CN1762798A - 磷酸铁锂的制备方法 - Google Patents
磷酸铁锂的制备方法 Download PDFInfo
- Publication number
- CN1762798A CN1762798A CNA2005100297254A CN200510029725A CN1762798A CN 1762798 A CN1762798 A CN 1762798A CN A2005100297254 A CNA2005100297254 A CN A2005100297254A CN 200510029725 A CN200510029725 A CN 200510029725A CN 1762798 A CN1762798 A CN 1762798A
- Authority
- CN
- China
- Prior art keywords
- lithium phosphate
- ferric lithium
- solution
- product
- temperature
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
Description
化合物 | Li3PO4 | Fe(OH)2 | Fe(OH)3 | FePO4 |
ksp值 | 3.2×10-9 | 8×10-16 | 4×10-38 | 1.3×10-22 |
Claims (1)