CN109622780A - 一种低成本拉拔扩孔用模具的快速生产方法 - Google Patents
一种低成本拉拔扩孔用模具的快速生产方法 Download PDFInfo
- Publication number
- CN109622780A CN109622780A CN201811539675.8A CN201811539675A CN109622780A CN 109622780 A CN109622780 A CN 109622780A CN 201811539675 A CN201811539675 A CN 201811539675A CN 109622780 A CN109622780 A CN 109622780A
- Authority
- CN
- China
- Prior art keywords
- waste
- old top
- mold
- old
- reaming mold
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了一种低成本拉拔扩孔用模具的快速生产方法,其包括以下步骤:1)收集在穿制管材中因热磨损而变形的废旧顶头;2)按照所需要的拉拔扩孔用模具的规格尺寸,从步骤1)中选取相应规格尺寸的斜轧穿孔用的废旧顶头,确保废旧顶头的规格尺寸满足拉拔扩孔用模具的尺寸加工要求;3)根据拉拔扩孔用模具的长度以及两端的径向尺寸,对步骤2)中所选用的废旧顶头进行切割,利用切割装置锯切掉废旧顶头的头部、尾部,取用废旧顶头的中间部分,取用的废旧顶头中间部分记为内模毛坯件;4)对步骤3)中的内模毛坯件进行机加工。本发明采用废物再利用的方式生产拉拔扩孔用模具,其具有生产成本低,生产效率高等优点。
Description
技术领域
本发明涉及金属无缝管材生产技术领域,特别是涉及一种低成本拉拔扩孔用模具的快速生产方法。
背景技术
金属无缝管材广泛应用于我国工业生产中,且年使用量巨大,金属无缝管材在拉拔扩孔时经常要用到拔扩孔用模具,当金属无缝管材生产加工企业需要加工规格繁多且数量较少的金属无缝管材时,按照常规设计出图、投料制作加工的方法则会存在生产成本高、生产周期长等缺点,很少有厂家愿意生产。
发明内容
本发明的目的是提供一种低成本拉拔扩孔用模具的快速生产方法,其可以有效解决背景技术中所提到的技术问题。
为实现上述目的,本发明提供如下技术方案:
一种低成本拉拔扩孔用模具的快速生产方法,其包括以下步骤:
1)收集在穿制管材中因热磨损而变形的废旧顶头;
2)按照所需要的拉拔扩孔用模具的规格尺寸,从步骤1)中选取相应规格尺寸的斜轧穿孔用的废旧顶头,确保废旧顶头的规格尺寸满足拉拔扩孔用模具的尺寸加工要求;
3)根据拉拔扩孔用模具的长度以及两端的径向尺寸,对步骤2)中所选用的废旧顶头进行切割,利用切割装置锯切掉废旧顶头的头部、尾部,取用废旧顶头的中间部分,取用的废旧顶头中间部分记为内模毛坯件;
4)按照拉拔扩孔用模具的图纸要求,对步骤3)中的内模毛坯件进行机加工,即可获得拉拔扩孔用模具。
优选地,在步骤3)中,先根据拉拔扩孔用模具的长度以及两端的径向尺寸,利用标记笔在废旧顶头的两端划处标记线,再利用切割装置沿着废旧顶头两端的标记线锯切掉废旧顶头的头部、尾部,取用废旧顶头的中间部分。
优选地,在步骤1)中,根据所收集的废旧顶头的大小尺寸将不同尺寸范围的废旧顶头进行分类,再分组存放,并在每组废旧顶头存放处标记出废旧顶头的尺寸范围,保证各组废旧顶头的尺寸范围对应于相应规格尺寸的拉拔扩孔用模具。
与现有技术相比,本发明的有益效果是:
本发明采用废物再利用的方式生产拉拔扩孔用模具,将穿制管材后因热磨损而变形的废旧顶头进行再利用,节省了加工原材料、降低了生产成本,并且具有生产周期短、生产效率高等优点。
附图说明
图1是本发明实施例中废旧顶头的结构示意图;
图2是本发明实施例中拉拔扩孔用模具的结构示意图;
图3是本发明实施例中拉拔扩孔用模具的装配图;
图中,1、废旧顶头,2、拉拔扩孔用模具,3、拉杆。
具体实施方式
下面将对本发明实施例中的技术方案进行清楚、完整地描述,显然,所描述的实施例仅仅是本发明一部分实施例,而不是全部的实施例。基于本发明中的实施例,本领域普通技术人员在没有做出创造性劳动前提下所获得的所有其他实施例,都属于本发明保护的范围。
实施例一:
请参阅图1、图2和图3所示,一种低成本拉拔扩孔用模具的快速生产方法,其包括以下步骤:
1)收集在穿制管材中因热磨损而变形的废旧顶头1;
2)按照所需要的拉拔扩孔用模具的规格尺寸,从步骤1)中选取相应规格尺寸的斜轧穿孔用的废旧顶头,确保废旧顶头的规格尺寸满足拉拔扩孔用模具2的尺寸加工要求;
3)根据拉拔扩孔用模具2的长度以及两端的径向尺寸,对步骤2)中所选用的废旧顶头1进行切割,利用切割装置锯切掉废旧顶头1的头部、尾部,取用废旧顶头1的中间部分,取用的废旧顶头1中间部分记为内模毛坯件;
4)按照拉拔扩孔用模具2的图纸要求,对步骤3)中的内模毛坯件进行机加工,即可获得拉拔扩孔用模具。
实施例二:
请参阅图1、图2和图3所示,一种低成本拉拔扩孔用模具的快速生产方法,其包括以下步骤:
1)收集在穿制管材中因热磨损而变形的废旧顶头1,根据所收集的废旧顶头1的大小尺寸将不同尺寸范围的废旧顶头1进行分类,再分组存放,并在每组废旧顶头1存放处标记出废旧顶头1的尺寸范围,保证各组废旧顶头1的尺寸范围对应于相应规格尺寸的拉拔扩孔用模具2;
2)按照所需要的拔扩孔用模具2的规格尺寸,从步骤1)中选取相应规格尺寸的斜轧穿孔用的废旧顶头1,确保废旧顶头1的规格尺寸满足拉拔扩孔用模具2的尺寸加工要求;
3)先根据拉拔扩孔用模具2的长度以及两端的径向尺寸,利用标记笔在废旧顶头1的两端划处标记线,再利用切割装置沿着废旧顶头1两端的标记线锯切掉废旧顶头1的头部、尾部,取用废旧顶头1的中间部分,取用的废旧顶头1中间部分记为内模毛坯件;
4)按照拉拔扩孔用模具2的图纸要求,对步骤3)中的内模毛坯件进行机加工,即可获得拉拔扩孔用模具2。
以上内容仅仅是对本发明结构所作的举例和说明,所属本技术领域的技术人员对所描述的具体实施例做各种各样的修改或补充或采用类似的方式替代,只要不偏离发明的结构或者超越本权利要求书所定义的范围,均应属于本发明的保护范围。
Claims (3)
1.一种低成本拉拔扩孔用模具的快速生产方法,其特征在于,包括以下步骤:
1)收集在穿制管材中因热磨损而变形的废旧顶头;
2)按照所需要的拉拔扩孔用模具的规格尺寸,从步骤1)中选取相应规格尺寸的斜轧穿孔用的废旧顶头,确保废旧顶头的规格尺寸满足拉拔扩孔用模具的尺寸加工要求;
3)根据拉拔扩孔用模具的长度以及两端的径向尺寸,对步骤2)中所选用的废旧顶头进行切割,利用切割装置锯切掉废旧顶头的头部、尾部,取用废旧顶头的中间部分,取用的废旧顶头中间部分记为内模毛坯件;
4)按照拉拔扩孔用模具的图纸要求,对步骤3)中的内模毛坯件进行机加工,即可获得拉拔扩孔用模具。
2.根据权利要求1所述的一种低成本拉拔扩孔用模具的快速生产方法,其特征在于:在步骤3)中,先根据拉拔扩孔用模具的长度以及两端的径向尺寸,利用标记笔在废旧顶头的两端划处标记线,再利用切割装置沿着废旧顶头两端的标记线锯切掉废旧顶头的头部、尾部,取用废旧顶头的中间部分。
3.根据权利要求1或2所述的一种低成本拉拔扩孔用模具的快速生产方法,其特征在于:在步骤1)中,根据所收集的废旧顶头的大小尺寸将不同尺寸范围的废旧顶头进行分类,再分组存放,并在每组废旧顶头存放处标记出废旧顶头的尺寸范围,保证各组废旧顶头的尺寸范围对应于相应规格尺寸的拉拔扩孔用模具。