CN105729260A - 一种轧辊磨削工艺 - Google Patents

一种轧辊磨削工艺 Download PDF

Info

Publication number
CN105729260A
CN105729260A CN201410744805.7A CN201410744805A CN105729260A CN 105729260 A CN105729260 A CN 105729260A CN 201410744805 A CN201410744805 A CN 201410744805A CN 105729260 A CN105729260 A CN 105729260A
Authority
CN
China
Prior art keywords
grinding
speed
roll
roller
during
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201410744805.7A
Other languages
English (en)
Inventor
杨斌
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Chongqing Jinsheng Machinery Parts Manufacturing Co Ltd
Original Assignee
Chongqing Jinsheng Machinery Parts Manufacturing Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Chongqing Jinsheng Machinery Parts Manufacturing Co Ltd filed Critical Chongqing Jinsheng Machinery Parts Manufacturing Co Ltd
Priority to CN201410744805.7A priority Critical patent/CN105729260A/zh
Publication of CN105729260A publication Critical patent/CN105729260A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种轧辊磨削工艺,包括如下步骤:(1)砂轮速度;粗、精磨钢质轧辊25~35m/s,粗、精磨冷硬铸铁轧辊20~25m/s,超精磨削、镜面磨削时15~20m/s;(2)工件速度;粗磨时30~50m/min精磨时15~30m/min,精密抛光磨削时10~15m/min当磨削细长辊子时应采用低速,尤其是磨削辊身尺寸小的光压延辊时,工件轧辊的速度小于10m/min;(3)拖板纵向进给速度;粗磨时240~600m/min;或取工件每转拖板纵向进给量约为砂轮宽度的2/3~3/4;精磨时80~200m/min;或取工件每转拖板纵向进给量约为砂轮宽度的1/4~1/2;(4)拖板每往复行程横进给量;粗磨时横进给量应根据轧辊的硬度和磨削辊面的直径而定,一般取0.03~0.05mm/往复行程;对于材料硬、辊颈大的轧辊,应减小横进给量。

Description

一种轧辊磨削工艺
技术领域
本发明涉及一种轧辊磨削工艺。
背景技术
现有的轧辊磨削工艺存在工序安排不合理、工序繁多,工艺参数选择不合理,各工艺参数搭配不合理,且对操作者经验要求较高,使得生产成本偏高、产品质量偏低、成品率不高。
发明内容
有鉴于现有技术的上述缺陷,本发明所要解决的技术问题是提供一种工序合理、制造成本低的轧辊磨削工艺。
为实现上述目的,本发明提供了
一种轧辊磨削工艺,包括如下步骤:
(1)砂轮速度
粗、精磨钢质轧辊25~35m/s粗、精磨冷硬铸铁轧辊20~25m/s超精磨削、镜面磨削时15~20m/s
(2)工件(轧辊)速度粗磨时30~50m/min精磨时15~30m/min,精密抛光磨削时10~15m/min当磨削细长辊子时应采用低速,尤其是磨削辊身尺寸小的光压延辊时,工件轧辊的速度小于10m/min;
(3)拖板纵向进给速度;粗磨时240~600m/min;或取工件每转拖板纵向进给量约为砂轮宽度的2/3~3/4;精磨时80~200m/min;或取工件每转拖板纵向进给量约为砂轮宽度的1/4~1/2;
(4)拖板每往复行程横进给量;粗磨时横进给量应根据轧辊的硬度和磨削辊面的直径而定,一般取0.03~0.05mm/往复行程;对于材料硬、辊颈大的轧辊,应减小横进给量;精磨时0.005~0.01mm/往复行程;精密抛光磨削时0.002~0.005mm/往复行程;
(5)操作工艺注意事项;
A.按特定的工件选择砂轮,并作砂轮平衡和修整;
B.精磨轧辊时,上班后机床应开车空运转30分钟,待机床热平衡稳定和液压油排净空气后,再时行磨削加工,便于稳定磨削精度;
C.在整个磨削过程中,特别是超精磨削和抛光镜面磨削时,保证供给充分的、清洁的冷却液,避免磨削烧伤、表面划痕等磨削缺陷的产生;
D.对于精度要求高的辊子,在无进给光磨时,可以采取一边磨削,一边使辊子慢速范围内不断变换转速,以减少或打乱机床各种频率的振动对磨削圆度和磨削波纹的影响,提高轧辊磨削质量。
本发明的有益效果是:本发明工序合理,制造成本低,各参数搭配合理协调,能够有效地提高产品质量和生产效率。
具体实施方式
下面结合实施例对本发明作进一步说明:
一种轧辊磨削工艺,包括如下步骤:
(1)砂轮速度
粗、精磨钢质轧辊25~35m/s粗、精磨冷硬铸铁轧辊20~25m/s超精磨削、镜面磨削时15~20m/s
(2)工件(轧辊)速度粗磨时30~50m/min精磨时15~30m/min,精密抛光磨削时10~15m/min当磨削细长辊子时应采用低速,尤其是磨削辊身尺寸小的光压延辊时,工件轧辊的速度小于10m/min;
(3)拖板纵向进给速度;粗磨时240~600m/min;或取工件每转拖板纵向进给量约为砂轮宽度的2/3~3/4;精磨时80~200m/min;或取工件每转拖板纵向进给量约为砂轮宽度的1/4~1/2;
(4)拖板每往复行程横进给量;粗磨时横进给量应根据轧辊的硬度和磨削辊面的直径而定,一般取0.03~0.05mm/往复行程;对于材料硬、辊颈大的轧辊,应减小横进给量;精磨时0.005~0.01mm/往复行程;精密抛光磨削时0.002~0.005mm/往复行程;
(5)操作工艺注意事项;
A.按特定的工件选择砂轮,并作砂轮平衡和修整;
B.精磨轧辊时,上班后机床应开车空运转30分钟,待机床热平衡稳定和液压油排净空气后,再时行磨削加工,便于稳定磨削精度;
C.在整个磨削过程中,特别是超精磨削和抛光镜面磨削时,保证供给充分的、清洁的冷却液,避免磨削烧伤、表面划痕等磨削缺陷的产生;
D.对于精度要求高的辊子,在无进给光磨时,可以采取一边磨削,一边使辊子慢速范围内不断变换转速,以减少或打乱机床各种频率的振动对磨削圆度和磨削波纹的影响,提高轧辊磨削质量。

Claims (1)

1.一种轧辊磨削工艺,其特征是;包括如下步骤:
(1)砂轮速度,粗、精磨钢质轧辊25~35m/s粗、精磨冷硬铸铁轧辊20~25m/s超精磨削、镜面磨削时15~20m/s;
(2)工件(轧辊)速度,粗磨时30~50m/min精磨时15~30m/min,精密抛光磨削时10~15m/min当磨削细长辊子时应采用低速,尤其是磨削辊身尺寸小的光压延辊时,工件轧辊的速度小于10m/min;
(3)拖板纵向进给速度,粗磨时240~600m/min;或取工件每转拖板纵向进给量约为砂轮宽度的2/3~3/4;精磨时80~200m/min;或取工件每转拖板纵向进给量约为砂轮宽度的1/4~1/2;
(4)拖板每往复行程横进给量;粗磨时横进给量应根据轧辊的硬度和磨削辊面的直径而定,一般取0.03~0.05mm/往复行程;对于材料硬、辊颈大的轧辊,应减小横进给量;精磨时0.005~0.01mm/往复行程;精密抛光磨削时0.002~0.005mm/往复行程;
(5)操作工艺注意事项;
A.按特定的工件选择砂轮,并作砂轮平衡和修整;
B.精磨轧辊时,上班后机床应开车空运转30分钟,待机床热平衡稳定和液压油排净空气后,再时行磨削加工,便于稳定磨削精度;
C.在整个磨削过程中,特别是超精磨削和抛光镜面磨削时,保证供给充分的、清洁的冷却液,避免磨削烧伤、表面划痕等磨削缺陷的产生;
D.对于精度要求高的辊子,在无进给光磨时,可以采取一边磨削,一边使辊子慢速范围内不断变换转速,以减少或打乱机床各种频率的振动对磨削圆度和磨削波纹的影响,提高轧辊磨削质量。
CN201410744805.7A 2014-12-09 2014-12-09 一种轧辊磨削工艺 Pending CN105729260A (zh)