent/JP2013214005A5/ja
Pending legal-status Critical Current

Links

JP2012085208A 2012-04-04 2012-04-04 トナー Pending JP2013214005A (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP2012085208A JP2013214005A (ja) 2012-04-04 2012-04-04 トナー

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP2012085208A JP2013214005A (ja) 2012-04-04 2012-04-04 トナー

Publications (2)

Publication Number Publication Date
JP2013214005A JP2013214005A (ja) 2013-10-17
JP2013214005A5 true JP2013214005A5 (enExample) 2015-05-21

Family

ID=49587360

Family Applications (1)

Application Number Title Priority Date Filing Date
JP2012085208A Pending JP2013214005A (ja) 2012-04-04 2012-04-04 トナー

Country Status (1)

Country Link
JP (1) JP2013214005A (enExample)

Families Citing this family (9)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
WO2015080272A1 (ja) * 2013-11-28 2015-06-04 日本ゼオン株式会社 負帯電性トナー及びその製造方法
JP6300631B2 (ja) * 2014-05-14 2018-03-28 キヤノン株式会社 トナー粒子の製造方法およびトナーの製造方法
US10353306B2 (en) * 2015-03-31 2019-07-16 Zeon Corporation Method for producing negatively chargeable toner, and negatively chargeable toner
JP6521782B2 (ja) * 2015-07-30 2019-05-29 キヤノン株式会社 トナー
JP6562775B2 (ja) * 2015-08-28 2019-08-21 キヤノン株式会社 トナー及びトナーの製造方法
JP6619617B2 (ja) * 2015-11-02 2019-12-11 キヤノン株式会社 トナー粒子の製造方法
JP6742115B2 (ja) * 2016-03-03 2020-08-19 キヤノン株式会社 トナー粒子の製造方法
JP2022077739A (ja) 2020-11-12 2022-05-24 キヤノン株式会社 トナー
US20240053691A1 (en) * 2022-08-04 2024-02-15 Canon Kabushiki Kaisha Toner and method for producing toner

Family Cites Families (7)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP4387901B2 (ja) * 2004-09-08 2009-12-24 キヤノン株式会社 トナーキット及び画像形成方法
JP4481788B2 (ja) * 2004-10-15 2010-06-16 キヤノン株式会社 トナーおよび画像形成方法
JP2008015151A (ja) * 2006-07-05 2008-01-24 Canon Inc 磁性微粒子含有型樹脂キャリアを用いた二成分系現像剤
JP2009025327A (ja) * 2007-07-17 2009-02-05 Canon Inc トナー及び画像形成方法
KR101431947B1 (ko) * 2010-03-31 2014-08-19 캐논 가부시끼가이샤 토너 및 토너의 제조 방법
KR101346248B1 (ko) * 2010-03-31 2014-01-02 캐논 가부시끼가이샤 토너 및 토너 입자의 제조 방법
JP5455748B2 (ja) * 2010-03-31 2014-03-26 キヤノン株式会社 トナー及びトナー粒子の製造方法

Similar Documents

Publication Publication Date Title
JP2013214005A5 (enExample)
RU2013120200A (ru) Тонер
JP2010215923A5 (enExample)
JP2019502537A5 (enExample)
Lee et al. Optical properties and adhesion performance of optically clear acrylic pressure sensitive adhesives using chelate metal acetylacetonate
RU2017113383A (ru) Мелкодисперсные водные эмульсионные полимеры и их применение для гидрофобных покрытий
Lopez et al. Simultaneous Free‐Radical and Addition Miniemulsion Polymerization: Effect of the Chain Transfer Agent on the Microstructure of Polyurethane‐Acrylic Pressure‐Sensitive Adhesives
Fang et al. Effect of propyleneimine external cross-linker on the properties of acrylate latex pressure sensitive adhesives
Qie et al. Influence of polymer microstructure on the performance of post‐treated latex‐based pressure sensitive adhesives
JP2016098241A (ja) 水性エマルション、接着剤組成物、及び水性エマルションの製造方法
Sengupta et al. Copolymers from methyl methacrylate and butyl acrylate with hyperbranched architecture
JP2011256289A5 (enExample)
Stavrouli et al. pH/thermosensitive hydrogels formed at low pH by a PMMA‐PAA‐P2VP‐PAA‐PMMA pentablock terpolymer
Machotova et al. Effect of molar mass on film-forming properties of self-crosslinking latexes based on structured acrylic microgels
Thomson et al. Nitroxide-mediated surfactant-free emulsion polymerization of n-butyl methacrylate with a small amount of styrene
CN102808360A (zh) 耐温型高光纸品用水性上光油及其制备方法
Fang et al. Effect of trifunctional cross-linker triallyl isocyanurate (TAIC) on the surface morphology and viscoelasticity of the acrylic emulsion pressure-sensitive adhesives
Qie et al. Manipulating Latex Polymer Microstructure Using Chain Transfer Agent and Cross‐Linker to Modify PSA Performance and Viscoelasticity
JP2011215179A5 (ja) トナー粒子の製造方法及びイエロートナー
WO2014082786A3 (en) Paint composition which has excellent staining resistance and paint films obtained by coating same
JP2020526619A5 (enExample)
Fang et al. Manipulation of chain transfer agent and cross-linker concentration to modify the performance of fluorinated acrylate latex pressure sensitive adhesive
Caballero et al. Radical entry mechanisms in alkali-soluble-resin-stabilized latexes
TWI752192B (zh) 乳液、乳液的製備方法及使用乳液形成塗膜的方法
JP2012083440A5 (enExample)