Prior art keywords
parts
ludox
resin
titanium dioxide
glycol monoethyl
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Withdrawn
Application number
CN201711006708.8A
Other languages
Chinese (zh)
Inventor
杨雅雯
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Chengdu Newland Jingmao Trading Co Ltd
Original Assignee
Chengdu Newland Jingmao Trading Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Chengdu Newland Jingmao Trading Co Ltd filed Critical Chengdu Newland Jingmao Trading Co Ltd
Priority to CN201711006708.8A priority Critical patent/CN107663420A/en
Publication of CN107663420A publication Critical patent/CN107663420A/en
Withdrawn legal-status Critical Current

Links

Classifications

    • CCHEMISTRY; METALLURGY
    • C09DYES; PAINTS; POLISHES; NATURAL RESINS; ADHESIVES; COMPOSITIONS NOT OTHERWISE PROVIDED FOR; APPLICATIONS OF MATERIALS NOT OTHERWISE PROVIDED FOR
    • C09DCOATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR
    • C09D191/00Coating compositions based on oils, fats or waxes; Coating compositions based on derivatives thereof
    • C09D191/005Drying oils
    • CCHEMISTRY; METALLURGY
    • C08ORGANIC MACROMOLECULAR COMPOUNDS; THEIR PREPARATION OR CHEMICAL WORKING-UP; COMPOSITIONS BASED THEREON
    • C08KUse of inorganic or non-macromolecular organic substances as compounding ingredients
    • C08K3/00Use of inorganic substances as compounding ingredients
    • C08K3/18Oxygen-containing compounds, e.g. metal carbonyls
    • C08K3/20Oxides; Hydroxides
    • C08K3/22Oxides; Hydroxides of metals
    • C08K2003/2237Oxides; Hydroxides of metals of titanium
    • C08K2003/2241Titanium dioxide
    • CCHEMISTRY; METALLURGY
    • C08ORGANIC MACROMOLECULAR COMPOUNDS; THEIR PREPARATION OR CHEMICAL WORKING-UP; COMPOSITIONS BASED THEREON
    • C08KUse of inorganic or non-macromolecular organic substances as compounding ingredients
    • C08K3/00Use of inorganic substances as compounding ingredients
    • C08K3/18Oxygen-containing compounds, e.g. metal carbonyls
    • C08K3/24Acids; Salts thereof
    • C08K3/26Carbonates; Bicarbonates
    • C08K2003/265Calcium, strontium or barium carbonate
    • CCHEMISTRY; METALLURGY
    • C08ORGANIC MACROMOLECULAR COMPOUNDS; THEIR PREPARATION OR CHEMICAL WORKING-UP; COMPOSITIONS BASED THEREON
    • C08LCOMPOSITIONS OF MACROMOLECULAR COMPOUNDS
    • C08L2201/00Properties
    • C08L2201/08Stabilised against heat, light or radiation or oxydation
    • CCHEMISTRY; METALLURGY
    • C08ORGANIC MACROMOLECULAR COMPOUNDS; THEIR PREPARATION OR CHEMICAL WORKING-UP; COMPOSITIONS BASED THEREON
    • C08LCOMPOSITIONS OF MACROMOLECULAR COMPOUNDS
    • C08L2205/00Polymer mixtures characterised by other features
    • C08L2205/03Polymer mixtures characterised by other features containing three or more polymers in a blend
    • C08L2205/035Polymer mixtures characterised by other features containing three or more polymers in a blend containing four or more polymers in a blend

Landscapes

  • Chemical & Material Sciences (AREA)
  • Oil, Petroleum & Natural Gas (AREA)
  • Life Sciences & Earth Sciences (AREA)
  • Engineering & Computer Science (AREA)
  • Materials Engineering (AREA)
  • Wood Science & Technology (AREA)
  • Organic Chemistry (AREA)
  • Compositions Of Macromolecular Compounds (AREA)
  • Paints Or Removers (AREA)

Abstract

The invention discloses a kind of preparation method of anti-aging paint, including titanium dioxide, powdered whiting, polyoxyethylene oleic acid ester, glycol monoethyl ether, styrene-acrylic emulsion, trbasic zinc phosphate, barium chromate, aluminium nitride, rosin resin, anti-yellowing resin, hydroxyethyl cellulose, Ludox, triphenyl phosphite, linseed oil and dimethyl malenate are configured by weight;Stirring is uniformly mixed and heated after solid matter is crushed with liquid.The beneficial effects of the invention are as follows:The present invention has the advantages of oxidation resistance is strong, paint can be avoided because exposure aoxidizes in atmosphere, so as to extend the service life of paint, and suitable for the adverse circumstances such as high temperature, humidity, pH-value be higher, it has formula simple, low manufacture cost, applied widely, the advantages of being readily produced, and is easy to promote the use of.

Description

A kind of preparation method of anti-aging paint
Technical field
It is a kind of preparation method of anti-aging paint specifically the present invention relates to paint field.
Background technology
Paint is that one kind can firmly be covered in body surface, and the chemistry for playing protection, decoration, mark and other specific uses mixes Compound coating.Paint as viscous oily pigment, it is inflammable in the case of not dry, it is not soluble in water, be slightly soluble in fat, dissolve in alcohol, aldehyde, Ether, benzene, alkane, it is soluble in gasoline, kerosene, diesel oil.
All it is by three kinds of film forming matter, subsidiary film forming matter and auxiliary film forming matter no matter painting kind or form Base substance forms:
Film forming matter:Also referred to as binding agent, it is organic high molecular compound such as natural resin that film forming matter is most of(It is rosin, big Paint), coating(Tung oil, linseed oil, soya-bean oil, fish oil etc.), the mix such as synthetic resin, form by pyroreaction, also whether there is The paint of machine thing combination(Such as:Inorganic zinc rich paint).Various film forming matters press the common xxx classes of national standard.It is the master for forming paint Body, decide the performance of paint film.If without film forming matter, simple pigment and auxiliary material can not form paint film.
Subsidiary film forming matter:Including various pigment, extender pigment, rust resisting pigment.Pigment provides color and covering for paint film Power, improves the protective value and decorative effect of paint, and the pigment of good weatherability can improve the service life of paint.Extender pigment can It is folded multiple by the accumulation of pigment using the performance of itself " sheet, needle-like " structure to increase the thickness of paint film, form fish scale The paint film of shape, the service life of paint film is improved, improve water proofing property and rust-proof effect.Rust resisting pigment passes through itself physics and chemistry Anti-rust action, prevent that metal surface is by corrosion by air, chemicals attack for body surface.
Auxiliary film forming matter:Including various auxiliary agents, solvent, various auxiliary agents are in the production process of paint, storage process, use Process and the forming process of paint film play very important effect.Although the amount used is all seldom, to the performance shadow of paint film Ring very big.Even it can not form paint film such as:Do not do, sink to the bottom caking, skinning.
Paint can be reacted and be led with the oxygen in air due to exposure for a long time in atmosphere under the conditions of prior art Cause aging, come off.
The content of the invention
It is an object of the invention to provide a kind of service life it is long, can avoid reacting with oxygen and cause aging The preparation method of anti-aging paint.
The present invention is achieved through the following technical solutions:A kind of preparation method of anti-aging paint, including following steps:
Step S1:By weight configure 20 ~ 26 parts of titanium dioxide, 10 ~ 15 parts of powdered whiting, 3 ~ 6 parts of polyoxyethylene oleic acid ester, 5 ~ 7 parts of glycol monoethyl ether, 2 ~ 4 parts of styrene-acrylic emulsion, 5 ~ 7 parts of trbasic zinc phosphate, 8 ~ 12 parts of barium chromate, 6 ~ 10 parts of aluminium nitride, rosin tree 3 ~ 7 parts of fat, 1 ~ 2 part of anti-yellowing resin, 5 ~ 7 parts of hydroxyethyl cellulose, 10 ~ 12 parts of Ludox, 6 ~ 8 parts of triphenyl phosphite, flax 3 ~ 5 parts of 12 ~ 18 parts of oil and dimethyl malenate;
Step S2:Titanium dioxide, powdered whiting, trbasic zinc phosphate, barium chromate, aluminium nitride, rosin resin, Ludox are well mixed, Uniform mixed mixture is crushed to more than 800 mesh;
Step S3:By mixture and polyoxyethylene oleic acid ester after being crushed in step S2, glycol monoethyl ether, styrene-acrylic emulsion, anti- Muntenite, hydroxy ethyl fiber, triphenyl phosphite, linseed oil and dimethyl malenate are uniformly mixed and heated to 120 DEG C ~ 150 ℃;
Step S4:The mixture in step S3 is set to be incubated 10 ~ 15 minutes in the environment of 120 DEG C ~ 150 DEG C, soaking time terminates Afterwards, stirred 20 minutes ~ 35 minutes in the environment of 120 DEG C ~ 150 DEG C, mixing speed is 800 ~ 1200 revs/min;
Step S5:After stirring, Temperature fall is painted.
Described 20 parts of titanium dioxide, 10 parts of powdered whiting, 3 parts of polyoxyethylene oleic acid ester, 5 parts of glycol monoethyl ether, benzene 2 parts of acrylic emulsion, 5 parts of trbasic zinc phosphate, 8 parts of barium chromate, 6 parts of aluminium nitride, 3 parts of rosin resin, 1 part of anti-yellowing resin, hydroxyethyl cellulose 5 Part, 10 parts of Ludox, 6 parts of triphenyl phosphite, 12 parts of linseed oil and 3 parts of dimethyl malenate.
Described 22 parts of titanium dioxide, 12 parts of powdered whiting, 3 parts of polyoxyethylene oleic acid ester, 6 parts of glycol monoethyl ether, benzene 2 parts of acrylic emulsion, 5 parts of trbasic zinc phosphate, 9 parts of barium chromate, 7 parts of aluminium nitride, 4 parts of rosin resin, 1 part of anti-yellowing resin, hydroxyethyl cellulose 6 Part, 11 parts of Ludox, 6 parts of triphenyl phosphite, 14 parts of linseed oil and 3 parts of dimethyl malenate.
Described 24 parts of titanium dioxide, 14 parts of powdered whiting, 5 parts of polyoxyethylene oleic acid ester, 6 parts of glycol monoethyl ether, benzene 2 parts of acrylic emulsion, 5 parts of trbasic zinc phosphate, 10 parts of barium chromate, 8 parts of aluminium nitride, 4 parts of rosin resin, 1 part of anti-yellowing resin, hydroxyethyl cellulose 3 parts of 6 parts, 10 parts of Ludox, 7 parts of triphenyl phosphite, 16 parts of linseed oil and dimethyl malenate.
Described 26 parts of titanium dioxide, 15 parts of powdered whiting, 6 parts of polyoxyethylene oleic acid ester, 7 parts of glycol monoethyl ether, benzene 4 parts of acrylic emulsion, 7 parts of trbasic zinc phosphate, 12 parts of barium chromate, 10 parts of aluminium nitride, 7 parts of rosin resin, 2 parts of anti-yellowing resin, hydroxy ethyl fiber 5 parts of 7 parts of element, 12 parts of Ludox, 8 parts of triphenyl phosphite, 18 parts of linseed oil and dimethyl malenate.
The present invention compared with prior art, has advantages below and beneficial effect:
The present invention has the advantages of oxidation resistance is strong, can avoid paint because exposure aoxidizes in atmosphere, so as to Extend the service life of paint, and suitable for the adverse circumstances such as high temperature, humidity, pH-value be higher, its have formula it is simple, Low manufacture cost, applied widely, the advantages of being readily produced, it is easy to promote the use of.
Embodiment
The present invention is described in further detail with reference to embodiment, but the implementation of the present invention is not limited to this.
Embodiment 1:
In the present embodiment, a kind of preparation method of anti-aging paint, including following steps:
Step S1:By weight configure 20 ~ 26 parts of titanium dioxide, 10 ~ 15 parts of powdered whiting, 3 ~ 6 parts of polyoxyethylene oleic acid ester, 5 ~ 7 parts of glycol monoethyl ether, 2 ~ 4 parts of styrene-acrylic emulsion, 5 ~ 7 parts of trbasic zinc phosphate, 8 ~ 12 parts of barium chromate, 6 ~ 10 parts of aluminium nitride, rosin tree 3 ~ 7 parts of fat, 1 ~ 2 part of anti-yellowing resin, 5 ~ 7 parts of hydroxyethyl cellulose, 10 ~ 12 parts of Ludox, 6 ~ 8 parts of triphenyl phosphite, flax 3 ~ 5 parts of 12 ~ 18 parts of oil and dimethyl malenate;
Step S2:Titanium dioxide, powdered whiting, trbasic zinc phosphate, barium chromate, aluminium nitride, rosin resin, Ludox are well mixed, Uniform mixed mixture is crushed to more than 800 mesh;
Step S3:By mixture and polyoxyethylene oleic acid ester after being crushed in step S2, glycol monoethyl ether, styrene-acrylic emulsion, anti- Muntenite, hydroxy ethyl fiber, triphenyl phosphite, linseed oil and dimethyl malenate are uniformly mixed and heated to 120 DEG C ~ 150 ℃;
Step S4:The mixture in step S3 is set to be incubated 10 ~ 15 minutes in the environment of 120 DEG C ~ 150 DEG C, soaking time terminates Afterwards, stirred 20 minutes ~ 35 minutes in the environment of 120 DEG C ~ 150 DEG C, mixing speed is 800 ~ 1200 revs/min;
Step S5:After stirring, Temperature fall is painted.
Described 20 parts of titanium dioxide, 10 parts of powdered whiting, 2 parts of polyoxyethylene oleic acid ester, 5 parts of glycol monoethyl ether, benzene 2 parts of acrylic emulsion, 5 parts of trbasic zinc phosphate, 8 parts of barium chromate, 6 parts of aluminium nitride, 3 parts of rosin resin, 1 part of anti-yellowing resin, hydroxyethyl cellulose 5 Part, 10 parts of Ludox, 6 parts of triphenyl phosphite, 12 parts of linseed oil and 3 parts of present invention of dimethyl malenate have high temperature resistant, resisted The advantages of combustion ability is strong, the risk for triggering fire can be reduced, consequently facilitating storage and managenent, and it is painted on furniture, wall coverings, wall After body, can when fire occurs from fire retardation, loss caused by reduce fire, it has, and formula is simple, is fabricated to This is low, applied widely, the advantages of being readily produced, and is easy to promote the use of.
Embodiment 2:
On the basis of above-described embodiment, in the present embodiment, a kind of preparation method of anti-aging paint, including by weight 20 parts of titanium dioxide, 10 parts of powdered whiting, 3 parts of polyoxyethylene oleic acid ester, 5 parts of glycol monoethyl ether, 2 parts of styrene-acrylic emulsion, phosphoric acid 5 parts of zinc, 8 parts of barium chromate, 6 parts of aluminium nitride, 3 parts of rosin resin, 1 part of anti-yellowing resin, 5 parts of hydroxyethyl cellulose, 10 parts of Ludox, 3 parts of 6 parts of triphenyl phosphite, 12 parts of linseed oil and dimethyl malenate.
Embodiment 3:
On the basis of above-described embodiment, in the present embodiment, a kind of preparation method of anti-aging paint, including by weight 22 parts of titanium dioxide, 12 parts of powdered whiting, 3 parts of polyoxyethylene oleic acid ester, 6 parts of glycol monoethyl ether, 2 parts of styrene-acrylic emulsion, phosphoric acid 5 parts of zinc, 9 parts of barium chromate, 7 parts of aluminium nitride, 4 parts of rosin resin, 1 part of anti-yellowing resin, 6 parts of hydroxyethyl cellulose, 11 parts of Ludox, 3 parts of 6 parts of triphenyl phosphite, 14 parts of linseed oil and dimethyl malenate.
Embodiment 4:
On the basis of above-described embodiment, in the present embodiment, a kind of preparation method of anti-aging paint, including by weight 24 parts of titanium dioxide, 14 parts of powdered whiting, 5 parts of polyoxyethylene oleic acid ester, 6 parts of glycol monoethyl ether, 2 parts of styrene-acrylic emulsion, phosphoric acid 5 parts of zinc, 10 parts of barium chromate, 8 parts of aluminium nitride, 4 parts of rosin resin, 1 part of anti-yellowing resin, 6 parts of hydroxyethyl cellulose, Ludox 10 Part, 7 parts of triphenyl phosphite, 16 parts of linseed oil and 3 parts of dimethyl malenate.
Embodiment 5:
On the basis of above-described embodiment, in the present embodiment, a kind of preparation method of anti-aging paint, including by weight 26 parts of titanium dioxide, 15 parts of powdered whiting, 6 parts of polyoxyethylene oleic acid ester, 7 parts of glycol monoethyl ether, 4 parts of styrene-acrylic emulsion, phosphoric acid 7 parts of zinc, 12 parts of barium chromate, 10 parts of aluminium nitride, 7 parts of rosin resin, 2 parts of anti-yellowing resin, 7 parts of hydroxyethyl cellulose, Ludox 12 Part, 8 parts of triphenyl phosphite, 18 parts of linseed oil and 5 parts of dimethyl malenate.
It is described above, be only presently preferred embodiments of the present invention, any formal limitation not done to the present invention, it is every according to Any simply modification, the equivalent variations made according to the technical spirit of the present invention to above example, each fall within the protection of the present invention Within the scope of.

Claims (5)

  1. A kind of 1. preparation method of anti-aging paint, it is characterised in that:Including following steps:
    Step S1:By weight configure 20 ~ 26 parts of titanium dioxide, 10 ~ 15 parts of powdered whiting, 3 ~ 6 parts of polyoxyethylene oleic acid ester, 5 ~ 7 parts of glycol monoethyl ether, 2 ~ 4 parts of styrene-acrylic emulsion, 5 ~ 7 parts of trbasic zinc phosphate, 8 ~ 12 parts of barium chromate, 6 ~ 10 parts of aluminium nitride, rosin tree 3 ~ 7 parts of fat, 1 ~ 2 part of anti-yellowing resin, 5 ~ 7 parts of hydroxyethyl cellulose, 10 ~ 12 parts of Ludox, 6 ~ 8 parts of triphenyl phosphite, flax 3 ~ 5 parts of 12 ~ 18 parts of oil and dimethyl malenate;
    Step S2:Titanium dioxide, powdered whiting, trbasic zinc phosphate, barium chromate, aluminium nitride, rosin resin, Ludox are well mixed, Uniform mixed mixture is crushed to more than 800 mesh;
    Step S3:By mixture and polyoxyethylene oleic acid ester after being crushed in step S2, glycol monoethyl ether, styrene-acrylic emulsion, anti- Muntenite, hydroxy ethyl fiber, triphenyl phosphite, linseed oil and dimethyl malenate are uniformly mixed and heated to 120 DEG C ~ 150 ℃;
    Step S4:The mixture in step S3 is set to be incubated 10 ~ 15 minutes in the environment of 120 DEG C ~ 150 DEG C, soaking time terminates Afterwards, stirred 20 minutes ~ 35 minutes in the environment of 120 DEG C ~ 150 DEG C, mixing speed is 800 ~ 1200 revs/min;
    Step S5:After stirring, Temperature fall is painted.
  2. A kind of 2. preparation method of anti-aging paint according to claim 1, it is characterised in that:Described titanium dioxide 20 Part, 10 parts of powdered whiting, 3 parts of polyoxyethylene oleic acid ester, 5 parts of glycol monoethyl ether, 2 parts of styrene-acrylic emulsion, 5 parts of trbasic zinc phosphate, chromium Sour 8 parts of barium, 6 parts of aluminium nitride, 3 parts of rosin resin, 1 part of anti-yellowing resin, 5 parts of hydroxyethyl cellulose, 10 parts of Ludox, phosphorous acid three 3 parts of 6 parts of phenyl ester, 12 parts of linseed oil and dimethyl malenate.
  3. A kind of 3. preparation method of anti-aging paint according to claim 1, it is characterised in that:Described titanium dioxide 22 Part, 12 parts of powdered whiting, 3 parts of polyoxyethylene oleic acid ester, 6 parts of glycol monoethyl ether, 2 parts of styrene-acrylic emulsion, 5 parts of trbasic zinc phosphate, chromium Sour 9 parts of barium, 7 parts of aluminium nitride, 4 parts of rosin resin, 1 part of anti-yellowing resin, 6 parts of hydroxyethyl cellulose, 11 parts of Ludox, phosphorous acid three 3 parts of 6 parts of phenyl ester, 14 parts of linseed oil and dimethyl malenate.
  4. A kind of 4. preparation method of anti-aging paint according to claim 1, it is characterised in that:Described titanium dioxide 24 Part, 14 parts of powdered whiting, 5 parts of polyoxyethylene oleic acid ester, 6 parts of glycol monoethyl ether, 2 parts of styrene-acrylic emulsion, 5 parts of trbasic zinc phosphate, chromium Sour 10 parts of barium, 8 parts of aluminium nitride, 4 parts of rosin resin, 1 part of anti-yellowing resin, 6 parts of hydroxyethyl cellulose, 10 parts of Ludox, phosphorous acid 3 parts of 7 parts of triphenylmethyl methacrylate, 16 parts of linseed oil and dimethyl malenate.
  5. A kind of 5. preparation method of anti-aging paint according to claim 1, it is characterised in that:Described titanium dioxide 26 Part, 15 parts of powdered whiting, 6 parts of polyoxyethylene oleic acid ester, 7 parts of glycol monoethyl ether, 4 parts of styrene-acrylic emulsion, 7 parts of trbasic zinc phosphate, chromium Sour 12 parts of barium, 10 parts of aluminium nitride, 7 parts of rosin resin, 2 parts of anti-yellowing resin, 7 parts of hydroxyethyl cellulose, 12 parts of Ludox, phosphorous acid 5 parts of 8 parts of triphenylmethyl methacrylate, 18 parts of linseed oil and dimethyl malenate.
CN201711006708.8A 2017-10-25 2017-10-25 A kind of preparation method of anti-aging paint Withdrawn CN107663420A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN201711006708.8A CN107663420A (en) 2017-10-25 2017-10-25 A kind of preparation method of anti-aging paint

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN201711006708.8A CN107663420A (en) 2017-10-25 2017-10-25 A kind of preparation method of anti-aging paint

Publications (1)

Publication Number Publication Date
CN107663420A true CN107663420A (en) 2018-02-06

Family

ID=61097820

Family Applications (1)

Application Number Title Priority Date Filing Date
CN201711006708.8A Withdrawn CN107663420A (en) 2017-10-25 2017-10-25 A kind of preparation method of anti-aging paint

Country Status (1)

Country Link
CN (1) CN107663420A (en)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN108610973A (en) * 2018-05-10 2018-10-02 诸城市福日机械有限公司 A kind of vehicle frame protection paint and preparation method thereof

Citations (9)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN103408971A (en) * 2013-07-03 2013-11-27 青阳县恒源化工原料有限责任公司 Anti-aging modified calcium carbonate for paint-latex paint and preparation method thereof
CN104073041A (en) * 2014-07-24 2014-10-01 周彩球 Steel surface treatment paint
CN104194600A (en) * 2014-08-27 2014-12-10 句容市石狮冲压件厂 Antibacterial fluorescent coating for outdoor deck chair and preparation method of antibacterial fluorescent coating
CN105199580A (en) * 2015-10-23 2015-12-30 王海平 Anticorrosive environment-friendly spray paint formula
CN105670374A (en) * 2016-03-23 2016-06-15 布志刚 Production formula and preparation method of anti-aging paint
CN106810971A (en) * 2015-11-27 2017-06-09 沈阳顺风新城建筑材料有限公司 A kind of general emulsion paint of organic-silicon-modified inner-outer wall and preparation method thereof
CN107033682A (en) * 2016-11-25 2017-08-11 中山摩尔化学工业有限公司 A kind of environment-friendly type styrene-acrylate emulsion coating and preparation method thereof
CN107057565A (en) * 2017-06-26 2017-08-18 郑堂玲 A kind of paint formulation containing Ludox
CN107216785A (en) * 2017-08-08 2017-09-29 合肥安力电力工程有限公司 It is a kind of for fire-resistant anticorrosion paint of power cable and preparation method thereof

Patent Citations (9)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN103408971A (en) * 2013-07-03 2013-11-27 青阳县恒源化工原料有限责任公司 Anti-aging modified calcium carbonate for paint-latex paint and preparation method thereof
CN104073041A (en) * 2014-07-24 2014-10-01 周彩球 Steel surface treatment paint
CN104194600A (en) * 2014-08-27 2014-12-10 句容市石狮冲压件厂 Antibacterial fluorescent coating for outdoor deck chair and preparation method of antibacterial fluorescent coating
CN105199580A (en) * 2015-10-23 2015-12-30 王海平 Anticorrosive environment-friendly spray paint formula
CN106810971A (en) * 2015-11-27 2017-06-09 沈阳顺风新城建筑材料有限公司 A kind of general emulsion paint of organic-silicon-modified inner-outer wall and preparation method thereof
CN105670374A (en) * 2016-03-23 2016-06-15 布志刚 Production formula and preparation method of anti-aging paint
CN107033682A (en) * 2016-11-25 2017-08-11 中山摩尔化学工业有限公司 A kind of environment-friendly type styrene-acrylate emulsion coating and preparation method thereof
CN107057565A (en) * 2017-06-26 2017-08-18 郑堂玲 A kind of paint formulation containing Ludox
CN107216785A (en) * 2017-08-08 2017-09-29 合肥安力电力工程有限公司 It is a kind of for fire-resistant anticorrosion paint of power cable and preparation method thereof

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN108610973A (en) * 2018-05-10 2018-10-02 诸城市福日机械有限公司 A kind of vehicle frame protection paint and preparation method thereof

Similar Documents

Publication Publication Date Title
US2385800A (en) Paint
CN105199580A (en) Anticorrosive environment-friendly spray paint formula
CN104631207A (en) Waterproof coating for water-based paperboards and preparation method thereof
CN101143988A (en) Water-based flame-retardant fireproof wood paint
CN108912928A (en) Fire-retardant, waterproof aqueous core shell acrylic esters resin coating and paint preparation method
CN107880614A (en) A kind of preparation method of moisture-resisting lacquer
CN107868526A (en) A kind of formula of moisture-resisting lacquer
KR20170099205A (en) Anti-corrosion water-soluble paint and varnish composition
CN107663421A (en) A kind of formula of anti-aging paint
CN107663420A (en) A kind of preparation method of anti-aging paint
CN102051105B (en) Solvent-free coumarone modified epoxy heavy-duty anticorrosive coating
CN107793923A (en) A kind of formula of antiultraviolet paint
CN107880619A (en) A kind of preparation method of antiultraviolet paint
CN107805457A (en) A kind of preparation method of anti-aging paint
CN107805456A (en) A kind of formula of anti-aging paint
CN106833214A (en) A kind of environment protection oil paint and preparation method thereof
CN107880703A (en) A kind of preparation method of fire-retardant paint
CN107892830A (en) A kind of environment protection oil paint preparation method for floor
CN107880618A (en) A kind of formula of fire-retardant paint
CN107699019A (en) A kind of preparation method of anti-corrosion fire-retardant paint
CN107858027A (en) A kind of environment protection oil paint formula for floor
CN107573749A (en) A kind of wall decoration composition
DE19530836C1 (en) Corrosion resistant coating for bronze
CN111138949A (en) Multifunctional primer and preparation method thereof
CN107828257A (en) A kind of strong paint formulation of anti-corrosion fire resistance property

Legal Events

Date Code Title Description
PB01 Publication
PB01 Publication
SE01 Entry into force of request for substantive examination
SE01 Entry into force of request for substantive examination
WW01 Invention patent application withdrawn after publication
WW01 Invention patent application withdrawn after publication

Application publication date: 20180206