CN1927574A - 具橡胶饰片的鞋底制造方法 - Google Patents

具橡胶饰片的鞋底制造方法 Download PDF

Info

Publication number
CN1927574A
CN1927574A CN 200510098370 CN200510098370A CN1927574A CN 1927574 A CN1927574 A CN 1927574A CN 200510098370 CN200510098370 CN 200510098370 CN 200510098370 A CN200510098370 A CN 200510098370A CN 1927574 A CN1927574 A CN 1927574A
Authority
CN
China
Prior art keywords
sole
rubber
mould
stock
rubber decoration
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN 200510098370
Other languages
English (en)
Other versions
CN100400276C (zh
Inventor
刘坤钟
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CNB2005100983704A priority Critical patent/CN100400276C/zh
Publication of CN1927574A publication Critical patent/CN1927574A/zh
Application granted granted Critical
Publication of CN100400276C publication Critical patent/CN100400276C/zh
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种具橡胶饰片的鞋底制造方法,是预先制备一橡胶饰片,该橡胶饰片具有一下层及一上层,该上层内含的交联剂浓度低于该下层,先使该下层已熟化,但是该上层尚残存交联能力。当该橡胶饰片放入一模具中后,可将一大底胚料填入该模具中,且使该大底胚料与该橡胶饰片的上层接触,再对该模具进行热压,该饰片的上层利用残存的交联能力继续与该大底胚料完成交联反应,就可获得一具有饰片的鞋底。

Description

具橡胶饰片的鞋底制造方法
技术领域
本发明涉及一种鞋底,特别是涉及一种具橡胶饰片的鞋底制造方法。
背景技术
一般的鞋底,为了达到鞋底底面的装饰、止滑目的,在成型时,是利用至少一橡胶饰片与一大底胚料结合成一鞋底。
针对饰片与大底胚料均采用橡胶材质,所应用的成型方法,是先制备一模具,且该模具具有一下模、一与该下模对应设置的上模及一可与该下模配合的中模。该下模具有一由一分色岭所界定而成的定位部。且先利用该中模将一具有交联剂的橡胶薄片朝该分色岭压制,就可在该定位部中形成一饰片,且在该分色岭外部形成一余料,当取出中板、余料后,再将一具有交联剂的大底胚料填入该下模中,且对该模具进行热压后,可使该饰片与该大底胚料完成交联反应,且可制成一具有橡胶饰片的鞋底。
这种成形方法,利用饰片与大底胚料采用相同材质,虽然可在该模具内部直接使该饰片与该大底胚料完成交联反应并固结成一体,但是,利用该中模对橡胶薄片以形成饰片的操作速度慢,且该饰片在加热以前相当软、定位性不佳,在填入该大底胚料时容易移动,会导致不良品。
另外,针对饰片与大底胚料分别采用橡胶及乙烯-乙酸乙烯共聚物材质,所应用的成型方法,是先对一已熟化的橡胶饰片的结合面进行打粗、上胶等作业,再将该橡胶饰片放入一模具中,接着,将一已发泡完成的大底胚料置入该模具中,再闭模以进行热压成型及结合作业,促使该大底胚料在热压塑型的同时可与该橡胶饰片结合。
这种成型方法因为要预先对饰片进行打粗、上胶作业,也会延长制造过程且会增加制造成本。
发明内容
本发明的目的在于提供一种可简化制程且可提升产能、提高品质的具橡胶饰片的鞋底制造方法。
本发明具橡胶饰片的鞋底制造方法,包含下列步骤:(A)预先制备一橡胶饰片,该橡胶饰片具有一下层及一固设在该下层上的上层,该上层内含的交联剂浓度低于该下层,使该下层已完成交联反应且呈熟化状态,但是该上层尚残存交联能力。(B)将该橡胶饰片放入一模具中。(C)将一大底胚料填入该模具中,且使该大底胚料与该橡胶饰片的上层接触。(D)对该模具进行热压,且使该橡胶饰片的上层利用残存的交联能力继续与该大底胚料完成交联反应。(E)开模,获得一具有橡胶饰片的鞋底。
借此,该饰片可预先大量制作,且利用该饰片残存的交联能力,可在该模具内部直接与该大底胚料进行交联反应而固结成一体,该鞋底的成型速度快、产能佳,可降低制造成本。
附图说明
下面结合附图及实施例对本发明进行详细说明:
图1是本发明一较佳实施例的流程图;
图2是本发明上述较佳实施例所应用设备的部份平面分解图,说明一饰片可放置在一模具的定位部中;
图3是本发明上述较佳实施例的闭模成型示意图,说明将一大底胚料填入模具内可与该饰片一上层进行交联固结;
图4是本发明上述较佳实施例所制成的鞋底剖面图。
具体实施方式
如图1所示,本发明具橡胶饰片的鞋底制造方法较佳实施例,包含下列步骤:
步骤一:配合参阅图2,预先制备一模具100及一橡胶饰片10。该模具100具有一底模110及一与该底模110相对设置的顶模120,该底模110具有一由一顶面凹设而成的模穴130、一设置在该模穴130中的定位部140,该定位部140是由一分色岭150所圈绕形成。该橡胶饰片10具有一下层11及一固设在该下层11上的上层12,该上层12内含的交联剂浓度低于该下层11,且该下层11已完成交联反应且呈熟化状态,但是该上层12尚残存交联能力,也就是说,将构成下层11及上层12的生料叠置并进行加热且控制加热时间,由于该下层11的交联剂浓度较高、交联反应速度较快,而上层12交联剂浓度较低、交联反应速度较慢,所以当下层11完成交联反应并达熟化状态时,该上层12的交联剂并未完全反应完成,仍残存交联能力,且该下层11可与该上层12因为交联而固结成一体。
步骤二:将该橡胶饰片10放入该模具100的定位部140中。
步骤三:如图3所示,将一大底胚料20填入该模具100的模穴130中,且使该大底胚料20与该橡胶饰片10的上层12接触。本实施例的大底胚料20可为具有交联剂的橡胶生料。
步骤四:如图3所示,该顶模120与该底模110产生闭合,且对该模具100进行热压,该橡胶饰片10的上层12利用残存的交联能力继续与该大底胚料20完成交联反应,且与该大底胚料20产生稳固结合。
步骤五:如图4所示开模,就可获得一具有橡胶饰片10的鞋底30。
因此,利用上述步骤所制成的鞋底,是可在底部形成饰片,而可达到装饰及止滑目的。
另外,当该大底胚料20是选用已发泡的乙烯-乙酸乙烯共聚物胚材时,则在上述步骤四与该步骤五之间,就必须增设一步骤四’,且该步骤四’是对该模具100进行冷却,使该橡胶饰片10及该大底胚料20定型。
且本发明的鞋底制造方法具有下列功效:
一、该饰片10可预先大量制作,且可免去打粗、上胶等作业,制作快速、成本低。
二、该饰片10放置在该模具100的定位部140中后,因为下层11已完成交联反应而可产生较佳的定位性,不会受该大底胚料20的置入动作而产生位移。
三、该饰片10利用该上层12残存的交联能力,可在该模具100内部直接与该大底胚料20进行交联反应而固结成一体,该鞋底30的成型速度快、产能佳,可降低制造成本。

Claims (4)

1.一种具橡胶饰片的鞋底制造方法,其特征在于包含下列步骤:
(A)预先制备一橡胶饰片,该橡胶饰片具有一下层及一固设在该下层上的上层,该上层内含的交联剂浓度低于该下层,使该下层已完成交联反应且呈熟化状态,但是该上层尚残存交联能力;
(B)将该橡胶饰片放入一模具中;
(C)将一大底胚料填入该模具中,且使该大底胚料与该橡胶饰片的上层接触;
(D)对该模具进行热压,且使该橡胶饰片的上层利用残存的交联能力继续与该大底胚料完成交联反应;及
(E)开模,获得一具有橡胶饰片的鞋底。
2.如权利要求1所述的具橡胶饰片的鞋底制造方法,其特征在于:该步骤(B)的橡胶饰片是放置定位在该模具的一定位部中,该定位部是由一分色岭所圈绕形成。
3.如权利要求1所述的具橡胶饰片的鞋底制造方法,其特征在于:该步骤(C)的大底胚料为具有交联剂的橡胶生料。
4.如权利要求1所述的具橡胶饰片的鞋底制造方法,其特征在于:该步骤(C)的大底胚料为已发泡的乙烯-乙酸乙烯共聚物,且该鞋底制造方法还包含有一介于步骤(D)与步骤(E)之间的步骤(D-1),该步骤(D-1)是对该模具进行冷却,使该橡胶饰片及大底胚料定型。
CNB2005100983704A 2005-09-08 2005-09-08 具橡胶饰片的鞋底制造方法 Expired - Fee Related CN100400276C (zh)