CN2395867Y - 一种制作圆孔混凝土构件的芯管 - Google Patents

一种制作圆孔混凝土构件的芯管 Download PDF

Info

Publication number
CN2395867Y
CN2395867Y CN 99248323 CN99248323U CN2395867Y CN 2395867 Y CN2395867 Y CN 2395867Y CN 99248323 CN99248323 CN 99248323 CN 99248323 U CN99248323 U CN 99248323U CN 2395867 Y CN2395867 Y CN 2395867Y
Authority
CN
China
Prior art keywords
pipe
circular hole
concrete component
core
making
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN 99248323
Other languages
English (en)
Inventor
万程
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN 99248323 priority Critical patent/CN2395867Y/zh
Application granted granted Critical
Publication of CN2395867Y publication Critical patent/CN2395867Y/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本实用新型公开了一种制作圆孔混凝土构件的芯管,芯管包括硬管和软管,硬管外套有软管。所述的硬管外套有用塑料或橡胶制成的软管。所述的硬管为钢管。它可使抽拔芯管容易,且不会产生裂纹,还能提高圆孔混凝土构件的强度。

Description

一种制作圆孔混凝土构件的芯管
本实用新型涉及一种制作圆孔混凝土构件时使用的芯管。
目前制作圆孔混凝土构件使用的芯管,多数是采用钢管作为芯管。制作圆孔混凝土构件时,在模具中固定有数根作为芯管的钢管,钢管外径与混凝土构件中的圆孔内径相当,然后往上述模具中浇铸混凝土,过一定时间,将芯管抽拔出来,待混凝土硬化后再将上述模具打开,即可制成一定形状的、带圆孔的混凝土构件。但该种芯管,使制作圆孔混凝土构件存在以下问题,特别是快硬性水泥制品的生产过程中,抽拔芯管的时间控制非常困难,时间早了,会使制品塌落;时间晚了,又会使芯管抽拔困难,常出现由于抽拔芯管而引起的制品开裂,或产生裂纹,或将芯管固死在制品中而难以拔出等,而且其强度亦大大降低。
本实用新型的目的是要提供一种制作圆孔混凝土构件时使用的芯管,它可使抽拔芯管容易,且不会产生裂纹,还能提高圆孔混凝土构件的强度。
本实用新型的目的是这样实现的:一种制作圆孔混凝土构件的芯管,芯管包括硬管和软管,硬管外套有软管。
所述的硬管外套有用塑料或橡胶制成的软管。
所述的硬管为钢管。
所述的硬管外经小于软管的内径,软管外径与混凝土构件中的圆孔内径相应。
所述的钢管外经小于软管的内径,软管外径与混凝土构件中的圆孔内径相应。
本实用新型由于在硬管外还套有塑料或橡胶软管,软管与混凝土之间的摩擦力较小,因此抽拔时容易;由于塑料、橡胶软管表面光滑且有弹性,抽拔时不会在混凝土构件中产生内、外裂纹,因此制品的强度与外观性能得到显著改善;抽拔时间容易控制,不会出现塌落或固死现象;塑料或橡胶软管制作可以极为密封,克服原有技术容易使混凝土构件水泥浆外溢的问题,使制品内壁形成致密的水泥层。
下面结合附图详细说明依据本实用新型提出的制作圆孔混凝土构件使用的芯管的具体结构和工作原理。
图1是本实用新型制作圆孔混凝土构件的芯管及模具的剖视图。
图2是本实用新型圆孔混凝土构件的示意图。
如图1、2所示,制作圆孔混凝土构件使用的模具1,其内浇铸混凝土。模具1中水平排列固定数根由钢管2和软管3组成的芯管,钢管2外套有用塑料或橡胶制成的软管3,钢管2外经略小于软管3的内径,软管3外径与混凝土构件4中的圆孔5内径相应。
圆孔混凝土构件的生产制造方法:
一、在特定形状的模具1中按照一定距离水平排列固定数根由钢管2和软管3组成的芯管,芯管内部是钢管2,钢管2外套有用塑料或橡胶制成的软管3,钢管2外经小于软管3的内径,软管3外径与混凝土构件4中的圆孔5内径相应;
二、然后往模具1中浇铸混凝土;
三、待混凝土硬化后,将钢管2从塑料或橡胶软管3中抽拔出来;
四、再将塑料或橡胶软管3从混凝土中抽拔出来;
五、将模具1打开,即可制成一定形状的、带圆孔的混凝土构件4。
由于软管内有硬管,制品成型能振动密实,保证圆孔的形状,由于软管的弹性,使抽拔时不易使混凝土构件产生内、外裂纹,因此制品的强度与外观性能得到显著改善;抽拔时间容易控制,不会出现塌落或固死现象,而且塑料或橡胶软管制作可以极为密封,克服原有技术容易使混凝土构件水泥浆外溢的问题,使制品内壁形成致密的水泥层。

Claims (5)

1、一种制作圆孔混凝土构件的芯管,其特征在于:芯管包括硬管和软管,硬管外套有软管。
2、如权利要求1所述的一种制作圆孔混凝土构件的芯管,其特征在于:所述的硬管外套有用塑料或橡胶制成的软管。
3、如权利要求1、2所述的一种制作圆孔混凝土构件的芯管,其特征在于:所述的硬管为钢管。
4、如权利要求1、2所述的一种制作圆孔混凝土构件的芯管,其特征在于:所述的硬管外经小于软管的内径,软管外径与混凝土构件中的圆孔内径相应。
5、如权利要求3所述的一种制作圆孔混凝土构件的芯管,其特征在于:所述的钢管外经小于软管的内径,软管外径与混凝土构件中的圆孔内径相应。
CN 99248323 1999-10-11 1999-10-11 一种制作圆孔混凝土构件的芯管 Expired - Fee Related CN2395867Y (zh)