JP2003513167A5 - - Google Patents

Download PDF

Info

Publication number
JP2003513167A5
JP2003513167A5 JP2001533209A JP2001533209A JP2003513167A5 JP 2003513167 A5 JP2003513167 A5 JP 2003513167A5 JP 2001533209 A JP2001533209 A JP 2001533209A JP 2001533209 A JP2001533209 A JP 2001533209A JP 2003513167 A5 JP2003513167 A5 JP 2003513167A5
Authority
JP
Japan
Prior art keywords
sulfur
less
powder metallurgy
sulfide particles
toughness
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP2001533209A
Other languages
English (en)
Japanese (ja)
Other versions
JP2003513167A (ja
JP4941854B2 (ja
Filing date
Publication date
Priority claimed from US09/425,664 external-priority patent/US6238455B1/en
Application filed filed Critical
Publication of JP2003513167A publication Critical patent/JP2003513167A/ja
Publication of JP2003513167A5 publication Critical patent/JP2003513167A5/ja
Application granted granted Critical
Publication of JP4941854B2 publication Critical patent/JP4941854B2/ja
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Links

JP2001533209A 1999-10-22 2000-10-13 固結された粉末冶金物品、同物品から作られた鋼線及び同鋼線の製造方法 Expired - Lifetime JP4941854B2 (ja)

Applications Claiming Priority (3)

Application Number Priority Date Filing Date Title
US09/425,664 1999-10-22
US09/425,664 US6238455B1 (en) 1999-10-22 1999-10-22 High-strength, titanium-bearing, powder metallurgy stainless steel article with enhanced machinability
PCT/US2000/028342 WO2001031076A1 (en) 1999-10-22 2000-10-13 Machinable high strength stainless steel

Publications (3)

Publication Number Publication Date
JP2003513167A JP2003513167A (ja) 2003-04-08
JP2003513167A5 true JP2003513167A5 (enExample) 2011-04-07
JP4941854B2 JP4941854B2 (ja) 2012-05-30

Family

ID=23687520

Family Applications (1)

Application Number Title Priority Date Filing Date
JP2001533209A Expired - Lifetime JP4941854B2 (ja) 1999-10-22 2000-10-13 固結された粉末冶金物品、同物品から作られた鋼線及び同鋼線の製造方法

Country Status (13)

Country Link
US (1) US6238455B1 (enExample)
EP (1) EP1222317B1 (enExample)
JP (1) JP4941854B2 (enExample)
KR (1) KR100732433B1 (enExample)
AT (1) ATE240417T1 (enExample)
AU (1) AU1083201A (enExample)
BR (1) BR0015059A (enExample)
CA (1) CA2387880A1 (enExample)
DE (1) DE60002745T2 (enExample)
ES (1) ES2199184T3 (enExample)
IL (1) IL149084A (enExample)
MX (1) MXPA02003989A (enExample)
WO (1) WO2001031076A1 (enExample)

Families Citing this family (34)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US7235212B2 (en) 2001-02-09 2007-06-26 Ques Tek Innovations, Llc Nanocarbide precipitation strengthened ultrahigh strength, corrosion resistant, structural steels and method of making said steels
JP2002147467A (ja) * 2000-08-29 2002-05-22 Nsk Ltd 転がり支持装置
DE10251413B3 (de) * 2002-11-01 2004-03-25 Sandvik Ab Verwendung eines korrosionsbeständigen, martensitisch aushärtenden Stahls
US7901519B2 (en) * 2003-12-10 2011-03-08 Ati Properties, Inc. High strength martensitic stainless steel alloys, methods of forming the same, and articles formed therefrom
SE0300644L (sv) * 2003-03-07 2004-03-09 Sandvik Ab Användning av ett utskiljningshärdbart, martensitiskt rostfritt stål för tillverkning av implantat och osteosyntesprodukter
US7329383B2 (en) 2003-10-22 2008-02-12 Boston Scientific Scimed, Inc. Alloy compositions and devices including the compositions
SE528454C3 (sv) * 2004-12-23 2007-01-09 Sandvik Intellectual Property Utskiljningshärdbart martensitiskt rostfritt stål innefattande titansulfid
FR2887558B1 (fr) * 2005-06-28 2007-08-17 Aubert & Duval Soc Par Actions Composition d'acier inoxydable martensitique, procede de fabrication d'une piece mecanique a partir de cet acier et piece ainsi obtenue
US7780798B2 (en) 2006-10-13 2010-08-24 Boston Scientific Scimed, Inc. Medical devices including hardened alloys
SE531252C2 (sv) * 2007-06-12 2009-02-03 Sandvik Intellectual Property Krockbalk av utskiljningshärdat stål
JP5270926B2 (ja) * 2008-02-20 2013-08-21 三菱製鋼株式会社 鉄基焼結合金粉末
WO2010029505A2 (en) * 2008-09-12 2010-03-18 L. Klein Ag Free-machining powder metallurgy lead-free steel articles and method of making same
CN102203300B (zh) * 2008-10-31 2013-08-07 Crs控股公司 超高强度不锈合金带、其制备方法和使用其制备高尔夫球棍头的方法
FR2947565B1 (fr) * 2009-07-03 2011-12-23 Snecma Traitement cryogenique d'un acier martensitique a durcissement mixte
DE102010025287A1 (de) * 2010-06-28 2012-01-26 Stahlwerk Ergste Westig Gmbh Chrom-Nickel-Stahl
JP6113456B2 (ja) * 2012-10-17 2017-04-12 三菱日立パワーシステムズ株式会社 析出硬化型マルテンサイト系ステンレス鋼とそれを用いた蒸気タービン長翼
US20140161658A1 (en) * 2012-12-06 2014-06-12 Crs Holdings, Inc. High Strength Precipitation Hardenable Stainless Steel
US10094007B2 (en) * 2013-10-24 2018-10-09 Crs Holdings Inc. Method of manufacturing a ferrous alloy article using powder metallurgy processing
US20170279128A1 (en) * 2014-09-26 2017-09-28 Sandvik Intellectual Property Ab Bipolar fuel cell plate
ES2691992T3 (es) 2015-11-09 2018-11-29 Crs Holdings, Inc. Artículos de acero de pulvimetalurgia de maquinado libre y método de preparación de los mismos
CN107653421B (zh) * 2016-07-26 2019-12-10 中国科学院金属研究所 一种耐海水腐蚀的超高强度马氏体时效不锈钢
US20210032719A1 (en) * 2017-09-07 2021-02-04 Suzuki Garphyttan Ab Method of producing a cold drawn wire
DE102017131218A1 (de) 2017-12-22 2019-06-27 Voestalpine Böhler Edelstahl Gmbh & Co Kg Verfahren zum Herstellen eines Gegenstands aus einem Maraging-Stahl
DE102017131219A1 (de) 2017-12-22 2019-06-27 Voestalpine Böhler Edelstahl Gmbh & Co Kg Verfahren zum Herstellen eines Gegenstands aus einem Maraging-Stahl
CN108165870B (zh) * 2018-01-19 2019-06-18 天津荣程联合钢铁集团有限公司 一种钢锻件及其加工方法
CN108300936B (zh) * 2018-01-19 2019-05-17 天津荣程联合钢铁集团有限公司 一种抗压耐腐蚀钢锻件及其加工方法
US11692232B2 (en) 2018-09-05 2023-07-04 Gregory Vartanov High strength precipitation hardening stainless steel alloy and article made therefrom
KR20210079294A (ko) 2018-09-24 2021-06-29 팔스 베지츠 게엠베하 비용 효율적이며 기하학적으로 복잡한 피스를 얻기 위한 방법
MX2022007592A (es) * 2019-12-20 2022-07-19 Arcelormittal Proceso para la fabricacion de aditivo de aceros martensiticos.
US11702714B2 (en) 2020-02-26 2023-07-18 Crs Holdings, Llc High fracture toughness, high strength, precipitation hardenable stainless steel
CN119980085A (zh) * 2020-08-24 2025-05-13 华为技术有限公司 钢、钢结构件、电子设备及钢结构件的制备方法
EP3967423A1 (en) 2020-09-11 2022-03-16 Questek Innovations LLC Stainless steel powders for additive manufacturing
US12084752B2 (en) 2021-11-01 2024-09-10 Questek Innovations Llc Stainless steel powders for additive manufacturing
CN116970878B (zh) * 2023-08-07 2025-04-25 浙江全鼎磁电材料有限公司 高韧性高强度马氏体不锈钢、钢结构件及其制备方法与应用

Family Cites Families (11)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US3622307A (en) * 1968-05-15 1971-11-23 Armco Steel Corp Precipitation-hardenable chromium-nickel stainless steel
US3696486A (en) * 1969-08-25 1972-10-10 Int Nickel Co Stainless steels by powder metallurgy
SE469986B (sv) * 1991-10-07 1993-10-18 Sandvik Ab Utskiljningshärdbart martensitiskt rostfritt stål
US5720300A (en) * 1993-11-10 1998-02-24 C. R. Bard, Inc. High performance wires for use in medical devices and alloys therefor
JPH07138713A (ja) * 1993-11-15 1995-05-30 Daido Steel Co Ltd Fe基合金粉末及び高耐食性焼結体の製造方法
JP2980004B2 (ja) * 1995-08-07 1999-11-22 株式会社神戸製鋼所 バーリング加工性および打ち抜き加工性に優れた冷延鋼板とその製法
JPH08218118A (ja) * 1995-02-13 1996-08-27 Sumitomo Metal Ind Ltd 粒子微細分散型高ヤング率鋼材の製造方法
JPH08337853A (ja) * 1995-06-09 1996-12-24 Hitachi Ltd 高耐食性高強度オーステナイト焼結鋼とその製造方法及びその用途
US5681528A (en) * 1995-09-25 1997-10-28 Crs Holdings, Inc. High-strength, notch-ductile precipitation-hardening stainless steel alloy
JP3446449B2 (ja) * 1996-02-20 2003-09-16 Jfeスチール株式会社 耐リジング性に優れたフェライト系ステンレス鋼板
DE69718784T2 (de) * 1996-11-25 2003-12-18 Sumitomo Metal Industries, Ltd. Stahl mit hervorragender verarbeitbarkeit und damit hegestelltes bauteil

Similar Documents

Publication Publication Date Title
JP2003513167A5 (enExample)
ATE240417T1 (de) Hochfester rostfreier automatenstahl
USRE47529E1 (en) Fe-base in-situ composite alloys comprising amorphous phase
EP1825013B1 (en) Improved wear resistant alloy
TW200626731A (en) Cemented carbides
Bedolla-Jacuinde et al. Eutectic modification in a low-chromium white cast iron by a mixture of titanium, rare earths, and bismuth: I. Effect on microstructure
EP1361288A4 (en) HYDROESISTING COPPER ALLOY
CA2359188A1 (en) High-hardness powder metallurgy tool steel and article made therefrom
PL350819A1 (en) An enhanced machinability precipitation-hardenable stainless steel for critical applications
JPH0414182B2 (enExample)
JPH10298684A (ja) 強度、耐摩耗性及び耐熱性に優れたアルミニウム基合金−硬質粒子複合材料
Bihari et al. Effect on the mechanical properties of gray cast iron with variation of copper and molybdenum as alloying elements
JP2000192198A5 (enExample)
JPS6053098B2 (ja) 高強度および高靭性を有する耐摩耗性Cu合金
JPS6045267B2 (ja) 快削合金鋳鉄
JP2007002333A5 (enExample)
JPS6053097B2 (ja) 高強度および高靭性を有する耐摩耗性Cu合金
CN100447277C (zh) 一种铁铌硅合金
JP4047197B2 (ja) Ni基ホウ化物分散耐食耐摩耗性合金
JPS6393840A (ja) 低熱膨張鋳鉄
JPS6330379B2 (enExample)
JPS5910989B2 (ja) 快削性含クロム鋳鉄
Hsu et al. Fracture mechanics behaviour of austenitic compacted graphite cast iron
Ana-Marija et al. Effect of inoculation, cooling rate and charge composition on gray iron microstructure
JPH08120396A (ja) 鋳放しパーライト球状黒鉛鋳鉄及びその製造方法