CN201015913Y - Fpc软板快压用阻胶膜 - Google Patents
Fpc软板快压用阻胶膜 Download PDFInfo
- Publication number
- CN201015913Y CN201015913Y CNU2007200333772U CN200720033377U CN201015913Y CN 201015913 Y CN201015913 Y CN 201015913Y CN U2007200333772 U CNU2007200333772 U CN U2007200333772U CN 200720033377 U CN200720033377 U CN 200720033377U CN 201015913 Y CN201015913 Y CN 201015913Y
- Authority
- CN
- China
- Prior art keywords
- layer
- film
- soft board
- paper
- pressing
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
一种FPC软板快压用阻胶膜,包括一本体,其特征在于:所述本体由纸层和离型层复合而成,所述离型层为双层结构,包括薄膜层和吸附在薄膜层表面的防粘性液层。本实用新型利用离型层良好的离型性,使本体更易于被剥除,避免产生皱折,同时利用其阻胶性,避免接着剂的溢出,实现对软板良品率的提高,特别适用于快压工艺。
Description
技术领域
本实用新型涉及一种FPC软板压合过程中使用的离型膜,用于压合保护膜及PI,PET补强,起到离型与阻胶(抗溢胶)的作用,具体涉及一种软板(柔性线路板)在使用快压压合工艺时使用的阻胶膜。
背景技术
软板(FPC),即软性印刷电路板(Flexible Printed Circuit)的简称,相对于硬式电路板,软板材质特性为可挠性,且具有容易转折、重量轻、厚度薄等优点,因此经常应用于需要轻薄设计或可动式机构设计的产品,如手机、笔记型计算机、显示器、消费性电子产品、触控面板及IC构装等。
软板产品构造上由软性铜箔基板(FCCL)和软性绝缘层(常用PI或PET)以接着剂(胶)贴附后压合而成,按照导电铜箔的层数划分,分为单层板、双层板、多层板、双面板等,并依客户要求可贴附补强板等附件,以单层板为例,其基本工艺过程为:通常基材+透明胶+铜箔是一套买来的原材料,保护膜+透明胶是另一种买来的原材料。首先,铜箔要进行刻蚀等工艺处理来得到需要的电路,保护膜要进行钻孔以露出相应的焊盘,清洗之后再用热压法把两者结合起来。其他种类的板以及附贴的补强板在制作过程中均需采用热压合成,为避免压合的热板(SUS)与软板粘合或是损坏软板,需在热板与软板之间加设分隔垫层,以满足热压的需要。
在热压工艺中,根据热压时间的长短可分为传统热压和快压。其中快压工艺通常采用热板预压185℃10秒、185℃正压120秒实现。目前,在快压中使用的分隔垫层通常为日本三井公司生产的TPX膜(聚-4-甲基-1戊烯),该膜的厚度在50um~120um之间。在实际使用过程中发现,TPX膜的离型效果较差,也就是说,在热压工艺结束后,TPX膜难以从FPC板上剥除下来,尤其是在制作较薄的单面板时,剥除TPX膜过程中易使单面板产生皱折,影响FPC板面表面平整度;同时,TPX膜的成本较高,从而加大了整个FPC板的生产成本。
发明内容
本实用新型目的是提供一种具有良好离型性,阻胶性好的FPC软板快压用阻胶膜,通过使用该膜可降低FPC软板的生产成本,提高良品率。
为达到上述目的,本实用新型采用的技术方案是:一种FPC软板快压用阻胶膜,包括一本体,所述本体由纸层和离型层复合而成,所述离型层为双层结构,包括薄膜层和吸附在薄膜层表面的防粘性液层。
上述技术方案中,所述纸层可采用现有的牛皮纸、铜板纸、CCK纸或格拉辛纸等,薄膜层和防粘性液层共同构成离型层,起离型和阻胶的作用;其中,防粘性液层可采用环氧胶水、硅油类或非硅离型剂构成,首先将薄膜层与纸层热压复合形成复合膜,再涂覆一层环氧胶水或硅油或非硅离型剂,构成离型层,所述离型层的设置,既起到离型的作用,同时也起阻胶的作用,避免热压过程中FPC板保护膜的接着剂溢出,提高良品率。在使用时,铺于热板(SUS)与FPC软板之间压合,热板经预压10秒,185℃高温正压120秒,然后冷却,当温度降至23℃左右后开始剥离工序。
上述技术方案中,所述薄膜层由聚乙烯(PE)或者聚脂薄膜(PET)构成,其厚度在15~50微米之间,所述纸层由80~180克之间的纸片构成。
由于上述技术方案运用,本实用新型与现有技术相比具有的优点是:
1、由于本实用新型的本体由纸层、双层结构的离型层复合构成,利用离型层良好的离型性,使对本体的剥除更为容易,避免皱折的产生,同时利用离型层的阻胶性,可避免FPC板在热压过程中接着剂的溢出现象,提高良品率;
2、通过纸层与薄膜层的设置,在热压过程中,起到对热板(钢板)的压力缓冲,填补FPC板中保护膜与铜箔开口部位的缝隙,起到阻胶作用,有利于提高FPC良品率;
3、本实用新型采用PE(聚乙烯)等材料的薄膜层和吸附在薄膜层表面的防粘性液层构成离型层,适用于快压工艺,成本低,制备方便。
附图说明
附图1为本实用新型实施例一的结构示意图。
其中:1、纸层;2、薄膜层;3、防粘性液层。
具体实施方式
下面结合附图及实施例对本实用新型作进一步描述:
实施例一:参见附图1所示,一种FPC软板快压用阻胶膜,包括一本体,所述本体由120~180克的铜板纸层1、聚乙烯(PE)薄膜层2和环氧胶水层复合而成,其中,聚乙烯薄膜层的厚度为15~50微米,环氧胶水层与薄膜层一起构成离型层。
实施例二:一种FPC软板快压用阻胶膜,包括一本体,所述本体由纸层1、薄膜层2和防粘性液层3复合而成,所述纸层为120-180克的日本产CCK纸,缓冲层为PE(聚乙烯),厚度为20微米,防粘性液层采用硅油或者非硅离型剂构成。
实施例三:一种FPC软板快压用阻胶膜,包括一本体,所述本体由纸层1、薄膜层2和防粘性液层3复合而成,所述纸层为120-180克的牛皮纸,缓冲层为PET(聚脂),厚度为40微米,防粘性液层采用防粘胶水构成。
Claims (2)
1.一种FPC软板快压用阻胶膜,包括一本体,其特征在于:所述本体由纸层[1]和离型层复合而成,所述离型层为双层结构,包括薄膜层[2]和吸附在薄膜层表面的防粘性液层[3]。
2.根据权利要求1所述的FPC软板快压用阻胶膜,其特征在于:所述薄膜层由聚乙烯或者聚脂薄膜构成,其厚度在15~50微米之间,所述纸层由80~180克之间的纸片构成。