CN102764860B - 双熔炼炉锡棒铸棒生产装置 - Google Patents

双熔炼炉锡棒铸棒生产装置 Download PDF

Info

Publication number
CN102764860B
CN102764860B CN201210223172.6A CN201210223172A CN102764860B CN 102764860 B CN102764860 B CN 102764860B CN 201210223172 A CN201210223172 A CN 201210223172A CN 102764860 B CN102764860 B CN 102764860B
Authority
CN
China
Prior art keywords
tin
casting rod
smelting furnace
bar
smelting
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201210223172.6A
Other languages
English (en)
Other versions
CN102764860A (zh
Inventor
戴爱斌
伍永田
赵盛林
王继峰
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
GUANGXI TAIXING ELECTRONIC WELDING MATERIAL CO Ltd
Original Assignee
GUANGXI TAIXING ELECTRONIC WELDING MATERIAL CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by GUANGXI TAIXING ELECTRONIC WELDING MATERIAL CO Ltd filed Critical GUANGXI TAIXING ELECTRONIC WELDING MATERIAL CO Ltd
Priority to CN201210223172.6A priority Critical patent/CN102764860B/zh
Publication of CN102764860A publication Critical patent/CN102764860A/zh
Application granted granted Critical
Publication of CN102764860B publication Critical patent/CN102764860B/zh
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明涉及一种双熔炼炉锡棒铸棒生产装置,包括钢平台、安装在钢平台上的熔炼炉,金属锡在熔炼炉内高温熔炼搅拌,熔炼炉底部的放锡管连通铸棒机的保温箱,放锡管上安装有放锡阀,所述熔炼炉数量为2个,分别通过放锡阀和放锡管连通到铸棒机的保温箱,两台熔炼炉分别保证有一台铸棒、另一台熔炼,保持铸棒机连续工作。本发明通过两台熔炉共用一台铸棒机的设计,使两台熔炉错开时间熔炼合金,基本可以达到铸棒机不停机工作,大大缩短了铸棒周期,解决了铸棒机产能利用不足问题,通过改进设置,铸棒机生产能力增加一倍,并且可以降低设备操作人员的配置,设备改进成本低,效果明显。

Description

双熔炼炉锡棒铸棒生产装置
技术领域
本发明涉及一种锡焊料的熔炼、铸棒生产设备,适用于锡焊料棒材的生产。
背景技术
锡焊料是由以锡金属为主的多种元素合金,锡焊料生产首先要将各种元素在熔炉内炼制合金,并把合金制成一定尺寸的棒材以方便后继的挤压成型加工。
目前锡棒的铸造方式有两种,一种的浇铸、另一种是真空连铸,浇铸锡棒因为冷却成型时与空气接触,表面产生氧化皮,冷却时因得不到焊料补充产生缩孔,制出来的锡棒质量较差,还须进行剥皮、切除端头的工序,因此浇铸锡棒只在一些小工厂内使用较多。真空连铸工艺,通过铸棒机从保温炉底部牵引焊料,通过结晶器冷却成型,经切割后得到所需要的锡棒尺寸。真空铸棒在焊料由液态转为固态过程中与空气隔离,不会产生氧化皮,因有保温炉内不断有液态焊料补充,冷却过程中不会产生缩孔。一般的上规模的焊料厂都使用真空铸棒工艺,以确保产品质量。
现有真空铸棒工艺,一般由一台熔炉和一台铸棒机组合形成锡棒生产线,因为生产工艺要求,金属锭熔化及合金熔炼搅拌过程需要3—5个小时,这段时间铸棒机处于停机待料状态,一般锡棒铸棒机铸棒速度约为铸棒420Kg/小时,熔炉容量按1.5吨计算,一炉料约4个小时可以,熔炉需要重新熔化金属锭,这段时间铸棒机是闲置的,如此算来铸棒机的产能相当于只利用了一半,影响了铸棒效率,设备使用率不高,锡棒产量低下。
发明内容
本发明提供一种双熔炼炉锡棒铸棒生产装置,能够解决由于单台熔炼炉需要熔炼金属锭导致铸棒机使用率不高、生产效率低下的问题。
本发明双熔炼炉锡棒铸棒生产装置,包括钢平台、安装在钢平台上的熔炼炉,金属锡在熔炼炉内高温熔炼搅拌,熔炼炉底部的放锡管连通铸棒机的保温箱,放锡管上安装有放锡阀,所述熔炼炉数量为2个,分别通过放锡阀和放锡管连通到铸棒机的保温箱,两台熔炼炉分别保证有一台铸棒、另一台熔炼,保持铸棒机连续工作。
所述铸棒机的放锡管加热控制电路为可选择的双输出控制电路,由选择开关SA2控制。
本发明使用两台熔炉共用一台铸棒机设计,两台熔炉错开时间熔炼合金,基本可以达到铸棒机不停机工作,大大缩短了铸棒周期,铸棒机产能利用不足问题,通过改进设置,铸棒机生产能力增加一倍,并且可以降低设备操作人员的配置,设备改进成本低,效果明显。
附图说明
图1是本发明双熔炼炉锡棒铸棒生产装置的结构示意图。
图2是传统单个熔炼炉锡棒铸棒生产装置的结构示意图。
图3是本发明的放锡管加热控制电路原理图。
其中1——钢平台;2——熔炼炉;3——放锡阀;4——放锡管;5——保温箱;6——铸棒机。
具体实施方式
如图2所示,传统的单个熔炼炉锡棒铸棒生产装置包括钢平台1、安装在钢平台上的熔炼炉2,金属锡在熔炼炉内高温熔炼搅拌,熔炼炉2底部的放锡管4连通铸棒机6的保温箱5,放锡管4上安装有放锡阀3。
如图1、3所示,本发明双熔炼炉锡棒铸棒生产装置的熔炼炉数量为2个,分别通过放锡阀和放锡管连通到铸棒机的保温箱5,两台熔炼炉安装在熔炼平台上,锡锅底部有放锡管,通过阀门控制连接到铸棒机保温箱,保温箱增开一个进料口。两台熔炼炉分别保证有一台铸棒、另一台熔炼,保持铸棒机6连续工作。由于配套铸棒机的熔炼炉增加了一台,铸棒机放锡管保温电路须做改动,将原来的一套加热控制电路,改为可选择的双输出控制,由选择开关SA2控制。
实施例:传统单个熔炼炉锡棒铸棒生产线8小时可铸棒1.5吨,使用本发明双熔炼炉锡棒铸棒生产装置的生产线10个小时可完成铸棒3吨。如果是连续三班制生产,产量每条线每班可达3吨,比原来提高一倍的生产效率。
由于采用了两台炉共用一台铸棒机设计,两台熔炼炉始终保持有一台铸棒、一台熔炼,铸棒机无须在合金熔炼阶段停机,大大提高了铸棒机的效率。经测试,使用本发明双熔炼炉锡棒铸棒生产装置的生产线,相同产量情况下,按单班生产计算,每3吨产品可节省人工37.5%合12工时,按三班制计算,节省50%人工。设备投入节省一台铸棒机,铸棒机目前市场价为20万人民币,高位熔炉为10万元左右,节省设备投入33%合20万元。如果同时拥有多条生产线,效率更为提高,大大缩短了生产周期,节约了大量的设备投入及人工成本。

Claims (2)

1.一种双熔炼炉锡棒铸棒生产装置,包括钢平台(1)、安装在钢平台上的熔炼炉(2),金属锡在熔炼炉内高温熔炼搅拌,熔炼炉(2)底部的放锡管(4)连通铸棒机(6)的保温箱(5),放锡管(4)上安装有放锡阀(3),其特征在于:所述熔炼炉数量为2个,分别通过放锡阀和放锡管连通到铸棒机的保温箱(5),两台熔炼炉分别保证有一台铸棒、另一台熔炼,保持铸棒机(6)连续工作。
2. 根据权利要求1所述的双熔炼炉锡棒铸棒生产装置,其特征在于:所述铸棒机的放锡管(4)加热控制电路为可选择的双输出控制电路,由选择开关SA2控制。
CN201210223172.6A 2012-07-02 2012-07-02 双熔炼炉锡棒铸棒生产装置 Expired - Fee Related CN102764860B (zh)