JP2000334583A - 摩擦攪拌接合部の補修方法 - Google Patents
摩擦攪拌接合部の補修方法Info
- Publication number
- JP2000334583A JP2000334583A JP11145759A JP14575999A JP2000334583A JP 2000334583 A JP2000334583 A JP 2000334583A JP 11145759 A JP11145759 A JP 11145759A JP 14575999 A JP14575999 A JP 14575999A JP 2000334583 A JP2000334583 A JP 2000334583A
- Authority
- JP
- Japan
- Prior art keywords
- bead
- welding
- joining
- repair
- friction stir
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
造体を製造する際の接合部の補修方法の改良を図る。 【解決手段】 アルミ合金材であるA6N01材を母材
として、中空押出し成型された第1の部材20と第2の
部材30を接合部40に沿って摩擦攪拌接合を施した接
合ビード50を形成する。この接合ビード50に欠陥が
存在するときには、この欠陥を含むビードを研削加工に
より除去して、補修領域を形成する。この補修領域に対
してTIG溶接により補修ビードを加工する。このTI
G溶接の溶接棒を部材の母材と同じ材質でつくり、ビー
ドの組成を均一とする。摩擦攪拌接合部にヘアライン加
工を施すと、部材との境目と欠陥の痕跡の目立たない、
美感の高い表面を得ることができる。
Description
る補修方法に関するものである。
丸棒(回転工具という。)を回転させながら接合線に沿
って移動させ、接合部を発熱、軟化させ、塑性流動さ
せ、固相接合する方法である。回転工具は、接合部に挿
入する小径部と、外部に位置する大径部とからなる。小
径部と大径部は同軸である。小径部と大径部との境は接
合部に若干挿入されている。回転工具は接合の進行方向
に対して、後方に傾斜させている。
する側の表面に凸部が形成される。このため、接合部で
は板厚の減少となる。これを防止するため、被接合部材
の端部に回転工具側に突出する凸部を設け、これを含め
て摩擦攪拌接合している。また、凸部に替えて第3の板
を配置して摩擦攪拌接合している
の面板に直交する支え板を一体に設け、摩擦攪拌接合の
力によって面板が曲がることを防止している。これは特
開平9−309164号公報(EP0797043A
2)に示されている。
の側構体を接合する技術を示す。側構体の構造部材は、
例えばアルミ合金材(A6N01材)を押出し成型して
製作した帯状の押出し形材(部材)20,30を互の側
縁部で接合させ、この接合線40に沿って摩擦攪拌接合
を施して接合ビード50を形成する。次に、接合ビード
50を検査し、欠陥がなければそのままに、また欠陥が
発見されれば欠陥を補修した後に、ヘアライン加工等を
施して美感のある表面を形成する。
の接合線40に沿って摩擦攪拌接合を施して、接合ビー
ド50を形成した状態を示す。この接合ビード50を、
例えば超音波探傷検査等により検査し、図5の欠陥60
が発見されたものとする。尚、図1から図7(図3を除
く)において凸部 の端部の線は除いて示している。
を示す。第1の部材20と第2の部材30は、アルミ合
金材であるA6N01材を母材として押出し加工により
つくられている。この部材20,30に摩擦攪拌接合を
施して形成される接合ビード50も母材と同じA6N0
1材を成分となる。このビード50の欠陥を除去するた
めに欠陥部を含めてグラインダ等の工具により、加工を
施し、補修領域70を形成する。
を形成する。このMIG溶接には、MIG溶接に適した
溶接ワイヤが用いられている。この溶接ワイヤの材質
は、A5356規格の材料が用いられる。
合部にヘアライン加工52を施した状態を示す。ヘアラ
イン加工部52は、部材20,30の表面に対して同質
性の高い表面を有し、無塗装のままで、車両の側構体と
して使用することができる。
拌接合による接合ビードをMIG溶接して補修した接合
ビードにヘアライン加工を施すと、補修部82の表面
が、周囲の表面に対して異なる外観を示す。この補修部
の外観は、無塗装のままで車両の側構体として接合部材
を使用する際に、美観上問題となる。本発明は、上述し
た問題を解消する摩擦攪拌接合部の補修方法を提供する
ものである。
て形成した接合部の補修方法は、接合ビードに含まれる
欠陥を研削加工により除去して補修領域を形成する工程
と、形成された補修領域に部材の母材と同材料の溶接棒
を用いてTIG溶接によって補修ビードを形成する工程
とを備えるものである。そして、補修ビードと接合ビー
ドを含む接合部にヘアライン加工を施す工程を備えるこ
とができるものである。
攪拌接合の補修方法を示す。車両の側構体を構成する押
出し形材の第1の部材20と第2の部材30の接合部4
0に、摩擦攪拌接合を施して接合ビード50を形成す
る。
おいて、第1の部材20の凸部22と、第2の凸部32
の側端部を突き合わせて、摩擦攪拌接合によるビード5
0を形成する。
の外面として使用する場合には、接合された凸部を研削
加工等により平坦面54にして使用する。反対面を外側
にする場合には、接合された凸部はそのままにしておい
てもよい。この接合ビード50は、部材20,30の母
材であるA6N01材と同様の材質で形成される。
査は凸部が残っている状態で行っても、凸部を切削して
から行ってもよい。検査の結果、接合ビード50に割れ
やピット等の欠陥が発見されると、この欠陥を含む周囲
の接合ビード50をグラインダで除去(研削)して、補
修領域70を形成する。
0にTIG溶接により補修ビード100を形成する。つ
まり、肉盛り溶接する。このTIG溶接に当り、溶接棒
として母材と同じA6N01材の溶接棒を用意し、溶接
を行う。このA6N01材の溶接棒は母材の押出し形
(部材)20,30の余材を切断して製作したものであ
る。この溶接により、接合ビード50と補修ビード10
0は、同じ材料で形成されることとなる。TIG溶接
は、電極と溶接棒が異なるので、母材と同材質の材料を
容易に溶接棒にできる。
面にエアライン加工を行う。したがって、この接合ビー
ド部にヘアライン加工を施して得たヘアライン加工部5
4には、補修ビード100の痕跡は残らず品質の高い表
面を得ることができる。したがって、美感のよい車両を
構成することができる。
とき、溶接ワイヤはA5356材を使用している。この
組合せは溶接ワイヤメーカの推奨である。この組合せ
が、溶接強度、施行等の点から最もよい。形材:A6N
01材、溶接ワイヤ:A6N01材の組合せは、ワイ
ヤ:A6N01材が市販されていない。また、この両者
の組合せは溶接強度:溶接性等から除かれている。そこ
で、本発明では、A6N01材の余材を切断して、溶接
棒とした。
した後、行う場合がある。中空形材の場合で、両面に接
合部がある場合、上記TIG溶接はヘアライン加工を行
う外面の補修に用いる。内面側の補修は通材の材料であ
るA5356規格の材料の溶接ワイヤを用いたMIG溶
接を用いる。
をベットに近接して摩擦攪拌接合をすると、図10の部
材20,30の下面側の面は平滑に仕上がる。この面を
車両側の外面とし、エアライン加工を行う場合がある。
この接合ビードの補修を図10の下面側から行う場合に
も、上記TIG溶接による補修ができる。その後、補修
ビードを研削して平滑にする。
中空押出し成型してつくられる部材を摩擦攪拌接合によ
り接合してアルミ製の車両等の構造部材を構成する際
に、摩擦攪拌接合による接合ビードの欠陥を補修する際
に、欠陥部を研削加工等により除去して補修領域を形成
し、この補修領域に部材と同材質の溶接棒を用いて、T
IG溶接して補修ビードを形成するものである。
ドは同じ材質で形成されるので、ビードにヘアライン加
工を施したときに、補修ビードの痕跡は残らず、美感の
高い接合表面を得ることができる。したがって、無塗装
のままで、車両等を構成することができ、軽量化ととも
にリサイクルにも適した構造体を得ることができる。
図。
図。
図。
図。
図。
図。
明図。
Claims (2)
- 【請求項1】 アルミ合金を母材とする部材を摩擦攪拌
して形成した接合部の補修方法であって、 接合ビードに含まれる欠陥を研削加工により除去して補
修領域を形成する工程と、 形成された補修領域に部材の母材と同材料の溶接棒を用
いてTIG溶接によって補修ビードを形成する工程と、 を備える摩擦攪拌接合部の補修方法。 - 【請求項2】 補修ビードと接合ビードを含む接合部に
ヘアライン加工を施す工程を備える請求項1記載の摩擦
攪拌接合部の補修方法。