CN1388197A - 环保型喷胶及其工艺方法和用途 - Google Patents

环保型喷胶及其工艺方法和用途 Download PDF

Info

Publication number
CN1388197A
CN1388197A CN 02115305 CN02115305A CN1388197A CN 1388197 A CN1388197 A CN 1388197A CN 02115305 CN02115305 CN 02115305 CN 02115305 A CN02115305 A CN 02115305A CN 1388197 A CN1388197 A CN 1388197A
Authority
CN
China
Prior art keywords
environment
friendly type
spray glue
glue
type spray
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN 02115305
Other languages
English (en)
Other versions
CN1253521C (zh
Inventor
黄楚填
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Huang Chutian
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN 02115305 priority Critical patent/CN1253521C/zh
Publication of CN1388197A publication Critical patent/CN1388197A/zh
Application granted granted Critical
Publication of CN1253521C publication Critical patent/CN1253521C/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本发明公开一种环保型喷胶,该喷胶的最佳重量配比为:热塑性弹性体SBS 8%、松香6%、氢化松香7%、石油树脂4%、增粘树脂3%、6#溶剂油49.5%、丙酮5%、环已烷15%、丁脂2%和防老剂0.5%。其配制工艺方法如下:先将定量的6#溶剂油、丙酮、环已烷投入搅拌器内,开动机器搅拌均匀成为混合溶液;再依次把松香、氢化松香、石油树脂、增粘树脂、丁脂和防老剂投入搅拌器内在常温下搅拌约6小时使所有物料完全溶解成淡黄色胶液然后80目过滤即可。本发明的环保型喷胶无毒、成本低廉且干燥快,特别适合作为制造软体家俱的粘合剂。

Description

环保型喷胶及其工艺方法和用途
                        技术领域
本发明涉及一种粘合剂,尤其涉及一种环保型喷胶及其制作工艺和用途。
                        背景技术
目前市场上出现的热塑性弹性体SBS溶剂型喷胶,都不同比例的含有三苯(苯、甲苯、二甲苯)及卤代氢类剧毒、高毒性溶剂,三苯可以致癌,卤代氢类能影响人体新陈代谢及造成肝脏中毒,无论是长时间接触或短时间接触,都会不同程度地造成人体的急、慢性中毒,同时给周围环境造成严重的污染。专利号为90106727.X的发明专利的配方虽然解决了毒性污染的问题,但其成本较高,而且仅限于作为彩印覆膜的裱胶,另外,由于其配方采用了120#溶剂油,其干燥时间较长,因而限制其作为软体家俱粘合剂的应用。
                           发明内容
本发明的目的在于克服现有技术的不足之处而提供一种无毒、干燥快的环保型喷胶及其工艺方法和用途。
为达到上述发明目的,本发明的环保型喷胶的重量配比为:该喷胶的重量配比为:热塑性弹性体SBS5-15%、松香5-10%、氢化松香5-10%、石油树脂2-6%、增粘树脂2-6%、6#溶剂油45-55%、丙酮2-10%和环己烷10-20%;各组分之和为100%。
制作本发明的环保型喷胶的工艺方法如下:
a.先将定量的6#溶剂油、丙酮、环己烷投入搅拌器内,开动机器搅拌均匀成为混合溶液;
b.再将定量的热塑性弹性体SBS投入搅拌器内搅拌;
c.最后将定量的松香、氢化松香、石油树脂、增粘树脂、丁脂和防老剂投入搅拌器内搅拌;
d.以上物料全部投入搅拌器内后继续常温搅拌溶解约6小时,检查所有物料完全溶解成淡黄色胶液,然后80目过滤即可。
由于本发明的环保型喷胶无毒、且采用干燥快的6#溶剂油,因此特别适合应用于软体家俱的粘合,该应用也是本发明的重点之一。使用本发明的环保型喷胶粘贴软体家俱的方法如下:
a.清洁待粘贴软体家俱材质的贴面;
b.用喷枪把环保型喷胶均匀地喷涂在待粘贴材质的贴面;
c.放置1至3分钟,以喷涂层不粘手为准,即可加压粘合。
与现有技术相比,本发明的环保型喷胶具有如下优点:
1、本配方中不含三苯,及卤代烃类高毒性溶剂。
2、采用6#溶剂油,对人体基本无害,丙酮、环己烷都是低毒、微毒类溶剂,而且含量很低,只占胶水的15-20%,所以本配方对人体基本无害,超过国家的安全标准,符合环保及保护工人身心健康的要求。
3、本发明的环保型喷胶无味,喷涂均匀,成本低廉。
4、6#溶剂油干燥快,传统刷胶干燥时间,一般需要15至20分钟,而本发明的环保型喷胶干燥时间只需1至3分钟,大大地提高了施工效率,从而开辟了该类产品在制作软体家俱中的应用领域。
5、本发明的环保型喷胶粘性开放时间长,可达15至20分钟,操作时间弹性大。
                         具体实施方式
下面以实施例对本发明作进一步的说明:
该喷胶的最佳重量配比为:热塑性弹性体SBS8%、松香6%、氢化松香7%、石油树脂4%、增粘树脂3%、6#溶剂油49.5%、丙酮5%、环己烷15%、丁脂2%和防老剂0.5%。
制作本发明的环保型喷胶的工艺方法如下:
a.先将定量的6#溶剂油、丙酮、环己烷投入搅拌器内,开动机器搅拌均匀成为混合溶液;
b.再将定量的热塑性弹性体SBS投入搅拌器内搅拌;
c.最后将定量的松香、氢化松香、石油树脂、增粘树脂、丁脂和防老剂投入搅拌器内搅拌;
d.以上物料全部投入搅拌器内后继续常温搅拌溶解约6小时,检查所有物料完全溶解成淡黄色胶液,然后80目过滤即可。
本发明的环保型喷胶最适合用于粘贴软体家俱,该用途是本发明要求保护的重点之一,其施工方法包括如下步骤:
a.清洁待粘贴软体家俱材质的贴面;
b.用喷枪把环保型喷胶均匀地喷涂在待粘贴材质的贴面;
c.放置1至3分钟,以喷涂层不粘手为准,即可加压粘合。

Claims (6)

1、一种环保型喷胶,其特征在于:该喷胶的重量配比为:热塑性弹性体SBS5-15%、松香5-10%、氢化松香5-10%、石油树脂2-6%、增粘树脂2-6%、6#溶剂油45-55%、丙酮2-10%和环己烷10-20%;各组分之和为100%。
2、根据权利要求1所述的环保型喷胶,其特征在于:该喷胶的重量配比还包括1-3%的丁脂和0.5-1.0%的防老剂。
3、根据权利要求2所述的环保型喷胶,其特征在于:该喷胶的最佳重量配比为:热塑性弹性体SBS8%、松香6%、氢化松香7%、石油树脂4%、增粘树脂3%、6#溶剂油49.5%、丙酮5%、环己烷15%、丁脂2%和防老剂0.5%。
4、一种如权利要求1所述环保型喷胶的配制工艺方法,其特征在于:该方法包括如下步骤:
a.先将定量的6#溶剂油、丙酮、环己烷投入搅拌器内,开动机器搅拌均匀成为混合溶液;
b.再将定量的热塑性弹性体SBS投入搅拌器内搅拌;
c.最后将定量的松香、氢化松香、石油树脂和增粘树脂投入搅拌器内搅拌;
d.以上物料全部投入搅拌器内后继续常温搅拌溶解约6小时,检查所有物料完全溶解成淡黄色胶液,然后80目过滤即可。
5、根据权利要求4所述的环保型喷胶的配制工艺方法,其特征在于:在步骤C之后投入适量的丁脂和防老剂与其它物料充分搅拌混合。
6、一种使用权利要求1或3所述环保型喷胶粘贴软体家俱的方法,其特征在于:该方法包括如下步骤:
a.清洁待粘贴软体家俱材质的贴面;
b.用喷枪把环保型喷胶均匀地喷涂在待粘贴材质的贴面;
c.放置1至3分钟,以喷涂层不粘手为准,即可加压粘合。
CN 02115305 2002-05-27 2002-05-27 环保型喷胶及其工艺方法和用途 Expired - Fee Related CN1253521C (zh)