JP2000192348A5 - - Google Patents

Download PDF

Info

Publication number
JP2000192348A5
JP2000192348A5 JP1999286316A JP28631699A JP2000192348A5 JP 2000192348 A5 JP2000192348 A5 JP 2000192348A5 JP 1999286316 A JP1999286316 A JP 1999286316A JP 28631699 A JP28631699 A JP 28631699A JP 2000192348 A5 JP2000192348 A5 JP 2000192348A5
Authority
JP
Japan
Prior art keywords
yarn
denier
twisted
less
shrinkage
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP1999286316A
Other languages
English (en)
Other versions
JP2000192348A (ja
JP4278796B2 (ja
Filing date
Publication date
Application filed filed Critical
Priority to JP28631699A priority Critical patent/JP4278796B2/ja
Priority claimed from JP28631699A external-priority patent/JP4278796B2/ja
Publication of JP2000192348A publication Critical patent/JP2000192348A/ja
Publication of JP2000192348A5 publication Critical patent/JP2000192348A5/ja
Application granted granted Critical
Publication of JP4278796B2 publication Critical patent/JP4278796B2/ja
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Description

【請求項1】 単繊維繊度が2デニール以上の高収縮性ポリエステルフィラメント糸と単繊維繊度が3デニール以下の低収縮性ポリエステルフィラメント糸からなる、繊度が140〜200デニールの異収縮混繊糸に撚係数A(A=T・D1/2、T:撚糸数(回/m)、D:デ ニール)が8000〜23000の撚りが施された撚糸であって、撚り止め熱セット後の125℃での乾熱収縮率が4%以上、125℃での熱応力が7g以上、仕上げ加工後の150℃での乾熱収縮率が2%以下、150℃での熱応力が3g以下の撚糸にて織編物が構成されたことを特徴とする異収縮混繊糸の撚糸織編物。
【0006】
【課題を解決するための手段】
本発明は、単繊維繊度が2デニール以上の高収縮性ポリエステルフィラメント糸と単繊維繊度が3デニール以下の低収縮性ポリエステルフィラメント糸からなる、繊度が140〜200デニールの異収縮混繊糸に撚係数A(A=T・D1/2、T:撚糸数(回/m)、D:デ ニール)が8000〜23000の撚りが施された撚糸であって、撚り止め熱セット後の125℃での乾熱収縮率が4%以上、125℃での熱応力が7g以上、仕上げ加工後の150℃での乾熱収縮率が2%以下、150℃での熱応力が3g以下の撚糸にて織編物が構成されたことを特徴とする異収縮混繊糸の撚糸織編物、にある。
JP28631699A 1998-10-14 1999-10-07 異収縮混繊糸の撚糸織編物の製造方法 Expired - Fee Related JP4278796B2 (ja)