Prior art keywords
furnace
copper
stopper
energy
frequency furnace
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN 01253024
Other languages
English (en)
Inventor
金纪星
Original Assignee
戚建萍
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 戚建萍 filed Critical 戚建萍
Priority to CN 01253024 priority Critical patent/CN2482466Y/zh
Application granted granted Critical
Publication of CN2482466Y publication Critical patent/CN2482466Y/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Links

Landscapes

  • Manufacture And Refinement Of Metals (AREA)
  • Vertical, Hearth, Or Arc Furnaces (AREA)

Abstract

本实用新型公开了一种节能型水平连铸铜炉,由熔炼炉及通过连接体与其相连的保温工频炉组成,连接体内设有铜液流管,保温工频炉还通过连接体与温控调节保温炉相连,连接体内也设有铜液流管,其一端与设于保温工频炉下部的塞棒座相连,另一端与温控调节保温炉相通,保温工频炉上还设有塞棒,塞棒与塞棒座相密合。本实用新型适用于浇铸铜材,也适用于其他有色金属的浇铸。

Description

节能型水平连铸铜炉
一、技术领域
本实用新型涉及一种联体铸铜炉,尤其涉及一种节能型水平连铸铜炉。
二、背景技术
目前的铸铜工艺,都是采用将铜原料在熔炼炉熔化成铜液,铜液通过设有熔炼炉上口部的出液嘴倒入到保温工频炉中进行浇铸铜锭、铜棒等。这是传统的铸铜工艺,其缺点是铜液在操作过程中,接触空气,因此,铜液氧化损耗大,而且影响铜材质量,污染空气坏境,上述铜炉还存在耗能高,生产成本增高的缺点,而且操作工人劳动强度大。
三、发明内容
本实用新型专利的目的在于针对上述铜炉存在的缺点,提供一种节能、高效、铜液氧化小,质量好的节能型水平连铸铜炉。
本实用新型为节能型水平连铸铜炉,由熔炼炉及与其相连的保温工频炉组成,熔炼炉与保温工频炉之间设有连接体,在联接体内,设有铜液流管,其两端分别与熔炼炉和保温工频炉的下部相通,保温工频炉还通过连接体与温控调节保温炉相连,在连接体内也设有铜液流管,其一端与设于保温工频炉下部的塞棒座相连,而另一端则与温控调节保温炉的下部相通,保温工频炉上还设有塞棒,塞棒与塞棒座相密合。在温控调节保温炉的下部还设有结晶器座。
本实用新型与现有技术相比,具有以下优点;1、设于熔炼炉体下部的铜液流管的设置,解决了熔炼炉铜液倒液需要损耗热量及铜液氧化的难题,可节能20%,又提高了铜材质量。2、降低生产成本。3、减轻操作工人的劳动强度,节省劳动力,同时,改变了环境空气的污染。本实用新型适用于铜材的浇铸,特别适用于铜锭、空心铸锭的浇铸,也适用于其它有色金属的浇铸。
四、附图说明
附图为本实用新型整体结构剖示图。
五、具体实施方案
如图所示,本实用新型的熔炼炉1通过连接体2与保温工频炉4相连,在连接体2内,设有铜液流管3,其两端分别与熔炼炉1和保温工频炉4的下部相通。保温工频炉4还通过连接体7与温控调节保温炉9相连,在连接体7内,还设有铜液流管8,铜液流管8的一端连接设于保温工频炉4下部的塞棒座6,而另一端则与温控调节保温炉9的下部相通。保温工频炉4上还设有塞棒5,塞棒5与塞棒座6相密合。在温控调节保温炉9的下部还设有结晶器座10。
本实用新型适用于浇铸铜材及其他有色金属产品。

Claims (3)

1、一种节能型水平连铸铜炉,由熔炼炉(1)及通过连接体(2)相连的保温工频炉(4)所组成,其特征在于连接体(2)内设有铜液流管(3),铜液流管(3)的两端分别与熔炼炉(1)和保温工频炉(4)的下部相通,保温工频炉(4)还通过连接体(7)与温控调节保温炉(9)相连,连接体(7)内也设有铜液流管(8),铜液流管(8)的一端与设于保温工频炉(4)下部的塞棒座(6)相通,而另一端则与温控调节保温炉(9)的下部相连。
2、根据权利要求1所述的节能型水平连铸铜炉,其特征在于所述的保温工频炉(4)上设有塞棒(5),塞棒(5)与塞棒座(6)相密合。
3、根据权利要求1所述的节能型水平连铸铜炉,其特征在于所述的温控调节保温炉(9)的下部还设有结晶器座(10)。
CN 01253024 2001-08-13 2001-08-13 节能型水平连铸铜炉 Expired - Fee Related CN2482466Y (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN 01253024 CN2482466Y (zh) 2001-08-13 2001-08-13 节能型水平连铸铜炉

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN 01253024 CN2482466Y (zh) 2001-08-13 2001-08-13 节能型水平连铸铜炉

Publications (1)

Publication Number Publication Date
CN2482466Y true CN2482466Y (zh) 2002-03-20

Family

ID=33662599

Family Applications (1)

Application Number Title Priority Date Filing Date
CN 01253024 Expired - Fee Related CN2482466Y (zh) 2001-08-13 2001-08-13 节能型水平连铸铜炉

Country Status (1)

Country Link
CN (1) CN2482466Y (zh)

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN101698207B (zh) * 2009-10-20 2011-07-20 无锡隆达金属材料有限公司 铜合金盘管的生产方法
CN102764860A (zh) * 2012-07-02 2012-11-07 广西泰星电子焊接材料有限公司 双熔炼炉锡棒铸棒生产装置

Cited By (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN101698207B (zh) * 2009-10-20 2011-07-20 无锡隆达金属材料有限公司 铜合金盘管的生产方法
CN102764860A (zh) * 2012-07-02 2012-11-07 广西泰星电子焊接材料有限公司 双熔炼炉锡棒铸棒生产装置
CN102764860B (zh) * 2012-07-02 2014-08-06 广西泰星电子焊接材料有限公司 双熔炼炉锡棒铸棒生产装置

Similar Documents

Publication Publication Date Title
CN2482466Y (zh) 节能型水平连铸铜炉
CN209726787U (zh) 一种燃气坩埚炉
CN2791067Y (zh) 可倾坩埚快速熔铝炉
CN207227513U (zh) 一种自耗电极
CN1270852C (zh) 电渣重熔补缩工艺
CN207057614U (zh) 一种拆卸式真空炉浇铸用石墨嘴
CN2641557Y (zh) 潜流式工频有芯组合电炉
CN2524189Y (zh) 一种感应加热熔炼炉
CN2173671Y (zh) 钢锭定向凝固装置
CN201876117U (zh) 一种铝屑回收熔炼炉
CN2288799Y (zh) 小方坯连铸机结晶器
CN2288185Y (zh) 用紫杂铜生产无氧铜的配套装置
CN2274191Y (zh) 精铝生产定向结晶炉
CN202726036U (zh) 一种用于工业硅炉外精炼的感应加热抬包
CN2644048Y (zh) 垂直连铸装置
CN2312946Y (zh) 一种新型铝液混合炉
CN2407317Y (zh) 熔炼炉
CN206359656U (zh) 一种多晶硅铸锭炉
CN2526110Y (zh) 一种铜合金水平连铸电磁搅拌结晶装置
CN2336307Y (zh) 浇注炉衬
CN2636180Y (zh) 单晶材料生产的新炉型
CN2672059Y (zh) 复合式加热玻璃电熔炉
CN2851283Y (zh) 铝保持炉的铝水抬包直接加料机构
CN217154953U (zh) 一种船形熔锌电炉
CN219178294U (zh) 一种方便拆卸更换铜夹的锗锭还原炉

Legal Events

Date Code Title Description
C14 Grant of patent or utility model
GR01 Patent grant
C19 Lapse of patent right due to non-payment of the annual fee
CF01 Termination of patent right due to non-payment of annual fee