CN1410479A - 溶剂稀释软膜防锈油 - Google Patents

溶剂稀释软膜防锈油 Download PDF

Info

Publication number
CN1410479A
CN1410479A CN 02116500 CN02116500A CN1410479A CN 1410479 A CN1410479 A CN 1410479A CN 02116500 CN02116500 CN 02116500 CN 02116500 A CN02116500 A CN 02116500A CN 1410479 A CN1410479 A CN 1410479A
Authority
CN
China
Prior art keywords
oil
rust
forming material
petroleum
type anti
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN 02116500
Other languages
English (en)
Other versions
CN1142261C (zh
Inventor
雷军
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CNB021165009A priority Critical patent/CN1142261C/zh
Publication of CN1410479A publication Critical patent/CN1410479A/zh
Application granted granted Critical
Publication of CN1142261C publication Critical patent/CN1142261C/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本发明涉及一种复合型防锈添加剂,以及石油溶剂与该添加剂和成膜材料混合调制而成溶剂稀释型软膜防锈油。本发明的目的在于提供一种复合型防锈添加剂和一种复合成膜材料,与石油溶剂混合调制而成的防锈油。克服了现有技术的不足,极大的提高了产品的防锈性。盐雾箱试验,钢片通过14天不锈,湿热试验钢片,铜片通过60天不锈,防锈添加剂,成膜材料与石油溶剂完全混溶。呈现为均匀液体。

Description

溶剂稀释型软膜防锈油
技术领域
本发明涉及一种复合型防锈添加剂,以及石油溶剂与该添加剂和成膜材料混合而成溶剂稀释型软膜防锈油。
技术背景
现有的溶剂稀释型软膜防锈油当前存在的主要问题是抗盐雾性能差,一般的产品盐雾箱试验10号钢片不到5天就生锈,黄铜、紫铜不到4天生锈,而且由于防锈剂和成膜材料在溶剂中难以完全溶解,产品的油基稳定性差,储存后产品发生分层和沉淀,影响产品的使用效果,不能满足沿海地区和海上运输黑色金属和有色金属制品的封存防锈要求。
发明内容
本发明的目的在于提出一种复合型防锈添加剂和一种复合成膜材料,与石油溶剂混合调制而成的防锈油,克服了现有技术的不足。极大的提高了产品的防锈性,盐雾箱试验钢片,铜片通过14天不锈,湿热试验钢片,铜片通过60天不锈,防锈添加剂,成膜材料与石油溶剂完全混溶,呈现为均匀液体。
本发明中,复合型防锈添加剂是液体石油磺酸钡,氧化石油脂钡皂,二聚酸、苯三唑十八胺和司苯80等混合物,成膜材料是石油树脂,乙烯丙烯共聚物(OCP),MHV150精矿油。
在本发明的复合型防锈添加剂中,液态石油磺酸钡∶氧化石油脂钡皂∶二聚酸∶苯三唑十八胺∶司苯80(重量比)30~40∶40~50∶10~15∶4~5∶10~15。
在本发明的复合成膜材料中石油树脂∶乙烯丙烯共聚物(OCP)∶MHV150精矿油(重量比)为30~40∶20~30∶20~30。
在本发明中,复合型防锈添加剂,复合成膜材料,溶剂汽油混合物中比例分别15~20%,16~22%。
本发明的复合型防锈添加剂,复合成膜材料,能与石油溶剂充分的溶解。调制而成的溶剂稀释型软膜防锈油具有极好抗盐雾性能和抗湿热性能,油膜薄,不大于20μm,油膜透明,能满足沿海,海上运输和湿热地区有色金属和黑色金属的制品的封存防锈要求,封存防锈期3~5年。
具体实施方式
本发明将通过实施例进一步说明。
实施例1
该复合型防锈添加剂成分(重量比)
石油树酯                  36
氧化石油脂钡皂            48
二聚酸                    7
苯三唑十八胺              2
司苯80                    7
将上述成分混合,制得本发明的复合型防锈添加剂。
实施例2
该复合成膜材料成分
石油树酯                      42
乙烯丙烯共聚物                33
HVI精制矿油                   25
将上述各组分混合均匀,得到该复合成膜材料。
实施例3
200号溶剂汽油80份,灯用煤油29份,2.6二叔丁基对甲酚1份。
上述各组份混合制得石油溶剂。
该石油溶剂60份,与实施例1复合型防锈添加剂20份,实施例2复合成膜材料20份混合,可得到溶剂稀释型软膜防锈油。

Claims (4)

1、本发明中复合型防锈添加剂是液体石油磺酸钡氧化石油脂钡皂,二聚酸,苯三唑十八胺和司苯80混合物。成膜材料是石油树脂,乙烯丙烯共聚物(OCP)MHV150精矿油。
2、根据权利要求1所述的复化型防锈添加剂,其特征在于:液态石油磺酸钡∶氧化石油脂钡皂∶二聚酸∶苯三唑十八胺∶司本80(重量比)为30~40∶40~50∶10~15∶4~5∶10~15。复合成膜材料中石油树脂∶乙烯丙烯共聚物(OCP)∶HVI150精矿油为30~40∶20~30∶20~30。
3、本发明中复合型防锈添加剂,复合成膜材料,溶剂汽油混合物中比例分别为15~20%,16~22%。
4、根据权利要求1所述的复合型防锈添加剂,其特征在于:具有极好抗盐雾性能和抗湿热性能,油膜不大于20μm油膜透明,能满足沿海,海上运输和湿热地区有色金属和黑色金属的封存防锈要求。
CNB021165009A 2002-04-03 2002-04-03 溶剂稀释型软膜防锈油 Expired - Fee Related CN1142261C (zh)