CN103817889A - 注塑模具冷却装置 - Google Patents
注塑模具冷却装置 Download PDFInfo
- Publication number
- CN103817889A CN103817889A CN201210473235.3A CN201210473235A CN103817889A CN 103817889 A CN103817889 A CN 103817889A CN 201210473235 A CN201210473235 A CN 201210473235A CN 103817889 A CN103817889 A CN 103817889A
- Authority
- CN
- China
- Prior art keywords
- cooling water
- mold
- cooling
- water pipe
- injection mold
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了一种注塑模具冷却装置,包括模板和设于模板中间的模芯,所述模板的两侧分别设有进水管接口和出水管接口,所述模芯内设有螺旋状的冷却水管,所述冷却水管通过第一管道连接进水管接口,冷却水管通过第二管道连接出水管接口,本发明在模芯的内部设置螺旋状的冷却水管,这样冷却水顺着螺旋状的冷却水管逐一上去,冷却面积大,能够吸走大量的热量,而且冷却均匀,模芯内部的稳定性提高,有效的提高了模具的使用寿命,增加了注塑产品的质量。
Description
技术领域
本发明涉及一种模具辅助装置,特别涉及一种注塑模具冷却装置。
背景技术
模具在注塑过程中由于高温塑胶的热量传递,如果冷却不够充分会导致模具温度不稳定,导致产品尺寸不问题,普通的注塑机上会在模具的上方安装一个喷水冷却水管,但这样的装置,水只是从模具表面流过,没有办法真正起到模具模芯的冷却,而且模芯的冷却面积较小,无法带走足够的热量,这样就无法保持模芯的温度稳定,进而导致产品尺寸不稳定,无法进行正常生产。
发明内容
为了克服上述缺陷,本发明提供了一种能稳定控制模具温度,保证产品尺寸稳定的模具模芯冷却装置。
本发明为了解决其技术问题所采用的技术方案是:一种注塑模具冷却装置,包括模板和设于模板中间的模芯,所述模板的两侧分别设有进水管接口和出水管接口,所述模芯内设有螺旋状的冷却水管,所述冷却水管通过第一管道连接进水管接口,冷却水管通过第二管道连接出水管接口。
作为本发明的进一步改进,所述冷却水管的螺距小于冷却水管的横截面直径。
本发明的有益效果是:本发明在模芯的内部设置螺旋状的冷却水管,这样冷却水顺着螺旋状的冷却水管逐一上去,冷却面积大,能够吸走大量的热量,而且冷却均匀,模芯内部的稳定性提高,有效的提高了模具的使用寿命,增加了注塑产品的质量。
附图说明
图1为本发明结构示意图。
具体实施方式
为了加深对本发明的理解,下面将结合实施例和附图对本发明作进一步详述,该实施例仅用于解释本发明,并不构成对本发明保护范围的限定。图1出示了本发明一种注塑模具冷却装置的一种实施方式,包括模板1和设于模板中间的模芯2,所述模板1的两侧分别设有进水管接口3和出水管接口4,所述模芯2内设有螺旋状的冷却水管5,所述冷却水管5通过第一管道6连接进水管接口3,冷却水管5通过第二管道7连接出水管接口4,所述冷却水管5的螺距小于冷却水管的横截面直径,由于水路在模芯2的冷却水管5运行时是均匀向上的,所以模芯内的温度也会比较均匀,同时冷却面积较大能够带走大量的热量,能最大程度保持模芯的温度稳定。
Claims (2)
1.一种注塑模具冷却装置,包括模板(1)和设于模板中间的模芯(2),其特征在于:所述模板(1)的两侧分别设有进水管接口(3)和出水管接口(4),所述模芯(2)内设有螺旋状的冷却水管(5),所述冷却水管(5)通过第一管道(6)连接进水管接口(3),冷却水管(5)通过第二管道(7)连接出水管接口(4)。
2.根据权利要求1所述的注塑模具冷却装置,其特征在于:所述冷却水管(5)的螺距小于冷却水管的横截面直径。