CN105419682A - 一种用于粘贴标签用胶黏剂 - Google Patents
一种用于粘贴标签用胶黏剂 Download PDFInfo
- Publication number
- CN105419682A CN105419682A CN201510864851.5A CN201510864851A CN105419682A CN 105419682 A CN105419682 A CN 105419682A CN 201510864851 A CN201510864851 A CN 201510864851A CN 105419682 A CN105419682 A CN 105419682A
- Authority
- CN
- China
- Prior art keywords
- solution
- deionized water
- sticking
- add
- stir
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了一种用于粘贴标签用胶黏剂,包括组份:乙烯-乙酸乙烯酯共聚物乳液、乙酸乙烯酯、丙烯酸、聚乙烯醇、烷基酚聚氧乙烯醚、邻苯二甲酸二辛酯、邻苯二甲酸二丁酯、过硫酸铵、硫酸铝、氯化铝、氧化锌、氯丁胶、正丁醇和去离子水,各组份按质量比是:100:35:23:8::7:7:6:1.5:0.09:0.03:0.01:11.5:0.02:65.6;本产品具有粘接强度大、无毒、快干、价格较低等优点。除用于粘接聚乙烯、聚丙烯塑料包装瓶外,也可用于其他塑料包装瓶与纸质标签的粘贴。
Description
技术领域
本发明涉及一种用于粘贴标签用胶黏剂。
背景技术
日常生活中,一些日用化工产品、食品、医药及其他很多产品,其包装容器大多数是由聚乙烯或聚丙烯塑料制成。由于聚乙烯、聚丙烯的分子结构中存在无极性基团,加之具有高结晶性,表面自由能较低,一般胶黏剂很难湿润这些材料的表面,制作的标签容易从包装盒表面脱离。用表面处理法,水客改变聚乙烯及聚丙烯的表面极性,但处理方法比较复杂,在实际应用中受到限制。
目前常用的胶黏剂与由聚乙烯或聚丙烯塑料制品表面很难粘合,容易从包装盒表面脱离。
发明内容
本发明的目的是解决的胶黏剂与由聚乙烯或聚丙烯塑料制品表面很难粘合,容易从包装盒表面脱离的问题。
本发明采用的技术方案是:一种用于粘贴标签用胶黏剂,包括组份:乙烯-乙酸乙烯酯共聚物乳液、乙酸乙烯酯、丙烯酸、聚乙烯醇、烷基酚聚氧乙烯醚、邻苯二甲酸二辛酯、邻苯二甲酸二丁酯、过硫酸铵、硫酸铝、氯化铝、氧化锌、氯丁胶、正丁醇和去离子水,各组份按质量比是:100:35:23:8::7:7:6:1.5:0.09:0.03:0.01:11.5:0.02:65.6;
制作步骤是:
(1)在带搅拌器的容器中将硫酸铝、氯化铝、氧化锌用10倍量的去离子水溶解,制得溶液A;
(2)在装有搅拌器、回流冷凝器的高剪釜中,加入总量1/3的去离子水、聚乙烯醇,搅拌1h,使聚乙烯醇完全溶解,加入1/3的烷基酚聚氧乙烯醚、15%的乙酸乙烯酯,开启分散电机(35HZ)、乳化电机(45HZ)搅拌30-40min;
(3)升温至60~65℃,滴加2/5的过硫酸铵溶液(质量分数为0.2%),搅拌反应2.5h;
(4)向步骤2中混合液加入剩余的去离子水、丙烯酸、剩余的烷基酚聚氧乙烯醚和剩余的乙酸乙烯酯,搅拌升温至72~75℃,反应0.5h;
(5)向步骤3中混合液中均匀滴加剩余的过硫酸铵溶液,加毕后保持搅拌20min,然后升温至90~95℃,保温反应0.5h;
(6)降温至50℃,加入碳酸氢钠溶液(30%),调pH值为6~7,加入邻苯二甲酸二丁酯,搅拌0.5h使其混合均匀后得到半成品B;
(7)向半成品B中加入乙烯-乙酸乙烯酯共聚物乳液,搅拌30-40min后,加入邻苯二甲酸二辛酯和由步骤1制得的溶液A,开始搅拌时加入正丁醇,搅拌60-70min后,加入碳酸氢钠溶液(30%)调节PH值6.5-7.5,加入氯丁胶,搅拌30min即制得产品。
本发明的有益效果是:本产品具有粘接强度大、无毒、快干、价格较低等优点。除用于粘接聚乙烯、聚丙烯塑料包装瓶外,也可用于其他塑料包装瓶与纸质标签的粘贴。
具体实施方式
实施例1:
(1)在带搅拌器的容器中将0.09kg硫酸铝、0.03kg氯化铝、0.01kg氧化锌用40kg的去离子水溶解,制得溶液A;
(2)在装有搅拌器、回流冷凝器的高剪釜中,加入20kg的去离子水、8kg聚乙烯醇,搅拌1h,使聚乙烯醇完全溶解,加入2kg的烷基酚聚氧乙烯醚、5.25kg的乙酸乙烯酯,开启分散电机(35HZ)、乳化电机(45HZ)搅拌30-40min;
(3)升温至60~65℃,滴加0.6kg过硫酸铵溶液(质量分数为0.2%),搅拌反应2.5h;
(4)向步骤2中混合液加入5.6kg去离子水、丙烯酸、剩余的烷基酚聚氧乙烯醚和剩余的乙酸乙烯酯,搅拌升温至72~75℃,反应0.5h;
(5)向步骤3中混合液中均匀滴加剩余的过硫酸铵溶液,加毕后保持搅拌20min,然后升温至90~95℃,保温反应0.5h;
(6)降温至50℃,加入碳酸氢钠溶液(30%),调pH值为6~7,加入邻苯二甲酸二丁酯,搅拌0.5h使其混合均匀后得到半成品B;
(7)向半成品B中加入乙烯-乙酸乙烯酯共聚物乳液,搅拌30-40min后,加入邻苯二甲酸二辛酯和由步骤1制得的溶液A,开始搅拌时加入正丁醇,搅拌60-70min后,加入碳酸氢钠溶液(30%)调节PH值6.5-7.5,加入氯丁胶,搅拌30min即制得产品。
实施例2
(1)在带搅拌器的容器中将0.09kg硫酸铝、0.03kg氯化铝、0.01kg氧化锌用40kg的去离子水溶解,制得溶液A;
(2)在装有搅拌器、回流冷凝器的高剪釜中,加入20kg的去离子水、8kg聚乙烯醇,搅拌1h,使聚乙烯醇完全溶解,加入2kg的烷基酚聚氧乙烯醚、5.25kg的乙酸乙烯酯,开启分散电机(35HZ)、乳化电机(45HZ)搅拌30-40min;
(3)升温至60~65℃,滴加0.6kg过硫酸铵溶液(质量分数为0.2%),搅拌反应2.5h;
(4)向步骤2中混合液加入5.6kg去离子水、丙烯酸、剩余的烷基酚聚氧乙烯醚和剩余的乙酸乙烯酯,搅拌升温至72~75℃,反应0.5h;
(5)向步骤3中混合液中均匀滴加剩余的过硫酸铵溶液,加毕后保持搅拌20min,然后升温至90~95℃,保温反应0.5h;
(6)降温至50℃,加入碳酸氢钠溶液(30%),调pH值为6~7,加入邻苯二甲酸二丁酯,搅拌0.5h使其混合均匀后得到半成品B;
(7)向半成品B中加入乙烯-乙酸乙烯酯共聚物乳液,搅拌30-40min后,加入邻苯二甲酸二辛酯和由步骤1制得的溶液A,开始搅拌时加入正丁醇,搅拌60-70min后,加入碳酸氢钠溶液(30%)调节PH值6.5-7.5,加入氯丁胶,搅拌30min即制得产品。
以上对本发明的实施方式作了说明,但是本发明不限于上述实施方式,在所属技术领域普通技术人员所具备的知识范围内,还可以在不脱离本发明宗旨的前提下做出各种变化。
Claims (1)
1.一种用于粘贴标签用胶黏剂,其特征是:包括组份:乙烯-乙酸乙烯酯共聚物乳液、乙酸乙烯酯、丙烯酸、聚乙烯醇、烷基酚聚氧乙烯醚、邻苯二甲酸二辛酯、邻苯二甲酸二丁酯、过硫酸铵、硫酸铝、氯化铝、氧化锌、氯丁胶、正丁醇和去离子水,各组份按质量比是:100:35:23:8::7:7:6:1.5:0.09:0.03:0.01:11.5:0.02:65.6;
制作步骤是:
在带搅拌器的容器中将硫酸铝、氯化铝、氧化锌用总量2/3去离子水溶解,制得溶液A;
在装有搅拌器、回流冷凝器的高剪釜中,加入总量1/3的去离子水、聚乙烯醇,搅拌1h,使聚乙烯醇完全溶解,加入1/3的烷基酚聚氧乙烯醚、15%的乙酸乙烯酯,开启分散电机、乳化电机搅拌30-40min;
升温至60~65℃,滴加2/5的过硫酸铵溶液,搅拌反应2.5h;
向步骤2中混合液加入剩余的去离子水、丙烯酸、剩余的烷基酚聚氧乙烯醚和剩余的乙酸乙烯酯,搅拌升温至72~75℃,反应0.5h;
向步骤3中混合液中均匀滴加剩余的过硫酸铵溶液,加毕后保持搅拌20min,然后升温至90~95℃,保温反应0.5h;
降温至50℃,加入碳酸氢钠溶液,调pH值为6~7,加入邻苯二甲酸二丁酯,搅拌0.5h使其混合均匀后得到半成品B;
向半成品B中加入乙烯-乙酸乙烯酯共聚物乳液,搅拌30-40min后,加入邻苯二甲酸二辛酯和由步骤1制得的溶液A,开始搅拌时加入正丁醇,搅拌60-70min后,加入碳酸氢钠溶液调节PH值6.5-7.5,加入氯丁胶,搅拌30min即制得产品。