CN117162216A - Paint falling restoration method for wooden doors and windows - Google Patents
Paint falling restoration method for wooden doors and windows Download PDFInfo
- Publication number
- CN117162216A CN117162216A CN202311363292.0A CN202311363292A CN117162216A CN 117162216 A CN117162216 A CN 117162216A CN 202311363292 A CN202311363292 A CN 202311363292A CN 117162216 A CN117162216 A CN 117162216A
- Authority
- CN
- China
- Prior art keywords
- paint
- hemp
- ash
- grinding
- oil
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses a paint falling restoration method for wooden doors and windows, which comprises the following steps: s1, white discharge: paint films are whitened, paint of the wooden doors and windows falls off, and wooden member oil decorations are armored, discolored and peeled off; s2, surface polishing: firstly, paint removal is carried out, and then, the surface of the wood structure subjected to paint removal is polished; s3, cleaning and caulking: cleaning the joint filling; s4, scraping ash and sticking linen; s5, grinding hemp ash: grinding the hemp with sand stone after the hemp is dried, grinding the hemp cloth to form a nap, hanging the nap with the grinded hemp threads, and cleaning the floating area; s6, scraping and coating the pressed hemp ash: after grinding the hemp ash, scraping, coating, pressing and polishing the hemp ash; s7, brushing raw paint water for the first time; s8, ash supplementing; s9, brushing paint water for the second time; s10, brushing the first-time lacquer; s11, brushing the second-time lacquer. According to the invention, the firmness of repairing the paint surface and the wood structure is improved by treating the original paint surface; the traditional method of adopting the lacquer has the advantages of durability, heat resistance, water resistance, corrosion resistance and the like.
Description
Technical Field
The invention relates to the technical field of paint repair for wood doors and windows, in particular to a paint falling repair method for wood doors and windows.
Background
With the continuous development of the social economy of China, the living standard is improved, people have higher pursuit on cultural life, and the people are more and more interested in the historical culture and national characteristics of China. Ancient towns and villages in various places of the country become hot spots for travel and leisure, and are also an important component in the field of building for the development and repair of ancient buildings.
The wooden door and window in the ancient architecture is exposed to the outside, and the surface layer of the wooden door and window is easy to fall off, crack, bulge and other problems after long-time wind and sun exposure; therefore, we propose a method for repairing paint falling off of wooden doors and windows.
Disclosure of Invention
The invention aims to provide a paint falling-off repairing method for wood doors and windows, which aims to solve the problems in the prior art.
In order to achieve the above purpose, the present invention provides the following technical solutions: a paint falling restoration method for wooden doors and windows comprises the following steps:
s1, white discharge: paint films are whitened, paint of the wooden doors and windows falls off, and wooden member oil decorations are armored, discolored and peeled off;
s2, surface polishing: firstly, paint removal is carried out, and then, the surface of the wood structure subjected to paint removal is polished;
s3, cleaning and caulking: cleaning the joint filling;
s4, scraping ash and sticking linen;
s5, grinding hemp ash: grinding the hemp with sand stone after the hemp is dried, grinding the hemp cloth to form a nap, hanging the nap with the grinded hemp threads, and cleaning the floating area;
s6, scraping and coating the pressed hemp ash: after grinding the hemp ash, scraping, coating, pressing and polishing the hemp ash;
s7, brushing raw paint water for the first time;
s8, ash supplementing;
s9, brushing paint water for the second time;
s10, brushing the first-time lacquer;
s11, brushing the second-time lacquer.
Preferably, the paint is removed in the step S2 by adopting a paint remover, and then the waste paint is cleaned by a cleaning tool; after the surface to be repaired is dried, the residual paint remover is cleaned by brushing the diluent; and polishing the surface to be repaired.
Preferably, the polishing standard is that the surface of the wood structure to be repaired is burr-shaped.
Preferably, in the step S4, the dust scraping and linen attaching cloth is as follows: firstly, the coarse ash is coated and scraped, and then the linen is pasted.
Preferably, the linen: firstly, mixing the oil fullness and the blood material into plasma, and coating the plasma on the lime; sticking the linen on the oil-filled plasma; after the hemp is well adhered, pressing with a hemp presser to make the oil slurry soak the hemp surface.
Preferably, if the base slurry is not saturated with the hemp, the slurry is prepared by filling with oil and water, the dried hemp is brushed again, and the hemp presser is used for pressing along with the sticking, so that the oil slurry is saturated with the hemp surface.
Preferably, the step S6 is to knife-coat and press the lime: adding middle ash fully with oil, mixing, smearing on hemp, repeatedly grinding and pressing to tightly combine the putty with hemp, covering with a layer of putty, trimming corners, naturally drying, and grinding to remove dust; after the equal-pressure flax ash is thoroughly dried, coating a layer of putty prepared by filling oil and intermediate ash on the flax ash, and after the equal-pressure flax ash is thoroughly dried, grinding and scraping; grinding the surface of the sand stone after the middle ash is dried; leveling corners, frame wires and slope edges by using fine ash and spreading a layer of fine ash.
Preferably, the raw lacquer material water consists of raw lacquer, tung oil, methyl methacrylate and polyethylene wax.
Preferably, the lacquer is prepared from raw lacquer, tung oil and mineral powder.
Preferably, after the step S3 of cleaning the caulking, an insect-proof treatment is performed.
Compared with the prior art, the invention has the beneficial effects that:
the firmness of the repaired paint surface and the wood structure is improved through the treatment of the original paint surface;
the traditional method of the lacquer is adopted, the lacquer is prepared from raw lacquer, tung oil and mineral powder, and has the advantages of durability, heat resistance, water resistance, corrosion resistance and the like.
Drawings
The accompanying drawings are included to provide a further understanding of the invention and are incorporated in and constitute a part of this specification, illustrate the invention and together with the embodiments of the invention, serve to explain the invention. In the drawings:
fig. 1 is a flow chart of the present invention.
Description of the embodiments
For the purpose of making the objects, technical solutions and advantages of the embodiments of the present invention more apparent, the technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings in the embodiments of the present invention, and it is apparent that the described embodiments are some embodiments of the present invention, but not all embodiments. All other embodiments, based on the embodiments of the invention, which are apparent to those of ordinary skill in the art without inventive faculty, are intended to be within the scope of the invention. Thus, the following detailed description of the embodiments of the invention, as presented in the figures, is not intended to limit the scope of the invention, as claimed, but is merely representative of selected embodiments of the invention.
Examples
Referring to fig. 1, in an embodiment of the invention, a method for repairing paint falling off of a wooden door and window includes the following steps:
s1, white discharge: paint films are whitened, paint of the wooden doors and windows falls off, and wooden member oil decorations are armored, discolored and peeled off;
s2, surface polishing: firstly, paint removal is carried out, then the surface of the wood structure after paint removal is polished, paint removal is carried out by adopting a paint remover in the step S2, and then a cleaning tool is used for cleaning waste paint; after the surface to be repaired is dried, the residual paint remover is cleaned by brushing the diluent; then polishing the surface to be repaired, wherein the polishing standard is that the surface of the wood structure to be repaired is burr-shaped;
s3, cleaning and caulking: cleaning the joint filling; after the gap filling is cleaned, insect prevention treatment is carried out, so that the wood structure is prevented from being damaged by insects;
s4, scraping ash and sticking linen, wherein the ash and sticking linen is scraped in the S4: firstly, coating coarse ash, and then pasting linen; the linen is pasted: firstly, mixing the oil fullness and the blood material into plasma, and coating the plasma on the lime; sticking the linen on the oil-filled plasma; after the hemp is well adhered, pressing with a hemp presser to enable the oil slurry to soak the surface of the hemp; if the bottom slurry does not saturate the hemp, the slurry is prepared by filling with oil and water, the dried hemp is brushed again, and the hemp presser is used for pressing along with sticking again, so that the oil slurry saturates the surface of the hemp;
s5, grinding hemp ash: grinding the hemp with sand stone after the hemp is dried, grinding the hemp cloth to form a nap, hanging the nap with the grinded hemp threads, and cleaning the floating area;
s6, scraping and coating the pressed hemp ash: after the hemp ash is ground, scraping, pressing and polishing the hemp ash, wherein the step S6 is to scrape, press the hemp ash: adding middle ash fully with oil, mixing, smearing on hemp, repeatedly grinding and pressing to tightly combine the putty with hemp, covering with a layer of putty, trimming corners, naturally drying, and grinding to remove dust; after the equal-pressure flax ash is thoroughly dried, coating a layer of putty prepared by filling oil and intermediate ash on the flax ash, and after the equal-pressure flax ash is thoroughly dried, grinding and scraping; grinding the surface of the sand stone after the middle ash is dried; leveling corners, frame wires and slope edges by using fine ash and spreading a layer of fine ash;
s7, brushing raw paint water for the first time, wherein the raw paint water consists of raw paint, tung oil, methyl methacrylate and polyethylene wax;
s8, ash supplementing;
s9, brushing raw paint water for the second time, wherein the raw paint water consists of raw paint, tung oil, methyl methacrylate and polyethylene wax;
s10, brushing a first-time lacquer, wherein the lacquer is prepared from raw lacquer, tung oil and mineral powder;
s11, brushing a second-time lacquer, wherein the lacquer is prepared from raw lacquer, tung oil and mineral powder.
Examples
Referring to fig. 1, in an embodiment of the invention, a method for repairing paint falling off of a wooden door and window includes the following steps:
s1, white discharge: paint films are whitened, paint of the wooden doors and windows falls off, and wooden member oil decorations are armored, discolored and peeled off;
s2, surface polishing: firstly, paint removal is carried out, then the surface of the wood structure after paint removal is polished, paint removal is carried out by adopting a paint remover in the step S2, and then a cleaning tool is used for cleaning waste paint; after the surface to be repaired is dried, the residual paint remover is cleaned by brushing the diluent; then polishing the surface to be repaired, wherein the polishing standard is that the surface of the wood structure to be repaired is burr-shaped;
s3, cleaning and caulking: cleaning the joint filling;
s4, scraping ash and sticking linen, wherein the ash and sticking linen is scraped in the S4: firstly, coating coarse ash, and then pasting linen; the linen is pasted: firstly, mixing the oil fullness and the blood material into plasma, and coating the plasma on the lime; sticking the linen on the oil-filled plasma; after the hemp is well adhered, pressing with a hemp presser to enable the oil slurry to soak the surface of the hemp; if the bottom slurry does not saturate the hemp, the slurry is prepared by filling with oil and water, the dried hemp is brushed again, and the hemp presser is used for pressing along with sticking again, so that the oil slurry saturates the surface of the hemp;
s5, grinding hemp ash: grinding the hemp with sand stone after the hemp is dried, grinding the hemp cloth to form a nap, hanging the nap with the grinded hemp threads, and cleaning the floating area;
s6, scraping and coating the pressed hemp ash: after the hemp ash is ground, scraping, pressing and polishing the hemp ash, wherein the step S6 is to scrape, press the hemp ash: adding middle ash fully with oil, mixing, smearing on hemp, repeatedly grinding and pressing to tightly combine the putty with hemp, covering with a layer of putty, trimming corners, naturally drying, and grinding to remove dust; after the equal-pressure flax ash is thoroughly dried, coating a layer of putty prepared by filling oil and intermediate ash on the flax ash, and after the equal-pressure flax ash is thoroughly dried, grinding and scraping; grinding the surface of the sand stone after the middle ash is dried; leveling corners, frame wires and slope edges by using fine ash and spreading a layer of fine ash;
s7, brushing raw paint water for the first time, wherein the raw paint water consists of raw paint, tung oil, methyl methacrylate and polyethylene wax;
s8, ash supplementing;
s9, brushing raw paint water for the second time, wherein the raw paint water consists of raw paint, tung oil, methyl methacrylate and polyethylene wax;
s10, brushing a first-time lacquer, wherein the lacquer is prepared from raw lacquer, tung oil and mineral powder;
s11, brushing a second-time lacquer, wherein the lacquer is prepared from raw lacquer, tung oil and mineral powder.
The firmness of the repaired paint surface and the wood structure is improved through the treatment of the original paint surface; the traditional method of the lacquer is adopted, the lacquer is prepared from raw lacquer, tung oil and mineral powder, and has the advantages of durability, heat resistance, water resistance, corrosion resistance and the like.
Finally, it should be noted that: the foregoing description is only a preferred embodiment of the present invention, and the present invention is not limited thereto, but it is to be understood that modifications and equivalents of some of the technical features described in the foregoing embodiments may be made by those skilled in the art, although the present invention has been described in detail with reference to the foregoing embodiments. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention should be included in the protection scope of the present invention.
Claims (10)
1. The paint falling restoration method for the wooden doors and windows is characterized by comprising the following steps of:
s1, white discharge: paint films are whitened, paint of the wooden doors and windows falls off, and wooden member oil decorations are armored, discolored and peeled off;
s2, surface polishing: firstly, paint removal is carried out, and then, the surface of the wood structure subjected to paint removal is polished;
s3, cleaning and caulking: cleaning the joint filling;
s4, scraping ash and sticking linen;
s5, grinding hemp ash: grinding the hemp with sand stone after the hemp is dried, grinding the hemp cloth to form a nap, hanging the nap with the grinded hemp threads, and cleaning the floating area;
s6, scraping and coating the pressed hemp ash: after grinding the hemp ash, scraping, coating, pressing and polishing the hemp ash;
s7, brushing raw paint water for the first time;
s8, ash supplementing;
s9, brushing paint water for the second time;
s10, brushing the first-time lacquer;
s11, brushing the second-time lacquer.
2. The method for repairing paint falling off from wooden doors and windows according to claim 1, wherein the paint is removed in the step S2 by adopting a paint remover, and then the waste paint is cleaned by a cleaning tool; after the surface to be repaired is dried, the residual paint remover is cleaned by brushing the diluent; and polishing the surface to be repaired.
3. The paint falling restoration method for wooden doors and windows according to claim 2, wherein the polishing standard is that the surface of the wooden structure to be restored is burr-shaped.
4. The paint falling restoration method for wooden doors and windows according to claim 1, wherein the step S4 is to scrape ash and paste linen: firstly, the coarse ash is coated and scraped, and then the linen is pasted.
5. The paint falling restoration method for wooden doors and windows according to claim 4, wherein the linen is attached to: firstly, mixing the oil fullness and the blood material into plasma, and coating the plasma on the lime; sticking the linen on the oil-filled plasma; after the hemp is well adhered, pressing with a hemp presser to make the oil slurry soak the hemp surface.
6. The method for repairing paint falling off of wooden doors and windows according to claim 5, wherein if the base slurry is not saturated with hemp, the slurry is prepared by filling with oil and water, the dried hemp is brushed again, and the hemp presser is used for pressing along with sticking again, so that the oil slurry is saturated with the hemp surface.
7. The paint falling restoration method for wooden doors and windows according to claim 1, wherein the step S6 is to scrape and paint and press the putty: adding middle ash fully with oil, mixing, smearing on hemp, repeatedly grinding and pressing to tightly combine the putty with hemp, covering with a layer of putty, trimming corners, naturally drying, and grinding to remove dust; after the equal-pressure flax ash is thoroughly dried, coating a layer of putty prepared by filling oil and intermediate ash on the flax ash, and after the equal-pressure flax ash is thoroughly dried, grinding and scraping; grinding the surface of the sand stone after the middle ash is dried; leveling corners, frame wires and slope edges by using fine ash and spreading a layer of fine ash.
8. The method for repairing paint falling off of wooden doors and windows according to claim 1, wherein raw paint water consists of raw paint, tung oil, methyl methacrylate and polyethylene wax.
9. The method for repairing paint falling off of wooden doors and windows according to claim 1, wherein the lacquer is prepared from raw lacquer, tung oil and mineral powder.
10. The paint falling restoration method for wooden doors and windows according to claim 1, wherein after the step S3 of cleaning and caulking, insect prevention treatment is performed.