Prior art keywords
riser
heat
rising head
casting
protecting layer
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN2011203298743U
Other languages
English (en)
Inventor
金忠贵
黄林刚
高佳健
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
FUXIN ZHONGFU LIGHT METAL TECHNOLOGY Co Ltd
Original Assignee
FUXIN ZHONGFU LIGHT METAL TECHNOLOGY Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by FUXIN ZHONGFU LIGHT METAL TECHNOLOGY Co Ltd filed Critical FUXIN ZHONGFU LIGHT METAL TECHNOLOGY Co Ltd
Priority to CN2011203298743U priority Critical patent/CN202199724U/zh
Application granted granted Critical
Publication of CN202199724U publication Critical patent/CN202199724U/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Links

Landscapes

  • Molds, Cores, And Manufacturing Methods Thereof (AREA)

Abstract

本实用新型属于铸造工艺装备,特别涉及一种金属型铸造用保温冒口,在模型(5)的上面固定设有一个冒口座(7),冒口座(7)上固定设有内冒口保护层(1)和外冒口保护层(4),内冒口保护层(1)和外冒口保护层(4)之间设有冒口保温层(3),冒口(2)置于内冒口保护层(1)中,金属型铸造用保温冒口是解决了铸件在浇注过程中,由于冒口凝固过早,导致缩松、缩孔的出现,在原来冒口外部增加一个导热系数很低的冒口保温层,使铸件在凝固过程中做到冒口最后凝固,铸件的工艺出品率可提高10%,废品率降低5%,保证铸件内部质量,消除了缩松、缩孔。

Description

金属型铸造用保温冒口
技术领域
本实用新型属于铸造工艺装备,特别涉及一种金属型铸造用保温冒口。
背景技术
原有的金属型冒口补缩效果差,导致铸件工艺出品率低,铸件内部出现缩松、结合缩孔,严重影响企业的经济效益和生产能力。
发明内容
本实用新型的目的在于克服上述技术不足,提供一种冒口补缩效果好,提高铸件工艺出品率的金属型铸造用保温冒口。
本实用新型解决技术问题采用的技术方案是:金属型铸造用保温冒口包括模型 、铸件、冒口,其特点是在模型的上面固定设有一个冒口座,冒口座上固定设有内冒口保护层和外冒口保护层,内冒口保护层和外冒口保护层之间设有冒口保温层,冒口置于内冒口保护层中。
本实用新型的有益效果是:金属型铸造用保温冒口是解决了铸件在浇注过程中,由于冒口凝固过早,导致缩松、缩孔的出现,在原来冒口外部增加一个导热系数很低的冒口保温层,使铸件在凝固过程中做到冒口最后凝固,铸件的工艺出品率可提高10%,废品率降低5%,保证铸件内部质量,消除了缩松、缩孔。
附图说明
以下结合附图以实施例具体说明。
图1是金属型铸造用保温冒口的结构及局剖图。
图中,1-内冒口保护层;2-冒口;3-冒口保温层;4-外冒口保护层;5-模型;6-铸件;7-冒口座。
具体实施方式
实施例,参照附图1,金属型铸造用保温冒口的模型5内铸有铸件6,模型5的上面固定设有一个冒口座7,冒口座7上固定设有内冒口保护层1和外冒口保护层4,内冒口保护层1和外冒口保护层4之间设有冒口保温层3,冒口2置于内冒口保护层1中。
金属型铸造用保温冒口的使用方法是:将冒口座7固定在模型5的上面,从冒口2向模型5内浇注金属熔液实施铸造。

Claims (1)

1.一种金属型铸造用保温冒口,包括模型(5)、铸件(6)、冒口(2),其特征在于在模型(5)的上面固定设有一个冒口座(7),冒口座(7)上固定设有内冒口保护层(1)和外冒口保护层(4),内冒口保护层(1)和外冒口保护层(4)之间设有冒口保温层(3),冒口(2)置于内冒口保护层(1)中。
CN2011203298743U 2011-09-05 2011-09-05 金属型铸造用保温冒口 Expired - Fee Related CN202199724U (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN2011203298743U CN202199724U (zh) 2011-09-05 2011-09-05 金属型铸造用保温冒口

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN2011203298743U CN202199724U (zh) 2011-09-05 2011-09-05 金属型铸造用保温冒口

Publications (1)

Publication Number Publication Date
CN202199724U true CN202199724U (zh) 2012-04-25

Family

ID=45963862

Family Applications (1)

Application Number Title Priority Date Filing Date
CN2011203298743U Expired - Fee Related CN202199724U (zh) 2011-09-05 2011-09-05 金属型铸造用保温冒口

Country Status (1)

Country Link
CN (1) CN202199724U (zh)

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN105371706A (zh) * 2015-12-09 2016-03-02 山东天宝化工股份有限公司 一种起爆具注药冒口及其使用方法
CN108465778A (zh) * 2018-02-05 2018-08-31 霍山县东胜铸造材料有限公司 一种发热保温冒口套

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN105371706A (zh) * 2015-12-09 2016-03-02 山东天宝化工股份有限公司 一种起爆具注药冒口及其使用方法
CN108465778A (zh) * 2018-02-05 2018-08-31 霍山县东胜铸造材料有限公司 一种发热保温冒口套

Similar Documents

Publication Publication Date Title
CN103464683B (zh) 一种熔模铸造方法
CN202894216U (zh) 针对大尺寸和复杂框架式钛合金薄壁铸件的浇注工装
CN204018648U (zh) 一种通过砂芯加热提高冒口补缩距离的铸造结构
CN104607595A (zh) 一种大型铝水器皿铸造装置
CN202199724U (zh) 金属型铸造用保温冒口
CN201127979Y (zh) 一种发动机缸盖重力浇注模具
CN102886496A (zh) 一种铸造补缩方法与装置
CN104174817B (zh) 一种海洋平台爬升机连接座的铸造及热处理工艺
CN104368760A (zh) 一种台阶形铝合金油底壳的铸造方法及其专用铸造模具
CN203764889U (zh) 高铁枕梁铸件顺序凝固成型模具
CN202097364U (zh) 箱角件u型外冷铁
CN204524227U (zh) 飞轮壳低压铸造模具
CN202539477U (zh) 高压开关法兰复合型铸造模具
CN202762962U (zh) 一种铸造模具
CN203019600U (zh) 低压电流互感器用浇注成型模具
CN204321097U (zh) 精密铸造单晶涡轮叶片模型工艺筋
CN103056286A (zh) 提高铸件表面质量的方法
CN201832983U (zh) 一种真空浇铸模具组件
CN102886506A (zh) 提高镁合金铸件机械性能的模具
CN204685960U (zh) 一种用于铝合金排油管铸型的防缩松结构
CN104368764A (zh) 精密铸造单晶涡轮叶片模型工艺筋
CN203437603U (zh) 新型镍铸锭用模具保温帽
CN203917814U (zh) 一种铝合金进水管的冒口结构
CN203330350U (zh) 一种新型的钳体铸造装置
CN203830677U (zh) 一种用于生产铝合金锭的铸锭模

Legal Events

Date Code Title Description
C14 Grant of patent or utility model
GR01 Patent grant
CF01 Termination of patent right due to non-payment of annual fee
CF01 Termination of patent right due to non-payment of annual fee

Granted publication date: 20120425

Termination date: 20190905