JP2002059254A - 溶解容器内の溶融金属の酸化抑制方法及び装置 - Google Patents
溶解容器内の溶融金属の酸化抑制方法及び装置Info
- Publication number
- JP2002059254A JP2002059254A JP2000241423A JP2000241423A JP2002059254A JP 2002059254 A JP2002059254 A JP 2002059254A JP 2000241423 A JP2000241423 A JP 2000241423A JP 2000241423 A JP2000241423 A JP 2000241423A JP 2002059254 A JP2002059254 A JP 2002059254A
- Authority
- JP
- Japan
- Prior art keywords
- molten metal
- supply
- melting vessel
- oxygen concentration
- injection
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
酸素濃度の計測監視の下に、金属材料の加熱と供給の両
方の停止により防止する。 【解決手段】 ノズル部材2と連通する計量室4を先端
部内に有し、回転自在な攪拌部材8と、その攪拌部材8
を貫通して先端の射出プランジャ12を計量室4に進退
自在に挿入した射出部材9とを内部に備える溶解容器1
を、ノズル部材2を下側にして斜めに設置して金属材料
を溶解する。溶解容器1の溶湯面15aより上の空間部
位を不活性ガス雰囲気となす。空間部位の酸素濃度を計
測監視する。計測した酸素濃度が設定基準値を超えたと
きにエラーとして、加熱と材料供給とを停止して溶融金
属の酸化を防止する。
Description
ウム又はそれら合金等の低融点の非鉄金属を、溶解容器
内で溶解して射出成形する場合の金属材料の酸化を防止
する方法と装置に関するものである。
には、大気中の酸素が付着又は吸着或いは酸化表層とし
てまといついていることと、供給時に金属材料と一緒に
大気中の酸素が送り込まれ易いことなどから、そのまま
溶解容器内で加熱溶解すると、溶解容器内の溶融金属で
あっても酸化が生じ易い。
金属飛沫が不純物である酸化スラッジとして、容器内壁
や攪拌部材等に付着して積もり、これが攪拌部材やプラ
ンジャの動作不良の原因となったり、あるいは溶湯面の
酸化物と共に不純物となって溶融金属に混じり込み、射
出成形された金属製品の品質低下の要因ともなってい
る。
酸素を、材料供給時に真空ポンプにより吸引して排除し
て、溶解容器内の酸素濃度の低減を図ったり、或いはア
ルゴン等の不活性ガスを溶解容器内に常時供給し、金属
材料の加熱溶解を不活性ガス雰囲気中で行うようにして
酸化を抑制したりしているが、自然の状態で生じた金属
材料の表面酸化による酸素については、それが微量であ
ることと、これといった排除手段もないことから、その
まま金属材料を加熱溶解している。
溶解を行ってゆくと、不活性ガス雰囲気中でありなが
ら、溶解容器内の酸素濃度が増して溶湯面が酸化し易く
なる。この酸素濃度の増加については、上記表面酸化に
よる酸素の存在も一因とされ、それが微量なものであつ
ても、溶解容器内に残る量は金属材料の供給量に比例し
て増し、いずれは酸素濃度の規定値を超えることになる
ので、これを何らかの手段をもって規定値以下に低減す
ることが切望されている。
の課題を、不活性ガス雰囲気中の酸素濃度の計測監視の
下に、金属材料の加熱と供給の両方を停止することによ
って解決することができる新たな溶融容器内の溶融金属
の酸化防止方法及び装置とを提供することにある。
の酸化防止方法は、ノズル部材と連通する計量室を先端
部内に有し、回転自在な攪拌部材と、その攪拌部材を貫
通して先端の射出プランジャを上記計量室に進退自在に
挿入した射出部材とを内部に備え、上記ノズル部材を下
側にして斜めに設置した溶解容器により金属材料を溶解
するにあたり、上記溶解容器の溶湯面より上の空間部位
を不活性ガス雰囲気となし、その空間部位の酸素濃度を
計測監視して、計測した酸素濃度が設定基準値を超えた
ときにエラーとして、加熱と材料供給とを停止して溶融
金属の酸化を防止してなる、というものである。
材と連通する計量室を先端部内に有し、回転自在な攪拌
部材と、その攪拌部材を貫通して先端の射出プランジャ
を上記計量室に進退自在に挿入した射出部材とを内部に
備え、上記ノズル部材を下側にして斜めに設置した溶解
容器の供給口に供給筒を立設し、その供給筒に粒状の金
属材料の供給装置を接続するとともに、上記溶解容器の
溶湯面より上の空間部位に不活性ガスを供給するガス管
路を供給筒内又は上側部に配設し、その供給筒の上部の
上記供給装置に、発信機能を有する酸素検知装置を供給
筒内に酸素センサを臨ませて取付けてなる、というもの
である。
外周囲にバンドヒータ3を備える円筒体からなる。この
溶解容器1は先端に設けたノズル部材2を下側にして、
型締装置(図は省略)に対し45°の角度で斜めに設置
されている。またノズル部材2と連通する溶解容器1の
先端部内は、容器内径よりも小径に縮径した所要長さの
計量室4に形成してある。
設してあり、その供給口5に立設した供給筒7に金属材
料の供給装置6が、溶解容器1に取付けた部材16によ
り保持して接続してある。また溶解容器1の後端は開口
状態にあって、その後端から攪拌及び射出手段を構成す
る溶融金属15の攪拌部材8と射出部材9とが内設して
ある。
攪拌翼10を断続的に旋回形成した回転軸からなる。こ
の攪拌翼10は溶解容器1の内径とほば等しい外径から
なり、また攪拌翼10よりも後方の軸部周囲には、溶解
容器1の内周面と接したガイド兼用の仕切用フランジ1
1が一体形成してある。
摺動自在に設けたロッド先端に、攪拌部材8の前面から
上記計量室4に嵌合した射出プランジャ12を有し、そ
の射出プランジャ12と共に前進移動して、計量室4に
蓄えた所定量の溶融金属15をノズル部材2から、図示
しない金型に射出充填する。
路で圧力容器14と接続している。このガス管路13
は、上記供給筒7の上側部から内部を通して、供給口5
より下側の攪拌翼10の近傍に開口端13aを位置させ
るか、または鎖線で示すように供給筒7の上側部に開口
端13aを接続するかして溶解容器1に設けてある。ま
たガス管路13の圧力容器14の近傍には減圧弁17と
流量弁18が配設してあり、これにより圧力容器14に
充填された不活性ガスの流出圧力及び流量をコントロー
ルできるようにしてある。
にスクリュコンベア62を備え、そのスクリュコンベア
62をシリンダ後端の電動モータ63により回転して、
シリンダ後部上側の投入口64から、シリンダ前部下側
の送出口65に接続した上記供給筒7に、粒状の金属材
料を移送する構造からなり、その供給筒7の上部のシリ
ンダ61の前部上に通孔66を開設して、発信機能を有
する酸素検知装置20が、酸素センサ19を通孔66か
ら供給筒7内に臨ませて取付けてある。
が、上記バンドヒータ3のヒータ電源と、供給装置6の
モータ電源の両方と電気的に接続され、それらの電源は
酸素検知装置20から出力された電気信号の入力により
OFF作動するように設定されている。
管路13を経て不活性ガスが溶解容器1の溶湯面15a
の上に噴出するか、または供給筒7内に噴出して、溶解
容器1内の空間部位を不活性ガス雰囲気となす。これに
より溶解容器1内に酸素が取り込まれていても、溶解し
た金属材料の酸化が防止される。また溶解容器1に供給
された不活性ガスの一部は、溶解容器1が斜設されてい
ることから、溶解容器1の上方の隙間又は供給装置6の
上記投入口64から排出される。これにより上部からの
溶解容器1内への大気の侵入が防止され、また供給装置
6でも不活性ガス雰囲気で金属材料の移送が行われるの
で、投入口64からの大気の侵入も防止されることにな
り、酸化原因となる酸素の侵入は金属材料の酸化表面の
微量な酸素のみとなる。
は、上記酸素検知装置20の酸素センサ19によりその
濃度が常に計測され、計測された酸素濃度が設定基準値
(たとえば10ppm )以下であれば、供給装置6による
材料供給と、ヒータによる加熱溶解作業とが継続され
て、上記射出プランジャ12の進退移動による溶融金属
の計量と金型への射出充填が行われる。
酸素濃度が規定の10ppm を超えると、酸素検知装置2
0がエラー信号を出力する。この出力信号により上記バ
ントヒータ3のヒータ電源がOFFとなって加熱停止と
なり、同時に上記供給装置6のモーター電源もOFFと
なって材料供給を停止して、アルゴンガスの供給のみが
続けられる。
料の表面にまといついている酸素も溶解容器1内に入り
込むことがないので、酸素濃度が規定以下に抑えられる
ようになる。また加熱停止により溶融金属の温度も抑え
られるようになる。この加熱停止と供給停止により酸素
濃度が設定基準値以下となると、再びヒータ電源とモー
ター電源の両方がON作動して加熱と材料供給とが再開
され、新たな金属材料の溶解が開始される。
された金属材料の酸化、特に溶湯面や飛沫となって空間
部位の壁面や部材に付着したスラッジの酸化が抑制さ
れ、スラッジが溶湯面に落ちて攪拌により溶融金属に混
入しても、酸化不純物としての混入は免れるので、溶融
金属を金型に射出して成形した金属製品でありながら、
高品質で成形精度の高いものとなる。また溶解及び射出
成形過程においても、固く蓄積した酸化スラッジによる
攪拌部材や射出部材の作動不良が防止され、長時間にわ
たる成形であっても酸化物による不都合が解消されて、
安定した成形を長く維持することが可能となる。
防止方法の実施を可能とする装置の概略図である。
Claims (2)
- 【請求項1】 ノズル部材と連通する計量室を先端部内
に有し、回転自在な攪拌部材と、その攪拌部材を貫通し
て先端の射出プランジャを上記計量室に進退自在に挿入
した射出部材とを内部に備え、上記ノズル部材を下側に
して斜めに設置した溶解容器により金属材料を溶解する
にあたり、 上記溶解容器の溶湯面より上の空間部位を不活性ガス雰
囲気となし、その空間部位の酸素濃度を計測監視して、
計測した酸素濃度が設定基準値を超えたときにエラーと
して、加熱と材料供給とを停止して溶融金属の酸化を防
止してなることを特徴とする溶融容器内の溶融金属の酸
化防止方法。 - 【請求項2】 ノズル部材と連通する計量室を先端部内
に有し、回転自在な攪拌部材と、その攪拌部材を貫通し
て先端の射出プランジャを上記計量室に進退自在に挿入
した射出部材とを内部に備え、上記ノズル部材を下側に
して斜めに設置した溶解容器の供給口に供給筒を立設
し、その供給筒に粒状の金属材料の供給装置を接続する
とともに、上記溶解容器の溶湯面より上の空間部位に不
活性ガスを供給するガス管路を供給筒内又は上側部に配
設し、その供給筒の上部の上記供給装置に、発信機能を
有する酸素検知装置を供給筒内に酸素センサを臨ませて
取付けてなることを特徴とする溶融容器内の溶融金属の
酸化防止装置。