CN109555316A - Environment protection architecture construction method - Google Patents

Environment protection architecture construction method Download PDF

Info

Publication number
CN109555316A
CN109555316A CN201811351202.5A CN201811351202A CN109555316A CN 109555316 A CN109555316 A CN 109555316A CN 201811351202 A CN201811351202 A CN 201811351202A CN 109555316 A CN109555316 A CN 109555316A
Authority
CN
China
Prior art keywords
metope
wall surface
treated
mortar
putty
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201811351202.5A
Other languages
Chinese (zh)
Inventor
邓泽华
李海深
邓恒华
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Crown Heng Construction Engineering Co Ltd
Original Assignee
Crown Heng Construction Engineering Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Crown Heng Construction Engineering Co Ltd filed Critical Crown Heng Construction Engineering Co Ltd
Priority to CN201811351202.5A priority Critical patent/CN109555316A/en
Publication of CN109555316A publication Critical patent/CN109555316A/en
Pending legal-status Critical Current

Abstract

The invention discloses environment protection architecture construction methods, include the following steps step 1, preparation of construction: a. tool prepares, including degumming agent, scraper plate, sand paper, bandage, guiding ruler, clearance gauge, angle grinder, land plaster, latex solution, cellulose aqueous solution etc.;Step 2, wall surface leveling: a. to step 1 treated metope does corner protector, corner protector 1:2 cement mortar, mortar slightly receive it is dry after smear into fillet with smoothing out with the fingers angle device;Step 3, metope cleans: a. is to pasting one layer of glass grid cloth or silk item at step 2 treated gap;Step 4, wall plaster: a. first sprays one of glue or varnish back cover to the inner wall surface in step 3;Step 5, sprayed coating wall surface spraying: is carried out with spray gun to step 4 treated metope.By the construction techniques of multi-step in the present invention, the buildings waterproof effect after making construction is improved, while the flat and smooth degree in inner wall of building face being made to be improved, to guarantee the normal use of building.

Description

Environment protection architecture construction method
Technical field
The present invention relates to technical field of building construction more particularly to environment protection architecture construction methods.
Background technique
Sponge city is a kind of urban construction new concept that country proposes.National house and town and country construction portion are required to 2020 The area in south, 20% or more completed region of the city reaches target call, and the area to 80% or more the year two thousand thirty reaches target call. It can thus be seen that country improve resident living environment and Urban Water Environment there is an urgent need to sponge city requirement city is under Have the function of infiltration, stagnant, storage, net, use, row when rain.It is key point for the problem of saving after rainwater-collecting, it is effective to guarantee Saving for rainwater avoids effect of the water resource waste in sponge city extremely important.
But construction techniques is relatively simple in existing sponge city, the buildings waterproof effect after construction is poor, together When inner wall of building face flat and smooth degree it is lower, thus influence building normal use.
Summary of the invention
1. technical problems to be solved
The purpose of the present invention is to solve construction techniques in sponge city in the prior art is relatively simple, after construction Buildings waterproof effect it is poor, while the lower problem of the flat and smooth degree in inner wall of building face, and the environment protection architecture construction party proposed Method.
2. technical solution
To achieve the goals above, present invention employs following technical solutions:
Environment protection architecture construction method, includes the following steps:
Step 1, preparation of construction:
A. tool prepare, including degumming agent, scraper plate, sand paper, bandage, guiding ruler, clearance gauge, angle grinder, land plaster, latex solution, Cellulose aqueous solution etc. hang vertical according to the smooth vertical case of substrate surface;
B. substrate surface is thoroughly scrubbed, is washed;
C. the base after scrubbing is carried out smearing bedding mortar, bottom is uniformly plated in using cement mixed mortar, with ruler school Rough hair face is scraped in direct join;
Step 2, wall surface leveling:
A. to step 1 treated metope does corner protector, corner protector 1:2 cement mortar, mortar slightly receive it is dry after smeared with smoothing out with the fingers angle device At fillet;
B. to step 1 treated metope float coat mortar, surface layer mortar is laid using 1:2:4 cement mortar, is then used Gently trowel smears out flat and smooth surface to trowel;
C. inner wall surface is handled, will be filled and led up at gap and uneven with gypsum putty, and tamp floating with putty, It is polished after putty is dry with sand paper or angle grinder, and floating dust is swept only in time, as mended with putty again there are also at uneven It is flat;
Step 3, metope cleans:
A. to one layer of glass grid cloth or silk item is pasted at step 2 treated gap, cloth is sticked to crack with lotion On, cloth should be straightened in when stick, it is flat to paste;
B. to step 2, treated that inner wall surface is further handled, and applies degumming agent thorough at the greasy dirt adhered to Bottom is removed, then clean with scour without sediment motion;
C. the metope in step 2 is checked, it is ensured that metope substantially dry;
Step 4, wall plaster:
A. one of glue or varnish back cover first sprayed to the inner wall surface in step 3, when spray uniformly must not should have omission, glue Mixing ratio by weight is clear water: latex=3:1, then using the gypsum putty in step 3 to step 3 treated inner wall surface into Row painting first pass putty;
B. after step 3, treated after metope is completely dried, and polishes flat to inner wall surface, then carries out painting second All over putty, room short side direction is parallel to big plate and carries out granted full, thickness are as follows: 3~4mm, to the gypsum putty 6~7 in step 3 At it is dry when, press polish is carried out to inner cavity surface with rubber flap and is had a shave, keeps inner wall surface surface layer smooth bright and clean, lines is straight, color is uniform Unanimously, firmly answer it is light and even, and must not worn out paint film, surface is cleaned up after mill;
Step 5, wall surface spraying;
Sprayed coating carried out with spray gun to step 4 treated metope, specking is uniform when spraying, and moving distance is all suitable In, when spraying since inconspicuous one, gradually moved in proper order to other end, until unobtrusively brush is received at place, there is not allowed that Connect raft.
Preferably, it in the step 1, after being scrubbed to substrate surface, and spills clear water and keeps 1 hour or more wet.
Preferably, the ratio of cement mixed mortar is 1:2:3 in the step 1.
Preferably, described, gypsum putty proportion is land plaster: latex solution: cellulose aqueous solution=80:55 in step 2: 70。
Preferably, in the step 3, base's moisture content is not greater than 5%.
Preferably, in the step 4, wall edge direction should be parallel to when painting first pass putty and is successively constructed, thickness Are as follows: 6~7mm, as wall once brush cannot from it is upper on earth when, should at many levels up and down simultaneously operation.
Preferably, the pressure of spray gun are as follows: 0.6~0.7N/mm2, and nozzle and facing are in 90 °, distance are as follows: 850px.
3. beneficial effect
Compared with the prior art, the present invention has the advantages that
In the present invention, by the construction techniques of multi-step, the buildings waterproof effect after making construction is improved, together When so that the flat and smooth degree in inner wall of building face is improved, thus guarantee building normal use.
Specific embodiment
The technical scheme in the embodiments of the invention will be clearly and completely described below, it is clear that described implementation Example is only a part of the embodiment of the present invention, instead of all the embodiments.
Embodiment 1:
Environment protection architecture construction method, includes the following steps:
Step 1, preparation of construction:
A. tool prepare, including degumming agent, scraper plate, sand paper, bandage, guiding ruler, clearance gauge, angle grinder, land plaster, latex solution, Cellulose aqueous solution etc. hang vertical according to the smooth vertical case of substrate surface;
B. substrate surface is thoroughly scrubbed, is washed, after being scrubbed to substrate surface, and spilt clear water and keep wet 1 Hour or more;
C. the base after scrubbing is carried out smearing bedding mortar, bottom is uniformly plated in using cement mixed mortar, with ruler school Rough hair face is scraped in direct join;
Step 2, wall surface leveling:
A. to step 1 treated metope does corner protector, corner protector 1:2 cement mortar, mortar slightly receive it is dry after smeared with smoothing out with the fingers angle device At fillet;
B. to step 1 treated metope float coat mortar, surface layer mortar is laid using 1:2:4 cement mortar, is then used Gently trowel smears out flat and smooth surface to trowel;
C. inner wall surface is handled, will be filled and led up at gap and uneven with gypsum putty, and tamp floating with putty, It is polished after putty is dry with sand paper or angle grinder, and floating dust is swept only in time, as mended with putty again there are also at uneven It is flat;
Step 3, metope cleans:
A. to one layer of glass grid cloth or silk item is pasted at step 2 treated gap, cloth is sticked to crack with lotion On, cloth should be straightened in when stick, it is flat to paste;
B. to step 2, treated that inner wall surface is further handled, and applies degumming agent thorough at the greasy dirt adhered to Bottom is removed, then clean with scour without sediment motion;
C. the metope in step 2 is checked, it is ensured that metope substantially dry;
Step 4, wall plaster:
A. one of glue or varnish back cover first sprayed to the inner wall surface in step 3, when spray uniformly must not should have omission, glue Mixing ratio by weight is clear water: latex=3:1, then using the gypsum putty in step 3 to step 3 treated inner wall surface into Row painting first pass putty;
B. after step 3, treated after metope is completely dried, and polishes flat to inner wall surface, then carries out painting second All over putty, room short side direction is parallel to big plate and carries out granted full, thickness are as follows: 3~4mm, to the gypsum putty 6~7 in step 3 At it is dry when, press polish is carried out to inner cavity surface with rubber flap and is had a shave, keeps inner wall surface surface layer smooth bright and clean, lines is straight, color is uniform Unanimously, firmly answer it is light and even, and must not worn out paint film, surface is cleaned up after mill;
Step 5, wall surface spraying;
Sprayed coating carried out with spray gun to step 4 treated metope, specking is uniform when spraying, and moving distance is all suitable In, when spraying since inconspicuous one, gradually moved in proper order to other end, until unobtrusively brush is received at place, there is not allowed that Connect raft.
Embodiment 2
Environment protection architecture construction method, includes the following steps:
Step 1, preparation of construction:
A. tool prepare, including degumming agent, scraper plate, sand paper, bandage, guiding ruler, clearance gauge, angle grinder, land plaster, latex solution, Cellulose aqueous solution etc. hang vertical according to the smooth vertical case of substrate surface;
B. substrate surface is thoroughly scrubbed, is washed, after being scrubbed to substrate surface, and spilt clear water and keep wet 1 Hour or more;
C. the base after scrubbing is carried out smearing bedding mortar, bottom is uniformly plated in using cement mixed mortar, with ruler school Rough hair face is scraped in direct join, and the ratio of cement mixed mortar is 1:2:3;
Step 2, wall surface leveling:
A. to step 1 treated metope does corner protector, corner protector 1:2 cement mortar, mortar slightly receive it is dry after smeared with smoothing out with the fingers angle device At fillet;
B. to step 1 treated metope float coat mortar, surface layer mortar is laid using 1:2:4 cement mortar, is then used Gently trowel smears out flat and smooth surface to trowel;
C. inner wall surface is handled, will be filled and led up at gap and uneven with gypsum putty, and tamp floating with putty, It is polished after putty is dry with sand paper or angle grinder, and floating dust is swept only in time, as mended with putty again there are also at uneven It is flat;
Step 3, metope cleans:
A. to one layer of glass grid cloth or silk item is pasted at step 2 treated gap, cloth is sticked to crack with lotion On, cloth should be straightened in when stick, it is flat to paste;
B. to step 2, treated that inner wall surface is further handled, and applies degumming agent thorough at the greasy dirt adhered to Bottom is removed, then clean with scour without sediment motion;
C. the metope in step 2 is checked, it is ensured that metope substantially dry;
Step 4, wall plaster:
A. one of glue or varnish back cover first sprayed to the inner wall surface in step 3, when spray uniformly must not should have omission, glue Mixing ratio by weight is clear water: latex=3:1, then using the gypsum putty in step 3 to step 3 treated inner wall surface into Row painting first pass putty;
B. after step 3, treated after metope is completely dried, and polishes flat to inner wall surface, then carries out painting second All over putty, room short side direction is parallel to big plate and carries out granted full, thickness are as follows: 3~4mm, to the gypsum putty 6~7 in step 3 At it is dry when, press polish is carried out to inner cavity surface with rubber flap and is had a shave, keeps inner wall surface surface layer smooth bright and clean, lines is straight, color is uniform Unanimously, firmly answer it is light and even, and must not worn out paint film, surface is cleaned up after mill;
Step 5, wall surface spraying;
Sprayed coating carried out with spray gun to step 4 treated metope, specking is uniform when spraying, and moving distance is all suitable In, when spraying since inconspicuous one, gradually moved in proper order to other end, until unobtrusively brush is received at place, there is not allowed that Connect raft.
Embodiment 3
Environment protection architecture construction method, includes the following steps:
Step 1, preparation of construction:
A. tool prepare, including degumming agent, scraper plate, sand paper, bandage, guiding ruler, clearance gauge, angle grinder, land plaster, latex solution, Cellulose aqueous solution etc. hang vertical according to the smooth vertical case of substrate surface;
B. substrate surface is thoroughly scrubbed, is washed, after being scrubbed to substrate surface, and spilt clear water and keep wet 1 Hour or more;
C. the base after scrubbing is carried out smearing bedding mortar, bottom is uniformly plated in using cement mixed mortar, with ruler school Rough hair face is scraped in direct join, and the ratio of cement mixed mortar is 1:2:3;
Step 2, wall surface leveling:
A. to step 1 treated metope does corner protector, corner protector 1:2 cement mortar, mortar slightly receive it is dry after smeared with smoothing out with the fingers angle device At fillet, the every side width of fillet is not less than 7cm;
B. to step 1 treated metope float coat mortar, surface layer mortar is laid using 1:2:4 cement mortar, is then used Gently trowel smears out flat and smooth surface to trowel;
C. inner wall surface is handled, will be filled and led up at gap and uneven with gypsum putty, gypsum putty proportion is stone Cream powder: latex solution: cellulose aqueous solution=80:55:70, and floating is tamped with putty, sand paper or angle grinder are used after putty is dry It polishes, and floating dust is swept only in time, as used putty filling-in again there are also at uneven;
Step 3, metope cleans:
A. to one layer of glass grid cloth or silk item is pasted at step 2 treated gap, cloth is sticked to crack with lotion On, cloth should be straightened in when stick, it is flat to paste;
B. to step 2, treated that inner wall surface is further handled, and applies degumming agent thorough at the greasy dirt adhered to Bottom is removed, then clean with scour without sediment motion;
C. the metope in step 2 is checked, it is ensured that metope substantially dry;
Step 4, wall plaster:
A. one of glue or varnish back cover first sprayed to the inner wall surface in step 3, when spray uniformly must not should have omission, glue Mixing ratio by weight is clear water: latex=3:1, then using the gypsum putty in step 3 to step 3 treated inner wall surface into Row painting first pass putty;
B. after step 3, treated after metope is completely dried, and polishes flat to inner wall surface, then carries out painting second All over putty, room short side direction is parallel to big plate and carries out granted full, thickness are as follows: 3~4mm, to the gypsum putty 6~7 in step 3 At it is dry when, press polish is carried out to inner cavity surface with rubber flap and is had a shave, keeps inner wall surface surface layer smooth bright and clean, lines is straight, color is uniform Unanimously, firmly answer it is light and even, and must not worn out paint film, surface is cleaned up after mill;
Step 5, wall surface spraying;
Sprayed coating carried out with spray gun to step 4 treated metope, specking is uniform when spraying, and moving distance is all suitable In, when spraying since inconspicuous one, gradually moved in proper order to other end, until unobtrusively brush is received at place, there is not allowed that Connect raft.
Embodiment 4
Environment protection architecture construction method, includes the following steps:
Step 1, preparation of construction:
A. tool prepare, including degumming agent, scraper plate, sand paper, bandage, guiding ruler, clearance gauge, angle grinder, land plaster, latex solution, Cellulose aqueous solution etc. hang vertical according to the smooth vertical case of substrate surface;
B. substrate surface is thoroughly scrubbed, is washed, after being scrubbed to substrate surface, and spilt clear water and keep wet 1 Hour or more;
C. the base after scrubbing is carried out smearing bedding mortar, bottom is uniformly plated in using cement mixed mortar, with ruler school Rough hair face is scraped in direct join, and the ratio of cement mixed mortar is 1:2:3;
Step 2, wall surface leveling:
A. to step 1 treated metope does corner protector, corner protector 1:2 cement mortar, mortar slightly receive it is dry after smeared with smoothing out with the fingers angle device At fillet, the every side width of fillet is not less than 7cm;
B. to step 1 treated metope float coat mortar, surface layer mortar is laid using 1:2:4 cement mortar, is then used Gently trowel smears out flat and smooth surface to trowel;
C. inner wall surface is handled, will be filled and led up at gap and uneven with gypsum putty, gypsum putty proportion is stone Cream powder: latex solution: cellulose aqueous solution=80:55:70, and floating is tamped with putty, sand paper or angle grinder are used after putty is dry It polishes, and floating dust is swept only in time, as used putty filling-in again there are also at uneven;
Step 3, metope cleans:
A. to one layer of glass grid cloth or silk item is pasted at step 2 treated gap, cloth is sticked to crack with lotion On, cloth should be straightened in when stick, it is flat to paste;
B. to step 2, treated that inner wall surface is further handled, and applies degumming agent thorough at the greasy dirt adhered to Bottom is removed, then clean with scour without sediment motion;
C. the metope in step 2 is checked, it is ensured that metope substantially dry, base's moisture content are not greater than 5%;
Step 4, wall plaster:
A. one of glue or varnish back cover first sprayed to the inner wall surface in step 3, when spray uniformly must not should have omission, glue Mixing ratio by weight is clear water: latex=3:1, then using the gypsum putty in step 3 to step 3 treated inner wall surface into Row painting first pass putty, should be parallel to wall edge direction when painting first pass putty and successively construct, thickness are as follows: 6~7mm, As wall once brush cannot from it is upper on earth when, should at many levels up and down simultaneously operation;
B. after step 3, treated after metope is completely dried, and polishes flat to inner wall surface, then carries out painting second All over putty, room short side direction is parallel to big plate and carries out granted full, thickness are as follows: 3~4mm, to the gypsum putty 6~7 in step 3 At it is dry when, press polish is carried out to inner cavity surface with rubber flap and is had a shave, keeps inner wall surface surface layer smooth bright and clean, lines is straight, color is uniform Unanimously, firmly answer it is light and even, and must not worn out paint film, surface is cleaned up after mill;
Step 5, wall surface spraying;
Sprayed coating, the pressure of spray gun are as follows: 0.6~0.7N/mm are carried out with spray gun to step 4 treated metope2, and Nozzle is in 90 ° with facing, distance are as follows: 850px, specking is uniform when spraying, and moving distance is all moderate, from inconspicuous when spraying One beginning, is gradually moved to other end in proper order, until unobtrusively brush is received at place, there is not allowed that connecing raft.
By the construction techniques of multi-step in the embodiment of the present invention, the buildings waterproof effect after making construction is mentioned Height, while the flat and smooth degree in inner wall of building face being made to be improved, to guarantee the normal use of building.
The foregoing is only a preferred embodiment of the present invention, but scope of protection of the present invention is not limited thereto, Anyone skilled in the art in the technical scope disclosed by the present invention, according to the technique and scheme of the present invention and its Inventive concept is subject to equivalent substitution or change, should be covered by the protection scope of the present invention.

Claims (8)

1. environment protection architecture construction method, which comprises the steps of:
Step 1, preparation of construction:
A. tool prepares, including degumming agent, scraper plate, sand paper, bandage, guiding ruler, clearance gauge, angle grinder, land plaster, latex solution, fiber Plain aqueous solution etc. hang vertical according to the smooth vertical case of substrate surface;
B. substrate surface is thoroughly scrubbed, is washed;
C. the base after scrubbing is carried out smearing bedding mortar, bottom is uniformly plated in using cement mixed mortar, simultaneously with ruler alignment Scrape rough hair face;
Step 2, wall surface leveling:
A. to step 1 treated metope does corner protector, corner protector 1:2 cement mortar, mortar slightly receive it is dry after smear into circle with smoothing out with the fingers angle device Angle;
B. to step 1 treated metope float coat mortar, surface layer mortar is laid using 1:2:4 cement mortar, then uses trowel Gently trowel smears out flat and smooth surface;
C. inner wall surface is handled, will be filled and led up at gap and uneven with gypsum putty, and tamp floating with putty, to greasy It is polished after son is dry with sand paper or angle grinder, and floating dust is swept only in time, as used putty filling-in again there are also at uneven;
Step 3, metope cleans:
A. to one layer of glass grid cloth or silk item is pasted at step 2 treated gap, cloth is sticked on crack with lotion, is glued When cloth should be straightened, paste it is flat;
B. to step 2, treated that inner wall surface is further handled, and applies degumming agent thoroughly clear at the greasy dirt adhered to It removes, it is then clean with scour without sediment motion;
C. the metope in step 2 is checked, it is ensured that metope substantially dry;
Step 4, wall plaster:
A. one of glue or varnish back cover first sprayed to the inner wall surface in step 3, when spray uniformly must not should have omission, glue weight Match ratio is clear water: latex=3:1, and then using the gypsum putty in step 3, to step 3, treated that inner wall surface is painted First pass putty;
B. after step 3, treated after metope is completely dried, and polishes flat to inner wall surface, then carry out painting second time it is greasy Son is parallel to room short side direction with big plate and carries out granted full, thickness are as follows: 3~4mm, it is dry to 6~7 one-tenth of gypsum putty in step 3 When, press polish is carried out to inner cavity surface with rubber flap and is had a shave, keeps inner wall surface surface layer smooth bright and clean, lines is straight, color uniformity, Firmly answer it is light and even, and must not worn out paint film, surface is cleaned up after mill;
Step 5, wall surface spraying;
Sprayed coating carried out with spray gun to step 4 treated metope, specking is uniform when spraying, and moving distance is all moderate, spray It when painting since inconspicuous one, is gradually moved in proper order to other end, until unobtrusively brush is received at place, there is not allowed that connecing raft.
2. environment protection architecture construction method according to claim 1, which is characterized in that in the step 1, washed to substrate surface After brush, and spills clear water and keep 1 hour or more wet.
3. environment protection architecture construction method according to claim 1, which is characterized in that cement mixed mortar in the step 1 Ratio be 1:2:3.
4. environment protection architecture construction method according to claim 1, which is characterized in that the every side width of fillet in the step 2 Not less than 7cm.
5. environment protection architecture construction method according to claim 1, which is characterized in that described, gypsum putty matches in step 2 For land plaster: latex solution: cellulose aqueous solution=80:55:70.
6. environment protection architecture construction method according to claim 1, which is characterized in that in the step 3, base's moisture content is not It obtains and is greater than 5%.
7. environment protection architecture construction method according to claim 1, which is characterized in that in the step 4, painting first pass is greasy The period of the day from 11 p.m. to 1 a.m should be parallel to wall edge direction and successively construct, thickness are as follows: 6~7mm, as wall once brush cannot from it is upper on earth when, answer Operation simultaneously up and down at many levels.
8. environment protection architecture construction method according to claim 1, which is characterized in that in the step 5, the pressure of spray gun Are as follows: 0.6~0.7N/mm2, and nozzle and facing are in 90 °, distance are as follows: 850px.
CN201811351202.5A 2018-11-14 2018-11-14 Environment protection architecture construction method Pending CN109555316A (en)