JP2008158252A5 - - Google Patents

Download PDF

Info

Publication number
JP2008158252A5
JP2008158252A5 JP2006346985A JP2006346985A JP2008158252A5 JP 2008158252 A5 JP2008158252 A5 JP 2008158252A5 JP 2006346985 A JP2006346985 A JP 2006346985A JP 2006346985 A JP2006346985 A JP 2006346985A JP 2008158252 A5 JP2008158252 A5 JP 2008158252A5
Authority
JP
Japan
Prior art keywords
toner
molecular weight
transmittance
integrated value
methanol
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP2006346985A
Other languages
English (en)
Japanese (ja)
Other versions
JP4909055B2 (ja
JP2008158252A (ja
Filing date
Publication date
Application filed filed Critical
Priority to JP2006346985A priority Critical patent/JP4909055B2/ja
Priority claimed from JP2006346985A external-priority patent/JP4909055B2/ja
Publication of JP2008158252A publication Critical patent/JP2008158252A/ja
Publication of JP2008158252A5 publication Critical patent/JP2008158252A5/ja
Application granted granted Critical
Publication of JP4909055B2 publication Critical patent/JP4909055B2/ja
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Links

JP2006346985A 2006-12-25 2006-12-25 トナー及びトナーの製造方法 Expired - Fee Related JP4909055B2 (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP2006346985A JP4909055B2 (ja) 2006-12-25 2006-12-25 トナー及びトナーの製造方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP2006346985A JP4909055B2 (ja) 2006-12-25 2006-12-25 トナー及びトナーの製造方法

Publications (3)

Publication Number Publication Date
JP2008158252A JP2008158252A (ja) 2008-07-10
JP2008158252A5 true JP2008158252A5 (cg-RX-API-DMAC7.html) 2010-02-12
JP4909055B2 JP4909055B2 (ja) 2012-04-04

Family

ID=39659217

Family Applications (1)

Application Number Title Priority Date Filing Date
JP2006346985A Expired - Fee Related JP4909055B2 (ja) 2006-12-25 2006-12-25 トナー及びトナーの製造方法

Country Status (1)

Country Link
JP (1) JP4909055B2 (cg-RX-API-DMAC7.html)

Families Citing this family (7)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP5268486B2 (ja) * 2008-08-06 2013-08-21 キヤノン株式会社 トナー
JP5473353B2 (ja) * 2009-02-23 2014-04-16 キヤノン株式会社 電子写真用トナー容器及び画像形成方法
JP5473354B2 (ja) * 2009-02-23 2014-04-16 キヤノン株式会社 電子写真用トナー容器及び画像形成方法
KR20130065336A (ko) * 2011-12-09 2013-06-19 삼성정밀화학 주식회사 정착성 및 광택성이 우수한 토너
JP6067981B2 (ja) 2012-03-15 2017-01-25 シャープ株式会社 粉砕トナーの製造方法
JP6471460B2 (ja) * 2014-11-04 2019-02-20 株式会社リコー トナー及びトナー製造方法
JP6552337B2 (ja) * 2015-08-26 2019-07-31 キヤノン株式会社 トナーの製造方法

Family Cites Families (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP3990839B2 (ja) * 1999-03-31 2007-10-17 キヤノン株式会社 トナー
JP3880325B2 (ja) * 2001-03-21 2007-02-14 キヤノン株式会社 磁性トナー、画像形成方法およびプロセスカートリッジ
JP4273054B2 (ja) * 2003-07-29 2009-06-03 キヤノン株式会社 トナー及び画像形成方法
JP4208784B2 (ja) * 2003-08-01 2009-01-14 キヤノン株式会社 トナー
JP4603802B2 (ja) * 2004-01-29 2010-12-22 キヤノン株式会社 カラートナー

Similar Documents

Publication Publication Date Title
Wang et al. Multiple H‐bonding cross‐linked supramolecular solid–solid phase change materials for thermal energy storage and management
TW536638B (en) Anti-reflection material and polarized film using the same
Rzayev et al. Nanochannel array plastics with tailored surface chemistry
Miguez et al. Evidence of FCC crystallization of SiO2 nanospheres
Asaoka et al. Normally oriented cylindrical nanostructures in amphiphilic PEO–LC diblock copolymers films
JP2008158252A5 (cg-RX-API-DMAC7.html)
Kato et al. Effect of topological constraint and confined motions on the viscoelasticity of polyrotaxane glass with different interactions between rings
EP3296325A1 (en) Elliptical, needle-shaped, or rod-shaped crosslinked polymer particles, and use thereof
JP2017171939A (ja) 扁平楕円状ポリマー粒子及びその用途
Martin et al. Tuning the wetting–dewetting and dispersion–aggregation transitions in polymer nanocomposites using composition of graft and matrix polymers
CN104995281A (zh) 光致变色固化性组合物
CN102533096B (zh) 可用于形成保护涂层的可辐射固化复合物涂料组合物
JP2007211164A5 (cg-RX-API-DMAC7.html)
JP2002146197A5 (cg-RX-API-DMAC7.html)
JP2010039291A5 (cg-RX-API-DMAC7.html)
Zhu et al. Preparation of PP/PC light‐diffusing materials with UV‐shielding property
JP2008299086A5 (cg-RX-API-DMAC7.html)
Liu et al. Poly (dimethylsiloxane) star polymers having nanosized silica cores
JP7414014B2 (ja) フレキシブルディスプレイ装置のカバーウィンドウおよびディスプレイ装置
JP2009276643A5 (cg-RX-API-DMAC7.html)
JP2012177057A (ja) 樹脂組成物、成形体及び光学用部材
Li et al. In situ formation of artificial moth-eye structure by spontaneous nano-phase separation
Seok et al. Structural effect of photoinitiators on electro‐optical properties of polymer‐dispersed liquid crystal composite films
JP2012083463A5 (cg-RX-API-DMAC7.html)
JP2019510119A (ja) 硬化性組成物、硬化物、および、光学部材