CN105057565A - 一种优质型砂及其制备方法 - Google Patents

一种优质型砂及其制备方法 Download PDF

Info

Publication number
CN105057565A
CN105057565A CN201510510188.9A CN201510510188A CN105057565A CN 105057565 A CN105057565 A CN 105057565A CN 201510510188 A CN201510510188 A CN 201510510188A CN 105057565 A CN105057565 A CN 105057565A
Authority
CN
China
Prior art keywords
parts
molding sand
sand
preparation
quality molding
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201510510188.9A
Other languages
English (en)
Inventor
孙爱琴
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Hefei Tenver Precision Casting Co Ltd
Original Assignee
Hefei Tenver Precision Casting Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Hefei Tenver Precision Casting Co Ltd filed Critical Hefei Tenver Precision Casting Co Ltd
Priority to CN201510510188.9A priority Critical patent/CN105057565A/zh
Publication of CN105057565A publication Critical patent/CN105057565A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种优质型砂及其制备方法,型砂由如下重量份的物质制成:180~200宝珠砂、20~30份镁橄榄石、5~10份黑刚玉、40~50份膨润土、8~10份双飞粉、1~2份煤粉、2~4份桐油、3~4份磷酸盐、2~3份六偏磷酸钠、4~6份羟丙基甲基纤维素。本发明型砂具有良好的透气性、强度和耐热性,可塑性和退让性也较好,制出的铸件表面光滑有亮度,降低了缩孔、气泡和变形的现象,成品率较高,且制作工艺简单,可降低生产污染。

Description

一种优质型砂及其制备方法
技术领域
本发明属于铸造领域,尤其涉及一种优质型砂及其制备方法。
背景技术
型砂是在铸造中用来造型的材料。型砂一般由铸造用原砂、型砂粘结剂和辅加物等造型材料按一定的比例混合而成,也可用天然含粘土的硅砂,通常的铸铝用的型砂配方中型砂粒径太大或太小,型砂料径太大,虽然透气性较好,但是铝砂件表面比较粗糙,光洁度不好,型砂料径太小,导致砂型透气性不好,铝铸件有气孔产生。
型砂在铸造生产中的作用极为重要,因型砂的质量不好而造成的铸件废品约占铸件总废品的30~50%,通常对型砂的要求有强度和热稳定性、流动性、可塑性、透气性和溃散性,即在铸件凝固后型砂是否容易破坏,是否容易从铸件上清除的性能。
随着铸造领域的迅速发展,人们对铸件的性能要求更高,从而要求型砂拥有更好的性能。
发明内容
本发明旨在提供一种优质型砂及其制备方法,本型砂不仅具有良好的性能,且制备方法简单合理,可降低生产污染。
本发明通过如下技术方案来实现:
一种优质型砂,由如下重量份的物质制成:
180~200宝珠砂、20~30份镁橄榄石、5~10份黑刚玉、40~50份膨润土、8~10份双飞粉、1~2份煤粉、2~4份桐油、3~4份磷酸盐、2~3份六偏磷酸钠、4~6份羟丙基甲基纤维素。
一种优质型砂的制备方法,包括如下步骤:
(1)将180~200宝珠砂、20~30份镁橄榄石、5~10份黑刚玉混合后放于13~15%的乙酸溶液浸泡4~5h后用去离子水洗涤,再用13~15%的氢氧化钠溶液浸泡4~5h后,并用去离子水洗涤至中性,然后将其烘干粉碎得粉碎砂粒备用;
(2)将粉碎砂粒同8~10份水混合后,再将40~50份膨润土、8~10份双飞粉和1~2份煤粉加入其中混合均匀得混合物备用;
(3)将3~4份磷酸盐、2~3份六偏磷酸钠、4~6份羟丙基甲基纤维素混合研磨均匀后,再同2~4份桐油加入到混合物中,配水湿混15~20min即可。
进一步的,步骤(1)所述粉碎砂粒可100%过200目筛,95%以上过300目筛,90%以上过400目筛。
进一步的,步骤(3)所述配水湿混后的成品含水量为4~6%。
本发明具有如下有益效果:
(1)首先对主体砂进行了去杂质处理,提高了其表面吸附能力和相对接触面积,其中,宝珠砂的砂粒为球形,流动性和透气性好,表面光滑结构致密,使得粘结剂可均匀覆盖,具有耐火度高、易溃散、稳定性好的特点;镁橄榄石具有较高的耐火度和抗金属氧化侵蚀能力,能有效的防止铸件产生化学粘砂;黑刚玉具有硬度适中、韧性高、耐高温、热态性能稳定的特点;三者构成的型砂的主要成分,使得型砂本体具有较好的可塑性、耐热性和稳定性。
(2)先将砂体表面附着水后,再加入粉状膨润土、双飞粉和煤粉,因为水已分散,没有较大的水滴,加入粘土后只能形成大量较小的粘土球,不仅可以消除干混时产生大量粉尘污染的现象,并且可降低混合所需能量,进一步缩短了混碾时间。
(3)添加的煤粉、磷酸盐、六偏磷酸钠和羟丙基甲基纤维素进一步提高了型砂的透气性、溃散性、防粘性、强度和耐热性。
(4)综上,本型砂具有良好的透气性、强度和耐热性,可塑性和退让性也较好,制出的铸件表面光滑有亮度,降低了缩孔、气泡和变形的现象,成品率可提高12~16%,且制作工艺简单易行,可降低生产污染。
具体实施方式
一种优质型砂,由如下重量份的物质制成:
200宝珠砂、25份镁橄榄石、8份黑刚玉、40份膨润土、10份双飞粉、2份煤粉、2份桐油、3份磷酸盐、2份六偏磷酸钠、5份羟丙基甲基纤维素。
一种优质型砂的制备方法,包括如下步骤:
(1)将200宝珠砂、25份镁橄榄石、8份黑刚玉混合后放于15%的乙酸溶液浸泡4h后用去离子水洗涤,再用13%的氢氧化钠溶液浸泡5h后,并用去离子水洗涤至中性,然后将其烘干粉碎得粉碎砂粒备用;
(2)将粉碎砂粒同9份水混合后,再将40份膨润土、10份双飞粉、2份煤粉加入其中混合均匀得混合物备用;
(3)将3份磷酸盐、2份六偏磷酸钠、5份羟丙基甲基纤维素混合研磨均匀后,再同2份桐油加入到混合物中,配水湿混20min即可。
进一步的,步骤(1)所述粉碎砂粒可100%过200目筛,95%以上过300目筛,90%以上过400目筛。
进一步的,步骤(3)所述配水湿混后的成品含水量为4~6%。
本发明型砂所测得的工艺性能参数如下:
湿压强度:0.115Mpa,透气率:97%,热湿拉强度:440Kpa,破碎指数:80%,抗弯强度:0.23MPa。
用本型砂做铸钢产品试验可发现铸件良率提高了14%。

Claims (4)

1.一种优质型砂,其特征在于,由如下重量份的物质制成:
180~200宝珠砂、20~30份镁橄榄石、5~10份黑刚玉、40~50份膨润土、8~10份双飞粉、1~2份煤粉、2~4份桐油、3~4份磷酸盐、2~3份六偏磷酸钠、4~6份羟丙基甲基纤维素。
2.一种优质型砂的制备方法,其特征在于,包括如下步骤:
(1)将180~200宝珠砂、20~30份镁橄榄石、5~10份黑刚玉混合后放于13~15%的乙酸溶液浸泡4~5h后用去离子水洗涤,再用13~15%的氢氧化钠溶液浸泡4~5h后,并用去离子水洗涤至中性,然后将其烘干粉碎得粉碎砂粒备用;
(2)将粉碎砂粒同8~10份水混合后,再将40~50份膨润土、8~10份双飞粉和1~2份煤粉加入其中混合均匀得混合物备用;
(3)将3~4份磷酸盐、2~3份六偏磷酸钠、4~6份羟丙基甲基纤维素混合研磨均匀后,再同2~4份桐油加入到混合物中,配水湿混15~20min即可。
3.根据权利要求2所述的一种优质型砂的制备方法,其特征在于,步骤(1)所述粉碎砂粒可100%过200目筛,95%以上过300目筛,90%以上过400目筛。
4.根据权利要求2所述的一种优质型砂及其制备方法,其特征在于,步骤(3)所述配水湿混后的成品含水量为4~6%。
CN201510510188.9A 2015-08-19 2015-08-19 一种优质型砂及其制备方法 Pending CN105057565A (zh)