JP2010159208A5 - - Google Patents

Info

Publication number
JP2010159208A5
JP2010159208A5 JP2010049663A JP2010049663A JP2010159208A5 JP 2010159208 A5 JP2010159208 A5 JP 2010159208A5 JP 2010049663 A JP2010049663 A JP 2010049663A JP 2010049663 A JP2010049663 A JP 2010049663A JP 2010159208 A5 JP2010159208 A5 JP 2010159208A5
Authority
JP
Japan
Prior art keywords
crystal particles
sodium
sodium hydrogen
hydrogen carbonate
aqueous solution
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP2010049663A
Other languages
English (en)
Other versions
JP2010159208A (ja
JP5062268B2 (ja
Filing date
Publication date
Application filed filed Critical
Priority to JP2010049663A priority Critical patent/JP5062268B2/ja
Priority claimed from JP2010049663A external-priority patent/JP5062268B2/ja
Publication of JP2010159208A publication Critical patent/JP2010159208A/ja
Publication of JP2010159208A5 publication Critical patent/JP2010159208A5/ja
Application granted granted Critical
Publication of JP5062268B2 publication Critical patent/JP5062268B2/ja
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Description

本発明は、上記の新規な知見に基づくもので、以下の構成を有するものである。
(1)平均粒子径50〜500μmの炭酸水素ナトリウム結晶粒子を、カリウム濃度が400質量ppm以下である炭酸水素ナトリウム含有水溶液の母液から析出させて製造し、前記母液から析出させた炭酸水素ナトリウム結晶粒子を、水または炭酸水素ナトリウム含有水溶液で水洗し、次いで、炭酸ガス濃度が3体積%以上の乾燥ガスを使用して該炭酸水素ナトリウム結晶粒子を乾燥せしめることにより、結晶粒子中のカリウム濃度が50質量ppm以下、かつ炭酸イオン濃度が炭酸ナトリウム換算で1質量%以下である炭酸水素ナトリウム結晶粒子を製造することを特徴とする固結性の小さい炭酸水素ナトリウム結晶粒子の製造方法。
(2)前記結晶粒子中のカリウム濃度が30質量ppm以下である、前記固結性の小さい炭酸水素ナトリウム結晶粒子の製造方法。
(3)前記炭酸水素ナトリウム含有水溶液が炭酸水素ナトリウムの飽和水溶液である、前記固結性の小さい炭酸水素ナトリウム結晶粒子の製造方法。

Claims (3)

  1. 平均粒子径50〜500μmの炭酸水素ナトリウム結晶粒子を、カリウム濃度が400質量ppm以下である炭酸水素ナトリウム含有水溶液の母液から析出させて製造し、前記母液から析出させた炭酸水素ナトリウム結晶粒子を、水または炭酸水素ナトリウム含有水溶液で水洗し、次いで、炭酸ガス濃度が3体積%以上の乾燥ガスを使用して該炭酸水素ナトリウム結晶粒子を乾燥せしめることにより、結晶粒子中のカリウム濃度が50質量ppm以下、かつ炭酸イオン濃度が炭酸ナトリウム換算で1質量%以下である炭酸水素ナトリウム結晶粒子を製造することを特徴とする固結性の小さい炭酸水素ナトリウム結晶粒子の製造方法。
  2. 前記結晶粒子中のカリウム濃度が30質量ppm以下である、請求項1に記載の固結性の小さい炭酸水素ナトリウム結晶粒子の製造方法。
  3. 記炭酸水素ナトリウム含有水溶液が炭酸水素ナトリウムの飽和水溶液である、請求項1または2に記載の固結性の小さい炭酸水素ナトリウム結晶粒子の製造方法。
JP2010049663A 2002-03-29 2010-03-05 固結性の小さい炭酸水素ナトリウム結晶粒子の製造方法 Expired - Fee Related JP5062268B2 (ja)