JP2013040116A - 可逆的付加開裂連鎖移動重合可能な部位を含有するビニルエーテルおよび重合体並びにそれらの製造方法 - Google Patents
可逆的付加開裂連鎖移動重合可能な部位を含有するビニルエーテルおよび重合体並びにそれらの製造方法 Download PDFInfo
- Publication number
- JP2013040116A JP2013040116A JP2011176689A JP2011176689A JP2013040116A JP 2013040116 A JP2013040116 A JP 2013040116A JP 2011176689 A JP2011176689 A JP 2011176689A JP 2011176689 A JP2011176689 A JP 2011176689A JP 2013040116 A JP2013040116 A JP 2013040116A
- Authority
- JP
- Japan
- Prior art keywords
- vinyl ether
- group
- polymerization
- polymer
- represented
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
Description
よい1価の有機基を示す)
で表される可逆的付加開裂連鎖移動重合可能な部位を有する重合体である。
で示される酸付加物とすることができる。得られたこの酸付加物(11)は、リビングカチオン重合の開始種に用いることができる。
で示されるアルケニルエーテルを重合させることにより、次の式(2)
で表される本発明の連鎖移動可能重合体が得られる。
で表されるアリール基又はアリールアルキル基を挙げることができる。
(1)重量平均分子量Mw、数平均分子量Mn及び重量平均分子量と数平均分子量の比(Mw/Mn)は、ポリスチレンゲル換算のゲル濾過クロマトグラフィー(GPC)で測定した[RI検出器、カラム(東ソー(株)製TSKgelカラムGHR−M×3)、溶離液はテトラヒドロフラン]。
(2)1H NMRは、JEOL社製JMN AL−300を用い、サンプルを重クロロホルムに溶解して測定した。
S−ベンジル−O−(2−ビニロキシエチル)ジチオカーボナートの合成
以下の反応式に従い、下記の手順で合成した。
末端に可逆的付加開裂連鎖移動重合可能な部位を含有するイソブチルビニル
エーテルのリビングカチオン重合
実施例1で得られたS−ベンジル−O−(2−ビニロキシエチル)ジチオカーボナートを用い、イソブチルビニルエーテルのリビングカチオン重合を実施した。まず、S−ベンジル−O−(2−ビニロキシエチル)ジチオカーボナートをヘキサンに溶解し、40mmol/L溶液に調整した。その溶液に乾燥HClガスを吹き込み、S−ベンジル−O−(2−ビニロキシエチル)ジチオカーボナートの塩酸付加体ヘキサン溶液(40mmol/L)を調整した。
ポリイソブチルビニルエーテルとポリ酢酸ビニルのブロック共重合体の合成
実施例2で7分間重合して得られた、末端に可逆的付加開裂連鎖移動重合可能な部位を含有するポリイソブチルビニルエーテル0.397g、酢酸ビニル1.087g、アゾビスイソブチロニトリル2.0mgおよびトルエン1.612gを三方活栓付き試験管に加え、その試験管を脱気した後、窒素下、70℃に加温して重合した。
ベンジル(2−ビニロキシエチル)トリチオカーボナートの合成
以下の反応式に従い、下記の手順で合成した。
末端に可逆的付加開裂連鎖移動重合可能な部位を含有するイソブチルビニル
エーテルのリビングカチオン重合
実施例4で得られたベンジル(2−ビニロキシエチル)トリチオカーボナートを用い、イソブチルビニルエーテルのリビングカチオン重合を実施した。まず、ベンジル(2−ビニロキシエチル)トリチオカーボナートをヘキサンに溶解し、20mmol/L溶液に調整した。その溶液に乾燥HClガスを吹き込み、ベンジル(2−ビニロキシエチル)トリチオカーボナートの塩酸付加体ヘキサン溶液(20mmol/L)を調整した。
ポリイソブチルビニルエーテルとポリアクリル酸エチルのブロック共重合体
の合成
実施例5で7分間重合して得られた末端に可逆的付加開裂連鎖移動重合可能な部位を含有するポリイソブチルビニルエーテル0.094g、アクリル酸エチル0.33mL、アゾビスイソブチロニトリル0.5mgおよびトルエン1.845mLを三方活栓付き試験管に加え、その試験管を脱気した後、窒素下70℃に加温して重合した。
Claims (5)