CN107805456A - A kind of formula of anti-aging paint - Google Patents
A kind of formula of anti-aging paint Download PDFInfo
- Publication number
- CN107805456A CN107805456A CN201711251199.5A CN201711251199A CN107805456A CN 107805456 A CN107805456 A CN 107805456A CN 201711251199 A CN201711251199 A CN 201711251199A CN 107805456 A CN107805456 A CN 107805456A
- Authority
- CN
- China
- Prior art keywords
- parts
- paint
- formula
- ludox
- phenylenediamine
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Withdrawn
Abstract
The invention discloses a kind of formula of anti-aging paint, including titanium dioxide, powdered whiting, alcohol ester 12, polyoxyethylene oleic acid ester, styrene-acrylic emulsion, titanium carbide, nickel phosphate, boron oxide, amino resins, long oil alkyd, hydroxyethyl cellulose, Ludox, triphenyl phosphite, linseed oil and inclined phenylenediamine are configured by weight;Stirring is uniformly mixed and heated after solid matter is crushed with liquid.The beneficial effects of the invention are as follows:The present invention has the advantages of oxidation resistance is strong, paint can be avoided because exposure aoxidizes in atmosphere, so as to extend the service life of paint, and suitable for the adverse circumstances such as high temperature, humidity, pH-value be higher, it has formula simple, low manufacture cost, applied widely, the advantages of being readily produced, and is easy to promote the use of.
Description
Technical field
It is a kind of formula of anti-aging paint specifically the present invention relates to paint field.
Background technology
Paint is that one kind can firmly be covered in body surface, and the chemistry for playing protection, decoration, mark and other specific uses mixes
Compound coating.Paint as viscous oily pigment, it is inflammable in the case of not dry, it is not soluble in water, be slightly soluble in fat, dissolve in alcohol, aldehyde,
Ether, benzene, alkane, it is soluble in gasoline, kerosene, diesel oil.
All it is by three kinds of film forming matter, subsidiary film forming matter and auxiliary film forming matter no matter painting kind or form
Base substance forms:
Film forming matter:Also referred to as binding agent, it is organic high molecular compound such as natural resin that film forming matter is most of(It is rosin, big
Paint), coating(Tung oil, linseed oil, soya-bean oil, fish oil etc.), the mix such as synthetic resin, form by pyroreaction, also whether there is
The paint of machine thing combination(Such as:Inorganic zinc rich paint).It is the main body for forming paint, decides the performance of paint film.If not into
Membrane substance, simple pigment and auxiliary material can not form paint film.
Subsidiary film forming matter:Including various pigment, extender pigment, rust resisting pigment.Pigment provides color and covering for paint film
Power, improves the protective value and decorative effect of paint, and the pigment of good weatherability can improve the service life of paint.Extender pigment can
It is folded multiple by the accumulation of pigment using the performance of itself " sheet, needle-like " structure to increase the thickness of paint film, form fish scale
The paint film of shape, the service life of paint film is improved, improve water proofing property and rust-proof effect.Rust resisting pigment passes through itself physics and chemistry
Anti-rust action, prevent that metal surface is by corrosion by air, chemicals attack for body surface.
Auxiliary film forming matter:Including various auxiliary agents, solvent, various auxiliary agents are in the production process of paint, storage process, use
Process and the forming process of paint film play very important effect.Although the amount used is all seldom, to the performance shadow of paint film
Ring very big.Even it can not form paint film such as:Do not do, sink to the bottom caking, skinning.
Paint can be reacted and be led with the oxygen in air due to exposure for a long time in atmosphere under the conditions of prior art
Cause aging, come off.
The content of the invention
It is an object of the invention to provide a kind of service life it is long, can avoid reacting with oxygen and cause aging
The formula of anti-aging paint.
The present invention is achieved through the following technical solutions:A kind of formula of anti-aging paint, including titanium white by weight
20 ~ 26 parts of powder, 10 ~ 15 parts of powdered whiting, 12 ~ 6 parts of alcohol ester, 4 ~ 9 parts of polyoxyethylene oleic acid ester, 1 ~ 5 part of styrene-acrylic emulsion,
4 ~ 9 parts of titanium carbide, 7 ~ 13 parts of nickel phosphate, 5 ~ 12 parts of boron oxide, 3 ~ 7 parts of amino resins, 1 ~ 4 part of long oil alkyd, hydroxyl second
4 ~ 9 parts of base cellulose, 10 ~ 12 parts of Ludox, 6 ~ 8 parts of triphenyl phosphite, 12 ~ 18 parts of linseed oil and inclined 2 ~ 6 parts of phenylenediamine.
Described 20 parts of titanium dioxide, 10 parts of powdered whiting, 12 parts of alcohol ester, 5 parts of polyoxyethylene oleic acid ester, phenylpropyl alcohol breast
2 parts of liquid, 5 parts of titanium carbide, 8 parts of nickel phosphate, 6 parts of boron oxide, 3 parts of amino resins, 1 part of long oil alkyd, hydroxy ethyl fiber
5 parts of element, 10 parts of Ludox, 6 parts of triphenyl phosphite, 12 parts of linseed oil and inclined 3 parts of phenylenediamine.
Described 22 parts of titanium dioxide, 12 parts of powdered whiting, 12 parts of alcohol ester, 6 parts of polyoxyethylene oleic acid ester, phenylpropyl alcohol breast
2 parts of liquid, 5 parts of titanium carbide, 9 parts of nickel phosphate, 7 parts of boron oxide, 4 parts of amino resins, 1 part of long oil alkyd, hydroxy ethyl fiber
6 parts of element, 11 parts of Ludox, 6 parts of triphenyl phosphite, 14 parts of linseed oil and inclined 3 parts of phenylenediamine.
Described 24 parts of titanium dioxide, 14 parts of powdered whiting, 12 parts of alcohol ester, 6 parts of polyoxyethylene oleic acid ester, phenylpropyl alcohol breast
2 parts of liquid, 5 parts of titanium carbide, 10 parts of nickel phosphate, 8 parts of boron oxide, 4 parts of amino resins, 1 part of long oil alkyd, hydroxy ethyl fiber
6 parts of element, 10 parts of Ludox, 7 parts of triphenyl phosphite, 16 parts of linseed oil and inclined 3 parts of phenylenediamine.
Described 26 parts of titanium dioxide, 15 parts of powdered whiting, 12 parts of alcohol ester, 7 parts of polyoxyethylene oleic acid ester, phenylpropyl alcohol breast
4 parts of liquid, 7 parts of titanium carbide, 12 parts of nickel phosphate, 10 parts of boron oxide, 7 parts of amino resins, 2 parts of long oil alkyd, ethoxy are fine
7 parts of dimension element, 12 parts of Ludox, 8 parts of triphenyl phosphite, 18 parts of linseed oil and inclined 5 parts of phenylenediamine.
The present invention compared with prior art, has advantages below and beneficial effect:
The present invention has the advantages of oxidation resistance is strong, can avoid paint because exposure aoxidizes in atmosphere, so as to
Extend the service life of paint, and suitable for the adverse circumstances such as high temperature, humidity, pH-value be higher, its have formula it is simple,
Low manufacture cost, applied widely, the advantages of being readily produced, it is easy to promote the use of.
Embodiment
The present invention is described in further detail with reference to embodiment, but the implementation of the present invention is not limited to this.
Embodiment 1:
In the present embodiment, a kind of formula of anti-aging paint, including 20 ~ 26 parts of titanium dioxide, powdered whiting by weight
10 ~ 15 parts, 12 ~ 6 parts of alcohol ester, 4 ~ 9 parts of polyoxyethylene oleic acid ester, 1 ~ 5 part of styrene-acrylic emulsion, 4 ~ 9 parts of titanium carbide, nickel phosphate 7 ~
13 parts, 5 ~ 12 parts of boron oxide, 3 ~ 7 parts of amino resins, 1 ~ 4 part of long oil alkyd, 4 ~ 9 parts of hydroxyethyl cellulose, Ludox
10 ~ 12 parts, 6 ~ 8 parts of triphenyl phosphite, 12 ~ 18 parts of linseed oil and inclined 2 ~ 6 parts of phenylenediamine.Its collocation method includes following
Step:
Step S1:20 ~ 26 parts of titanium dioxide, 10 ~ 15 parts of powdered whiting, 12 ~ 6 parts of alcohol ester, oleic acid is configured by weight to gather
4 ~ 9 parts of oxygen vinyl acetate, 1 ~ 5 part of styrene-acrylic emulsion, 4 ~ 9 parts of titanium carbide, 7 ~ 13 parts of nickel phosphate, 5 ~ 12 parts of boron oxide, amino resins 3 ~ 7
Part, 1 ~ 4 part of long oil alkyd, 4 ~ 9 parts of hydroxyethyl cellulose, 10 ~ 12 parts of Ludox, 6 ~ 8 parts of triphenyl phosphite, flax
12 ~ 18 parts of oil and inclined 2 ~ 6 parts of phenylenediamine;
Step S2:Titanium dioxide, powdered whiting, titanium carbide, nickel phosphate, boron oxide, amino resins, Ludox are well mixed,
Uniform mixed mixture is crushed to more than 800 mesh;
Step S3:By the mixture after being crushed in step S2 and alcohol ester 12, polyoxyethylene oleic acid ester, styrene-acrylic emulsion, long oil
Alkyd resin, hydroxy ethyl fiber, triphenyl phosphite, linseed oil and inclined phenylenediamine are uniformly mixed and heated to 120 DEG C ~ 150 DEG C;
Step S4:The mixture in step S3 is set to be incubated 10 ~ 15 minutes in the environment of 120 DEG C ~ 150 DEG C, soaking time terminates
Afterwards, stirred 20 minutes ~ 35 minutes in the environment of 120 DEG C ~ 150 DEG C, mixing speed is 800 ~ 1200 revs/min;
Step S5:After stirring, Temperature fall is painted.The present invention has the advantages of high temperature resistant, fire-resistant ability is strong, can reduce
Trigger the risk of fire, consequently facilitating storage and managenent, and be painted on after furniture, wall coverings, wall, can be when fire occurs
Play fire retardation, loss caused by reduce fire, its have formula simple, low manufacture cost, it is applied widely, be easy to raw
The advantages of production, it is easy to promote the use of
Embodiment 2:
On the basis of above-described embodiment, in the present embodiment, a kind of formula of anti-aging paint, including by weight described in
20 parts of titanium dioxide, 10 parts of powdered whiting, 12 parts of alcohol ester, 5 parts of polyoxyethylene oleic acid ester, 2 parts of styrene-acrylic emulsion, titanium carbide 5
Part, 8 parts of nickel phosphate, 6 parts of boron oxide, 3 parts of amino resins, 1 part of long oil alkyd, 5 parts of hydroxyethyl cellulose, Ludox 10
Part, 6 parts of triphenyl phosphite, 12 parts of linseed oil and inclined 3 parts of phenylenediamine.In the present embodiment, other parts not described with it is above-mentioned
The content of embodiment is identical, therefore does not repeat.
Embodiment 3:
On the basis of above-described embodiment, in the present embodiment, a kind of formula of anti-aging paint, including titanium white by weight
20 parts of powder, 10 parts of powdered whiting, 12 parts of alcohol ester, 5 parts of polyoxyethylene oleic acid ester, 2 parts of styrene-acrylic emulsion, 5 parts of titanium carbide, phosphorus
Sour 8 parts of nickel, 6 parts of boron oxide, 3 parts of amino resins, 1 part of long oil alkyd, 5 parts of hydroxyethyl cellulose, 10 parts of Ludox, Asia
6 parts of triphenyl phosphate, 12 parts of linseed oil and inclined 3 parts of phenylenediamine.In the present embodiment, other parts not described and above-described embodiment
Content it is identical, therefore do not repeat.
Embodiment 4:
On the basis of above-described embodiment, in the present embodiment, a kind of formula of anti-aging paint, including titanium white by weight
22 parts of powder, 12 parts of powdered whiting, 12 parts of alcohol ester, 6 parts of polyoxyethylene oleic acid ester, 2 parts of styrene-acrylic emulsion, 5 parts of titanium carbide, phosphorus
Sour 9 parts of nickel, 7 parts of boron oxide, 4 parts of amino resins, 1 part of long oil alkyd, 6 parts of hydroxyethyl cellulose, 11 parts of Ludox, Asia
6 parts of triphenyl phosphate, 14 parts of linseed oil and inclined 3 parts of phenylenediamine.In the present embodiment, other parts not described and above-described embodiment
Content it is identical, therefore do not repeat.
Embodiment 5:
On the basis of above-described embodiment, in the present embodiment, a kind of formula of anti-aging paint, including titanium white by weight
24 parts of powder, 14 parts of powdered whiting, 12 parts of alcohol ester, 6 parts of polyoxyethylene oleic acid ester, 2 parts of styrene-acrylic emulsion, 5 parts of titanium carbide, phosphorus
Sour 10 parts of nickel, 8 parts of boron oxide, 4 parts of amino resins, 1 part of long oil alkyd, 6 parts of hydroxyethyl cellulose, 10 parts of Ludox,
7 parts of triphenyl phosphite, 16 parts of linseed oil and inclined 3 parts of phenylenediamine.In the present embodiment, other parts not described and above-mentioned implementation
The content of example is identical, therefore does not repeat.
Embodiment 6:
On the basis of above-described embodiment, in the present embodiment, a kind of formula of anti-aging paint, including titanium white by weight
26 parts of powder, 15 parts of powdered whiting, 12 parts of alcohol ester, 7 parts of polyoxyethylene oleic acid ester, 4 parts of styrene-acrylic emulsion, 7 parts of titanium carbide, phosphorus
Sour 12 parts of nickel, 10 parts of boron oxide, 7 parts of amino resins, 2 parts of long oil alkyd, 7 parts of hydroxyethyl cellulose, 12 parts of Ludox,
8 parts of triphenyl phosphite, 18 parts of linseed oil and inclined 5 parts of phenylenediamine.In the present embodiment, other parts not described and above-mentioned implementation
The content of example is identical, therefore does not repeat.
It is described above, be only presently preferred embodiments of the present invention, any formal limitation not done to the present invention, it is every according to
Any simply modification, the equivalent variations made according to the technical spirit of the present invention to above example, each fall within the protection of the present invention
Within the scope of.
Claims (5)
- A kind of 1. formula of anti-aging paint, it is characterised in that:Including 20 ~ 26 parts of titanium dioxide, heavy carbonic acid by weight 10 ~ 15 parts of calcium, 4 ~ 9 parts of titanium carbide, 7 ~ 13 parts of nickel phosphate, 5 ~ 12 parts of boron oxide, 12 ~ 6 parts of alcohol ester, polyoxyethylene oleic acid ester 4 ~ 9 parts, 1 ~ 5 part of styrene-acrylic emulsion, 3 ~ 7 parts of amino resins, 1 ~ 4 part of long oil alkyd, 4 ~ 9 parts of hydroxyethyl cellulose, Ludox 10 ~ 12 parts, 6 ~ 8 parts of triphenyl phosphite, 12 ~ 18 parts of linseed oil and inclined 2 ~ 6 parts of phenylenediamine.
- A kind of 2. formula of anti-aging paint according to claim 1, it is characterised in that:Described 20 parts of titanium dioxide, again 10 parts of matter calcium carbonate, 12 parts of alcohol ester, 5 parts of polyoxyethylene oleic acid ester, 2 parts of styrene-acrylic emulsion, 5 parts of titanium carbide, 8 parts of nickel phosphate, oxygen Change 6 parts of boron, 3 parts of amino resins, 1 part of long oil alkyd, 5 parts of hydroxyethyl cellulose, 10 parts of Ludox, triphenyl phosphite 6 parts, 12 parts of linseed oil and inclined 3 parts of phenylenediamine.
- A kind of 3. formula of anti-aging paint according to claim 1, it is characterised in that:Described 22 parts of titanium dioxide, again 12 parts of matter calcium carbonate, 12 parts of alcohol ester, 6 parts of polyoxyethylene oleic acid ester, 2 parts of styrene-acrylic emulsion, 5 parts of titanium carbide, 9 parts of nickel phosphate, oxygen Change 7 parts of boron, 4 parts of amino resins, 1 part of long oil alkyd, 6 parts of hydroxyethyl cellulose, 11 parts of Ludox, triphenyl phosphite 6 parts, 14 parts of linseed oil and inclined 3 parts of phenylenediamine.
- A kind of 4. formula of anti-aging paint according to claim 1, it is characterised in that:Described 24 parts of titanium dioxide, again 14 parts of matter calcium carbonate, 12 parts of alcohol ester, 6 parts of polyoxyethylene oleic acid ester, 2 parts of styrene-acrylic emulsion, 5 parts of titanium carbide, 10 parts of nickel phosphate, 8 parts of boron oxide, 4 parts of amino resins, 1 part of long oil alkyd, 6 parts of hydroxyethyl cellulose, 10 parts of Ludox, phosphorous triphenyl phosphate 7 parts of ester, 16 parts of linseed oil and inclined 3 parts of phenylenediamine.
- A kind of 5. formula of anti-aging paint according to claim 1, it is characterised in that:Described 26 parts of titanium dioxide, again 15 parts of matter calcium carbonate, 12 parts of alcohol ester, 7 parts of polyoxyethylene oleic acid ester, 4 parts of styrene-acrylic emulsion, 7 parts of titanium carbide, 12 parts of nickel phosphate, 10 parts of boron oxide, 7 parts of amino resins, 2 parts of long oil alkyd, 7 parts of hydroxyethyl cellulose, 12 parts of Ludox, phosphorous acid three 8 parts of phenyl ester, 18 parts of linseed oil and inclined 5 parts of phenylenediamine.