JP2002307427A5 - - Google Patents
Download PDFInfo
- Publication number
- JP2002307427A5 JP2002307427A5 JP2001115604A JP2001115604A JP2002307427A5 JP 2002307427 A5 JP2002307427 A5 JP 2002307427A5 JP 2001115604 A JP2001115604 A JP 2001115604A JP 2001115604 A JP2001115604 A JP 2001115604A JP 2002307427 A5 JP2002307427 A5 JP 2002307427A5
- Authority
- JP
- Japan
- Prior art keywords
- seconds
- resin
- die
- melt
- weight
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
- 238000004898 kneading Methods 0.000 description 7
- 229920006038 crystalline resin Polymers 0.000 description 5
- 229920005989 resin Polymers 0.000 description 5
- 239000011347 resin Substances 0.000 description 5
- 239000000203 mixture Substances 0.000 description 4
- 239000011342 resin composition Substances 0.000 description 4
- 239000011159 matrix material Substances 0.000 description 3
- 238000000034 method Methods 0.000 description 3
- 238000001125 extrusion Methods 0.000 description 2
- 239000000155 melt Substances 0.000 description 2
- 229920006122 polyamide resin Polymers 0.000 description 2
- 238000002844 melting Methods 0.000 description 1
- 230000008018 melting Effects 0.000 description 1
- 229920001955 polyphenylene ether Polymers 0.000 description 1
- 239000012779 reinforcing material Substances 0.000 description 1
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP2001115604A JP4674989B2 (ja) | 2001-04-13 | 2001-04-13 | 物性が良好な混練方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP2001115604A JP4674989B2 (ja) | 2001-04-13 | 2001-04-13 | 物性が良好な混練方法 |
Publications (3)
| Publication Number | Publication Date |
|---|---|
| JP2002307427A JP2002307427A (ja) | 2002-10-23 |
| JP2002307427A5 true JP2002307427A5 (enExample) | 2008-05-22 |
| JP4674989B2 JP4674989B2 (ja) | 2011-04-20 |
Family
ID=18966475
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP2001115604A Expired - Lifetime JP4674989B2 (ja) | 2001-04-13 | 2001-04-13 | 物性が良好な混練方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JP4674989B2 (enExample) |
Families Citing this family (7)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP2005194291A (ja) | 2001-12-04 | 2005-07-21 | Asahi Kasei Corp | ポリフェニレンエーテル樹脂組成物 |
| US7547403B2 (en) | 2003-07-02 | 2009-06-16 | Polyplastics Co., Ltd. | Electroconductive resin composition |
| JP2010179627A (ja) * | 2009-02-09 | 2010-08-19 | Sekisui Plastics Co Ltd | 発泡性熱可塑性樹脂粒子の製造方法、熱可塑性樹脂発泡粒子の製造方法及び熱可塑性樹脂発泡成形体の製造方法 |
| TW201127889A (en) * | 2009-11-30 | 2011-08-16 | Sekisui Plastics | Foamable thermoplastic resin particle and production method thereof |
| JP5543806B2 (ja) * | 2010-03-09 | 2014-07-09 | 旭化成ケミカルズ株式会社 | 熱可塑性樹脂組成物及び製造方法 |
| CN104053696B (zh) | 2011-12-26 | 2015-07-08 | 胜技高分子株式会社 | 聚对苯二甲酸丁二醇酯树脂颗粒、以及该聚对苯二甲酸丁二醇酯树脂颗粒的制造方法 |
| JPWO2013121692A1 (ja) * | 2012-02-17 | 2015-05-11 | パナソニックIpマネジメント株式会社 | フィラーの分散方法及びマイクロ分散ミキサー |
Family Cites Families (8)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS48100454A (enExample) * | 1972-04-03 | 1973-12-18 | ||
| JP2882689B2 (ja) * | 1991-01-17 | 1999-04-12 | 旭化成工業株式会社 | 樹脂組成物の製造方法 |
| JP3701392B2 (ja) * | 1995-06-28 | 2005-09-28 | 旭化成ケミカルズ株式会社 | 押出方法 |
| JPH10180841A (ja) * | 1996-12-25 | 1998-07-07 | Asahi Chem Ind Co Ltd | 粉体のサイドフィード用押出機及びそれを用いた押出方法 |
| JP3374698B2 (ja) * | 1997-03-18 | 2003-02-10 | 住友化学工業株式会社 | 熱可塑性樹脂押出製品の製造方法 |
| JPH10310647A (ja) * | 1997-05-13 | 1998-11-24 | Asahi Chem Ind Co Ltd | オレフィン系熱可塑性エラストマー用押出機及びそれを用いた製造方法 |
| JP2000063664A (ja) * | 1998-08-25 | 2000-02-29 | Ube Ind Ltd | ポリアミド系樹脂組成物 |
| JP4116192B2 (ja) * | 1999-05-14 | 2008-07-09 | 富士フイルム株式会社 | 多層樹脂フィルムの製造法 |
-
2001
- 2001-04-13 JP JP2001115604A patent/JP4674989B2/ja not_active Expired - Lifetime
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JP2002307427A5 (enExample) | ||
| JP2002504584A5 (enExample) | ||
| WO2002098391A3 (en) | Process for preparing granular compositions | |
| JP2001525472A5 (enExample) | ||
| EP1341049A3 (en) | Dry toner composition | |
| RU2009128238A (ru) | Способ изготовления композиций порошкового противомикробного покрытия | |
| EP0230815B1 (fr) | Compositions thermoplastiques à base de polyétheramides et de copolymeres styrène-diène et leur procédé de fabrication | |
| JP2002316316A5 (enExample) | ||
| JPH09239726A (ja) | タンデム型混練装置及びそれを用いた熱可塑性樹脂及び/又はゴムの混練方法 | |
| CA2271862A1 (en) | Polymer mixture for slush molding | |
| CN107849241B (zh) | 制备聚合物组合物的方法以及通过所述方法能够获得的聚合物组合物 | |
| JP2022127843A5 (enExample) | ||
| CN120118424A (zh) | 聚丙烯复合材料及其制备方法和汽车内外饰件 | |
| JP3365711B2 (ja) | 中空成形用水溶性コア | |
| JP2002166421A (ja) | 廃棄オレフィンフィルムからの再生ペレット製造方法 | |
| US6884836B2 (en) | Polyolefin based resin film and a composition for a polyolefin type resin film | |
| JPH10100224A (ja) | 電池用セパレータの製造方法 | |
| CN116348541A (zh) | 液晶聚合物组合物、制品和制备方法 | |
| JP4881111B2 (ja) | 押出成形品の製造方法 | |
| JP2005335240A5 (enExample) | ||
| EP0086686B1 (fr) | Nouvelle composition thermoplastique à mémoire à base de polycaprolactone et de polychloroprène, son procédé de préparation et son utilisation notamment en orthopédie | |
| JP2818501B2 (ja) | 成形用結晶性ポリアリーレンサルファイド樹脂材料及びその調製法 | |
| JP2003053821A5 (enExample) | ||
| JP2864391B2 (ja) | 過共晶A▲l▼―Si系合金複合材料とその製造方法 | |