CN103669046A - 涤棉交织物去毛染色同步法工艺 - Google Patents

涤棉交织物去毛染色同步法工艺 Download PDF

Info

Publication number
CN103669046A
CN103669046A CN201310609990.4A CN201310609990A CN103669046A CN 103669046 A CN103669046 A CN 103669046A CN 201310609990 A CN201310609990 A CN 201310609990A CN 103669046 A CN103669046 A CN 103669046A
Authority
CN
China
Prior art keywords
dyeing
dehairing
synchronous
polyester
depilitant
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201310609990.4A
Other languages
English (en)
Other versions
CN103669046B (zh
Inventor
徐杏地
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Zhejiang Yuexin Technology Co ltd
Original Assignee
Zhejiang Orient Huaqiang Textile Dyeing & Printing Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Zhejiang Orient Huaqiang Textile Dyeing & Printing Co Ltd filed Critical Zhejiang Orient Huaqiang Textile Dyeing & Printing Co Ltd
Priority to CN201310609990.4A priority Critical patent/CN103669046B/zh
Publication of CN103669046A publication Critical patent/CN103669046A/zh
Application granted granted Critical
Publication of CN103669046B publication Critical patent/CN103669046B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开一种涤棉交织物去毛染色同步法工艺,属于涤棉交织物去毛、染色工艺的技术领域,包括如下步骤:将坯布置入机缸内→调pH值至6-7→加染料→升温至55℃时,加入中性去毛剂,保温40分钟→取毛样核对→加入助剂→以每分钟升1-2℃加温至120-130℃,保温30-40分钟→以每分钟降1-2℃降温至80℃,对颜色样→进水降温至50℃,排水→进水水洗→出布→脱水→开幅→水洗→成品定型。本发明涤棉交织物去毛染色同步法工艺,能源消耗小、生产成本低、产量高、次品率低,且成品挺括、光泽度好。

Description

涤棉交织物去毛染色同步法工艺
技术领域
本发明公开一种涤棉交织物去毛染色同步法工艺,属于涤棉交织物去毛、染色工艺的技术领域。
背景技术
目前,涤棉交织物都是采用先进行去毛,再进行染色的分步工艺,这种工艺时间长、次品率高、能源消耗大,从而导致生产成本高、产量低的问题,同时还存在成品不挺括、光泽度差的问题。
发明内容
本发明的目的是提供一种低成本、高产量、低次品率的涤棉交织物去毛染色同步法工艺。
为达到上述目的,本发明所采用的技术方案为:
一种涤棉交织物去毛染色同步法工艺,包括如下步骤:将坯布置入机缸内→调pH值至6-7→加染料→升温至55℃时,加入中性去毛剂,保温40分钟→取毛样核对→加入助剂→以每分钟升1-2℃加温至120-130℃,保温30-40分钟→以每分钟降1-2℃降温至80℃,对颜色样→进水降温至50℃,排水→进水水洗→出布→脱水→开幅→水洗→成品定型。
所述中性去毛剂的加入量为坯布重量的0.8-1.2%(相当于100公斤坯布要加0.8-1.2公斤的中性去毛剂)。
所述助剂为元明粉和分散匀染剂,其中,元明粉的浓度为10-30克/升(以染缸水位为基础计算,如:水位达到3吨位置时,加入元明粉的量为30-90千克),分散匀染剂的浓度为1.5-2.0克/升(以染缸水位为基础计算,如:水位达到3吨位置时,加入分散匀染剂的量为4.5-6千克)。
    本发明涤棉交织物去毛染色同步法工艺,能源消耗小、生产成本低、产量高、次品率低,且成品挺括、光泽度好。
具体实施方式
    实施例1
    一种涤棉交织物去毛染色同步法工艺,包括如下步骤:将坯布置入机缸内→调pH值至6→加染料→升温至55℃时,加入中性去毛剂,保温40分钟→取毛样核对→加入助剂→以每分钟升1℃加温至120℃,保温40分钟→以每分钟降1℃降温至80℃,对颜色样→进水降温至50℃,排水→进水水洗→出布→脱水→开幅→水洗→成品定型。
    上述中性去毛剂的加入量为坯布重量的1.0%。
上述助剂为元明粉和分散匀染剂,其中,元明粉的浓度为10克/升(以染缸水位为基础计算,如:水位达到3吨位置时,加入元明粉的量为30千克),分散匀染剂的浓度为1.5克/升(以染缸水位为基础计算,如:水位达到3吨位置时,加入分散匀染剂的量为4.5千克)。
    本实施例中,中性去毛剂为中性抛光酶,其厂商为浙江宏达化学制品有限公司,规格为400L。
    实施例2
    一种涤棉交织物去毛染色同步法工艺,包括如下步骤:将坯布置入机缸内→调pH值至7→加染料→升温至55℃时,加入中性去毛剂,保温40分钟→取毛样核对→加入助剂→以每分钟升2℃加温至130℃,保温30分钟→以每分钟降2℃降温至80℃,对颜色样→进水降温至50℃,排水→进水水洗→出布→脱水→开幅→水洗→成品定型。
    上述中性去毛剂的加入量为坯布重量的1.2%。
上述助剂为元明粉和分散匀染剂,其中,元明粉的浓度为30克/升(以染缸水位为基础计算,如:水位达到3吨位置时,加入元明粉的量为90千克),分散匀染剂的浓度为2.0克/升(以染缸水位为基础计算,如:水位达到3吨位置时,加入分散匀染剂的量为6千克)。
    本实施例中,中性去毛剂为中性抛光酶,其厂商为浙江宏达化学制品有限公司,规格为400L。
实施例3
    一种涤棉交织物去毛染色同步法工艺,包括如下步骤:将坯布置入机缸内→调pH值至6.5→加染料→升温至55℃时,加入中性去毛剂,保温40分钟→取毛样核对→加入助剂→以每分钟升1.5℃加温至125℃,保温35分钟→以每分钟降1.5℃降温至80℃,对颜色样→进水降温至50℃,排水→进水水洗→出布→脱水→开幅→水洗→成品定型。
    上述中性去毛剂的加入量为坯布重量的0.8%。
上述助剂为元明粉和分散匀染剂,其中,元明粉的浓度为20克/升(以染缸水位为基础计算,如:水位达到3吨位置时,加入元明粉的量为60千克),分散匀染剂的浓度为2.0克/升(以染缸水位为基础计算,如:水位达到3吨位置时,加入分散匀染剂的量为6千克)。
本实施例中,中性去毛剂为中性抛光酶,其厂商为浙江宏达化学制品有限公司,规格为400L。
上述实施例仅用于解释说明本发明的发明构思,而非对本发明权利保护的限定,凡利用此构思对本发明进行非实质性的改动,均应落入本发明的保护范围。

Claims (3)

1.一种涤棉交织物去毛染色同步法工艺,其特征在于包括如下步骤:将坯布置入机缸内→调pH值至6-7→加染料→升温至55℃时,加入中性去毛剂,保温40分钟→取毛样核对→加入助剂→以每分钟升1-2℃加温至120-130℃,保温30-40分钟→以每分钟降1-2℃降温至80℃,对颜色样→进水降温至50℃,排水→进水水洗→出布→脱水→开幅→水洗→成品定型。
2.如权利要求1所述的涤棉交织物去毛染色同步法工艺,其特征在于:所述中性去毛剂的加入量为坯布重量的0.8-1.2%。
3.如权利要求1所述的涤棉交织物去毛染色同步法工艺,其特征在于:所述助剂为元明粉和分散匀染剂,其中,元明粉的浓度为10-30克/升,分散匀染剂的浓度为1.5-2.0克/升。
CN201310609990.4A 2013-11-27 2013-11-27 涤棉交织物去毛染色同步法工艺 Active CN103669046B (zh)