CN107558229A - 一种挺括型夹克面料的加工工艺 - Google Patents

一种挺括型夹克面料的加工工艺 Download PDF

Info

Publication number
CN107558229A
CN107558229A CN201710737063.9A CN201710737063A CN107558229A CN 107558229 A CN107558229 A CN 107558229A CN 201710737063 A CN201710737063 A CN 201710737063A CN 107558229 A CN107558229 A CN 107558229A
Authority
CN
China
Prior art keywords
fabric
yarn
dyeing
well
processing
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201710737063.9A
Other languages
English (en)
Inventor
沈学如
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Jiangsu Aoyang Family Garment Co Ltd
Original Assignee
Jiangsu Aoyang Family Garment Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Jiangsu Aoyang Family Garment Co Ltd filed Critical Jiangsu Aoyang Family Garment Co Ltd
Priority to CN201710737063.9A priority Critical patent/CN107558229A/zh
Publication of CN107558229A publication Critical patent/CN107558229A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种挺括型夹克面料的加工工艺。这种挺括型夹克面料的加工工艺,包括纱线的制备、纱线的染色、织造布匹生坯、成品面料在含有防皱定型剂的浸渍液中浸轧处理、布匹烘干以及面料定型。本发明设计合理,面料由有机棉纤维、天丝纤维和聚酯纤维按质量比配比制成,聚酯纤维增加面料挺括和耐磨程度,天丝纤维使得面料不易起球;半成品面料在含有防皱定型剂的浸渍液中浸轧处理,提高面料的防皱性能。

Description

一种挺括型夹克面料的加工工艺
技术领域
本发明涉及一种挺括型夹克面料的加工工艺。
背景技术
夹克是英文jacket的译音,指衣长较短、胸围宽松、紧袖口克夫、紧下摆克夫式样的上衣。它是男女都能穿的短上衣的总称。夹克衫是人们现代生活中最常见的一种服装,由于它造型轻便、活泼、富有朝气,所以为广大男女青少年所喜爱,风行开始于上世纪80年代。现有的夹克面料五花八,夹克面料容易皱,影响穿着,同时制作工艺都比较复杂,对生产工艺要求较为严格,相应的制作出来的产品成本也比较高,影响了面料在普通人群中的应用普及。
发明内容
本发明要解决的技术问题是:克服现有技术的不足,提供一种结构简单,防皱性能好的挺括型夹克面料的加工工艺。
本发明解决其技术问题所采用的技术方案是:一种挺括型夹克面料的加工工艺,具有以下步骤:
(1)、纱线的制备,将有机棉纤维、天丝纤维和聚酯纤维按质量比1:1~1.5:2~4进行配比,通过并条、粗纱、细纱络筒制得坯纱;
(2)、纱线的染色,采用染色机对坯纱进行染色处理;
(3)、步骤(2)中的纱线喂入自动喷气织机,织造布匹生坯,上机幅宽为168cm,上机经密为230根/10cm,纬密为220根/10cm;
(4)、将步骤(3)制成的半成品面料在含有防皱定型剂的浸渍液中浸轧处理,压力3~3.5kg/cm2,带液率75~80%;
(5)、布匹烘干,将布匹在120~140℃焙烘3~5min;
(6)、采用烘培定型机将烘干后的夹克面料在140~150℃之间恒温0.5~2h。
进一步地,所述步骤(2)中对纱线进行染色处理,染色温度为50℃~70℃,工艺为先酸性染色后碱性固色;在染色过程中,选择性地加入螯合分散剂、无水硫酸钠、醋酸或纯碱。
进一步地,所述的步骤(4)中防皱定型剂由如下重量份的组分组成:
并加水配成质量含量30~50%的浸渍液。
本发明的有益效果是:本发明设计合理,具有以下优点:
(1)、面料由有机棉纤维、天丝纤维和聚酯纤维按质量比配比制成,聚酯纤维增加面料挺括和耐磨程度,天丝纤维使得面料不易起球;
(2)、采用先酸性染色后碱性固色的染色工艺,纱线着色牢固,不易褪色;
(3)、纱线喂入自动喷气织机,织造布匹生坯,大大提高了生产效率;
(4)、半成品面料在含有防皱定型剂的浸渍液中浸轧处理,提高面料的防皱性能;
(5)、设有烘干布匹工序,便于去除布匹中的水分,提高下一道热定型工序的生产效率。
具体实施方式
现在对本发明作进一步的说明。
一种挺括型夹克面料的加工工艺,具有以下步骤:
(1)、纱线的制备,将有机棉纤维、天丝纤维和聚酯纤维按质量比1:1.5:4进行配比,通过并条、粗纱、细纱络筒制得坯纱;
(2)、纱线的染色,采用染色机对坯纱进行染色处理,染色温度为65℃,工艺为先酸性染色后碱性固色;在染色过程中,选择性地加入螯合分散剂、无水硫酸钠、醋酸或纯碱;
(3)、步骤(2)中的纱线喂入自动喷气织机,织造布匹生坯,上机幅宽为168cm,上机经密为230根/10cm,纬密为220根/10cm;
(4)、将步骤(3)制成的半成品面料在含有防皱定型剂的浸渍液中浸轧处理,压力3.5kg/cm2,带液率80%;
(5)、布匹烘干,将布匹在140℃焙烘5min;
(6)、采用烘培定型机将烘干后的夹克面料在150℃之间恒温1.5h。
其中,步骤(4)中防皱定型剂由如下重量份的组分组成:
并加水配成质量含量45%的浸渍液。
以上述依据本发明的理想实施例为启示,通过上述的说明内容,相关工作人员完全可以在不偏离本项发明技术思想的范围内,进行多样的变更以及修改。本项发明的技术性范围并不局限于说明书上的内容,必须要根据权利要求范围来确定其技术性范围。

Claims (3)

1.一种挺括型夹克面料的加工工艺,其特征在于:具有以下步骤:
(1)、纱线的制备,将有机棉纤维、天丝纤维和聚酯纤维按质量比1:1~1.5:2~4进行配比,通过并条、粗纱、细纱络筒制得坯纱;
(2)、纱线的染色,采用染色机对坯纱进行染色处理;
(3)、步骤(2)中的纱线喂入自动喷气织机,织造布匹生坯,上机幅宽为168cm,上机经密为230根/10cm,纬密为220根/10cm;
(4)、将步骤(3)制成的半成品面料在含有防皱定型剂的浸渍液中浸轧处理,压力3~3.5kg/cm2,带液率75~80%;
(5)、布匹烘干,将布匹在120~140℃焙烘3~5min;
(6)、采用烘培定型机将烘干后的夹克面料在140~150℃之间恒温0.5~2h。
2.根据权利要求1所述的挺括型夹克面料的加工工艺,其特征在于:所述步骤(2)中对纱线进行染色处理,染色温度为50℃~70℃,工艺为先酸性染色后碱性固色;在染色过程中,选择性地加入螯合分散剂、无水硫酸钠、醋酸或纯碱。
3.根据权利要求1所述的挺括型夹克面料的加工工艺,其特征在于:所述的步骤(4)中防皱定型剂由如下重量份的组分组成:
并加水配成质量含量30~50%的浸渍液。
CN201710737063.9A 2017-08-24 2017-08-24 一种挺括型夹克面料的加工工艺 Pending CN107558229A (zh)