CN203679235U - 汽车铝合金车轮铸造用浇口套 - Google Patents

汽车铝合金车轮铸造用浇口套 Download PDF

Info

Publication number
CN203679235U
CN203679235U CN201320713624.9U CN201320713624U CN203679235U CN 203679235 U CN203679235 U CN 203679235U CN 201320713624 U CN201320713624 U CN 201320713624U CN 203679235 U CN203679235 U CN 203679235U
Authority
CN
China
Prior art keywords
sprue bush
heat
sprue
casting
boss
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201320713624.9U
Other languages
English (en)
Inventor
黎永山
李萍
徐启祥
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Jiangsu Kaite Automobile Parts Co Ltd
Original Assignee
Jiangsu Kaite Automobile Parts Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Jiangsu Kaite Automobile Parts Co Ltd filed Critical Jiangsu Kaite Automobile Parts Co Ltd
Priority to CN201320713624.9U priority Critical patent/CN203679235U/zh
Application granted granted Critical
Publication of CN203679235U publication Critical patent/CN203679235U/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

一种汽车铝合金车轮铸造用浇口套,该浇口套用陶瓷材料制成,浇口套安装在底模上,浇口套由上下两个部分一体制造而成,其中下部为浇口套的凸台部分,该凸台和底模型腔配合,当浇口套安装在底模上后可将其嵌合在底模上,凸起部位的宽度约为整个浇口套的1/6~1/8,浇口套凸台上安装有保温杯,保温杯和浇口套之间用耐火纤维糊粘结。使用时先将浇口套上部装入底模,然后在与浇口套凸台部分连接的保温杯上均匀抹上耐火纤维糊,将粘有耐火纤维糊的保温杯安装在浇口套凸台部位,使保温杯的浇口和浇口套的浇口完全重合,清除浇口套和保温杯连接部位的残渣,即完成了浇口套的安装,该浇口套具有保温性好、铸造性高的特点。

Description

汽车铝合金车轮铸造用浇口套
技术领域
本实用新型涉及铸造装备领域,具体地说涉及一种汽车铝合金车轮铸造用浇口套。
背景技术
铸造是汽车铝合金车轮最重要的生产环节,不仅关系到整个车轮的制造质量,而且对后续的热处理和机械加工有重要的影响。汽车铝合金车轮的铸造有低压铸造、差压铸造、重力铸造、挤压铸造等多种方式,而低压铸造因充型平稳、产品机械性能高、金属利用率高等优点,已成为汽车铝合金车轮首选的铸造方式,目前有约有80%以上的铝车轮采用低压铸造的方式进行制造。
浇口套作为汽车铝合金车轮低压铸造中重要的模具部件正越来越受到铝车轮制造行业的重视,该部件对浇注的平稳性和生产的稳定性有着重要的影响。因考虑铸造生产环境的恶劣,以及在生产过程中需要频繁安放过滤网和捅冒口,铝车轮行业一着使用H13钢为原材料制造铁浇口,虽然该浇口耐腐蚀性较强,但其不仅价格很昂贵,而且保温性差,不利于铝车轮低压铸造中的保温补缩;而且因浇口套的上口要装配保温杯,二者对接过程中因密封性较差常会在缝隙处产生挂渣和积铝,从而影响铸造的质量和效率,因此铝车轮行业需要寻找一种更适合的铸造用的浇口套。
发明内容
本发明的目的是克服现有技术的缺陷,提供一种兼具保温性和耐腐蚀性的铝车轮铸造用浇口套,同时解决浇口套和保温杯的连接处容易积铝、挂渣等问题,具体地说提供一种汽车铝合金车轮铸造用浇口套。
解决以上问题的具体方案是:一种汽车铝合金车轮铸造用浇口套,该浇口套用陶瓷材料制成,浇口套安装在底模上,浇口套由上下两个部分一体制造而成,其中下部为浇口套的凸台部分,该凸台和底模型腔配合,当浇口套安装在底模上后可将其嵌合在底模上,凸起部位的宽度约为整个浇口套的1/6~1/8,浇口套凸台上安装有保温杯,保温杯和浇口套之间用耐火纤维糊粘结。使用时先将浇口套上部装入底模,然后在与浇口套凸台部分连接的保温杯上均匀抹上耐火纤维糊,将粘有耐火纤维糊的保温杯安装在浇口套凸台部位,使保温杯的浇口和浇口套的浇口完全重合,清除浇口套和保温杯连接部位的残渣,即完成了浇口套的安装。在铸造过程中,因陶瓷浇口套抗击打能力比铁浇口差,因此要求铸造人员在捅冒口时应垂直轻捅,防止损坏浇口套。
该浇口套由于以耐高温、耐腐蚀的陶瓷材料代替了H13钢材料,不仅降低了铸造成本,而且使产品的铸造性更好;由于采用一体式浇口套并和底模的部位嵌合,并且在和保温杯连接部位用耐火纤维糊粘接,因此大大减少了挂渣和积铝问题,是汽车铝车轮铸造理想的模具附件。
附图说明
图1为本实用新型汽车铝合金车轮铸造用浇口套结构示意图;
图2本实用新型汽车铝合金车轮铸造用浇口套和保温杯装配图。
具体的实施方式
如图1、图2所示,一种汽车铝合金车轮铸造用浇口套,该浇口套为陶瓷材料制成,浇口套分为上部1和下部2二个部分,上下部一体制造而成,下部2为凸台结构,其体积约为整个浇口套的1/6;该凸起部位为和底模配合的安装面,即浇口套安装在底模上正好和其嵌合;浇口套下部2安装有保温杯3,在保温杯3和浇口套上部有耐火纤维糊4,该浇口套具有保温性好、铸造性高的特点,并且和传统的铁浇口相比更具成本优势。

Claims (1)

1.一种汽车铝合金车轮铸造用浇口套,其特征是:一种汽车铝合金车轮铸造用浇口套,该浇口套为陶瓷材料制成,浇口套分为上部(1)和下部(2)二个部分,上下部一体制造而成,其中下部(2)为浇口套的凸台部分,其体积为整个浇口套的1/6;该凸台和底模型腔配合,当浇口套安装在底模上后可将其嵌合在底模上,浇口套下部(2)安装有保温杯(3),保温杯(3)和浇口套之间用耐火纤维糊(4)粘结。
CN201320713624.9U 2013-11-13 2013-11-13 汽车铝合金车轮铸造用浇口套 Expired - Fee Related CN203679235U (zh)