CN104386952A - 高强度建筑隔热板制备方法 - Google Patents

高强度建筑隔热板制备方法 Download PDF

Info

Publication number
CN104386952A
CN104386952A CN201410525439.6A CN201410525439A CN104386952A CN 104386952 A CN104386952 A CN 104386952A CN 201410525439 A CN201410525439 A CN 201410525439A CN 104386952 A CN104386952 A CN 104386952A
Authority
CN
China
Prior art keywords
parts
dry
preparation
magnetic separation
water
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201410525439.6A
Other languages
English (en)
Other versions
CN104386952B (zh
Inventor
陈万国
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Luo Ying
Original Assignee
HEFEI XIANGRONG ENVIRONMENTAL PROTECTION TECHNOLOGY Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by HEFEI XIANGRONG ENVIRONMENTAL PROTECTION TECHNOLOGY Co Ltd filed Critical HEFEI XIANGRONG ENVIRONMENTAL PROTECTION TECHNOLOGY Co Ltd
Priority to CN201410525439.6A priority Critical patent/CN104386952B/zh
Publication of CN104386952A publication Critical patent/CN104386952A/zh
Application granted granted Critical
Publication of CN104386952B publication Critical patent/CN104386952B/zh
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种高强度建筑隔热板制备方法,该方法包括有以下步骤:1)、处理12-15份粉煤灰,通过磁选机磁选较低磁场强度的粉煤灰,然后用超细磨将磁选后的粉煤灰磨到1200目;2)、磁选后的粉煤灰与10-12份炉灰、6-8份磷石膏、12-14份火山岩纤维、28-30份水、5-7份羟乙基纤维素混合制成抗裂浆料,本发明的水淬渣用量大、节能环保,缓解水淬渣堆存处理带来的环境污染问题,同时为空心砖提供了新的原料。

Description

高强度建筑隔热板制备方法
 
技术领域
本发明涉及新型建材领域,具体属于一种高强度建筑隔热板制备方法。
 
背景技术
水淬渣是玻璃材质的玻璃、家具用品等等破碎后的产物,每年我国产生大量的水淬渣,这些水淬渣需要占用大量的堆放场地,且无法分解,回收利用成本很高。 
  长期以来,水淬渣的综合利用一直是个世界性难题,尽管国内外对水淬渣的综合利用进行了大量的研究,但是由于技术上和经济上的种种原因,大多数未付诸工业实现。
综合所述,用水淬渣为辅助原料生产水泥、墙体砖、道路材料已有报道,以水淬渣作为主要原料用于加气砌块的生产还未见报道。
 
发明内容
本发明的目的在于提供一种高强度建筑隔热板制备方法,水淬渣用量大、节能环保,缓解水淬渣堆存处理带来的环境污染问题,同时为空心砖提供了新的原料来源。
本发明的技术方案如下:
一种高强度建筑隔热板制备方法,该方法包括有以下步骤:
1)、处理12-15份粉煤灰
通过磁选机磁选较低磁场强度的粉煤灰,然后用超细磨将磁选后的粉煤灰磨到1200目;磁选后的粉煤灰与10-12份炉灰、6-8份磷石膏、12-14份火山岩纤维、28-30份水、5-7份羟乙基纤维素混合制成抗裂浆料,备用;
2)、水淬渣进行进行细磨后,取15-25份的水淬渣、24-27份水泥、3-5份稳泡剂、6-8份粘接剂、4.5-6.5份聚苯乙烯泡沫塑料、40-50份水混合,制得保温浆料;
3)、将保温浆料与抗裂浆料混合后注入到成型模具内压制形成生坯,压强为60-80Mpa;
4)、进行烘干,烘干分为低温区和高温区,首先进入低温区进行烘干,烘干温度为40-50℃,烘干时间16-20分钟;再进入高温区进行烘干,烘干温度为200-400℃,烘干时间20-40分钟,再进行低温区进行烘干,烘干温度为60-80℃,烘干时间6-10分钟。
所述保温浆料与抗裂浆料混合后注入到成型模具内压制形成生坯,压强为70Mpa。
本发明与现有技术相比具有如下优点:
与其他建筑材料相比,本发明所用水淬渣无需经过脱水、干燥处理即可直接使用,水淬渣用量大,均超过50%。
与其他建筑砌块相比,本发明生产的加气砌块容重轻,强度高,特别适用于高层建筑的承重墙或内墙隔断用。
与加气砌块相比,本发明的主要原料为水淬渣,有利于解决水淬渣堆存处理而带来的环境污染问题。
总之,本发明结合我国水淬渣量大、利用率低的实际情况,充分利用了各种物料的组成结构和化学特性,形成了以硅铝酸钙、水化硅酸钙等为主体的矿物结构,其产品性能符合建筑用承重和非承重墙体材料质量要求。砌块主要原材料为水淬渣,使用量大,有利于解决水淬渣堆存处理而带来的环境污染问题,为水淬渣的资源化利用开辟了一条新的利用途径。
 
具体实施方式
一种高强度建筑隔热板制备方法,该方法包括有以下步骤:
1)、处理12-15份粉煤灰
通过磁选机磁选较低磁场强度的粉煤灰,然后用超细磨将磁选后的粉煤灰磨到1200目;磁选后的粉煤灰与10-12份炉灰、6-8份磷石膏、12-14份火山岩纤维、28-30份水、5-7份羟乙基纤维素混合制成抗裂浆料,备用;
2)、水淬渣进行进行细磨后,取15-25份的水淬渣、24-27份水泥、3-5份稳泡剂、6-8份粘接剂、4.5-6.5份聚苯乙烯泡沫塑料、40-50份水混合,制得保温浆料;
3)、将保温浆料与抗裂浆料混合后注入到成型模具内压制形成生坯,压强为60-80Mpa;
4)、进行烘干,烘干分为低温区和高温区,首先进入低温区进行烘干,烘干温度为40-50℃,烘干时间16-20分钟;再进入高温区进行烘干,烘干温度为200-400℃,烘干时间20-40分钟,再进行低温区进行烘干,烘干温度为70℃,烘干时间6-10分钟。

Claims (2)

1.一种高强度建筑隔热板制备方法,其特征在于,该方法包括有以下步骤:
1)、处理12-15份粉煤灰
通过磁选机磁选较低磁场强度的粉煤灰,然后用超细磨将磁选后的粉煤灰磨到1200目;磁选后的粉煤灰与10-12份炉灰、6-8份磷石膏、12-14份火山岩纤维、28-30份水、5-7份羟乙基纤维素混合制成抗裂浆料,备用;
2)、水淬渣进行进行细磨后,取15-25份的水淬渣、24-27份水泥、3-5份稳泡剂、6-8份粘接剂、4.5-6.5份聚苯乙烯泡沫塑料、40-50份水混合,制得保温浆料;
3)、将保温浆料与抗裂浆料混合后注入到成型模具内压制形成生坯,压强为60-80Mpa;
4)、进行烘干,烘干分为低温区和高温区,首先进入低温区进行烘干,烘干温度为40-50℃,烘干时间16-20分钟;再进入高温区进行烘干,烘干温度为200-400℃,烘干时间20-40分钟,再进行低温区进行烘干,烘干温度为60-80℃,烘干时间6-10分钟。
2.根据权利要求1所述的高强度建筑隔热板制备方法,其特征在于,所述保温浆料与抗裂浆料混合后注入到成型模具内压制形成生坯,压强为70Mpa。
CN201410525439.6A 2014-10-09 2014-10-09 高强度建筑隔热板制备方法 Expired - Fee Related CN104386952B (zh)