CN103642086B - 一种氧化普鲁兰多糖-醇溶蛋白改性天然乳胶的方法 - Google Patents

一种氧化普鲁兰多糖-醇溶蛋白改性天然乳胶的方法 Download PDF

Info

Publication number
CN103642086B
CN103642086B CN201310546258.7A CN201310546258A CN103642086B CN 103642086 B CN103642086 B CN 103642086B CN 201310546258 A CN201310546258 A CN 201310546258A CN 103642086 B CN103642086 B CN 103642086B
Authority
CN
China
Prior art keywords
pullulan oxide
molten
pullulan
oxide
preparation
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201310546258.7A
Other languages
English (en)
Other versions
CN103642086A (zh
Inventor
苏建丽
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Foshan Shunfengsheng Latex Products Co ltd
Original Assignee
Qingdao Wenchuang Technology Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Qingdao Wenchuang Technology Co Ltd filed Critical Qingdao Wenchuang Technology Co Ltd
Priority to CN201310546258.7A priority Critical patent/CN103642086B/zh
Publication of CN103642086A publication Critical patent/CN103642086A/zh
Application granted granted Critical
Publication of CN103642086B publication Critical patent/CN103642086B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

一种氧化普鲁兰多糖-醇溶蛋白改性天然乳胶的方法,步骤为:(1)氧化普鲁兰多糖-醇溶蛋白蛋白复合物的制备:将氧化普鲁兰多糖加水溶解,向溶液中加入醇溶蛋白,混合均匀后冷冻干燥,然后将冻干物置于30℃下加热30min,得到氧化普鲁兰多糖-醇溶蛋白共价复合物备用;(2)改性乳胶膜的制备:配制氧化普鲁兰多糖-醇溶蛋白共价复合物水溶液,与天然乳胶液混合搅拌均匀,进行乳胶膜硫化处理,待乳液稳定无气泡后,于70℃下浇注成膜,得到改性乳胶膜。本发明制备的天然乳胶具备耐老化性、抗过敏性。

Description

一种氧化普鲁兰多糖-醇溶蛋白改性天然乳胶的方法
技术领域
本发明涉及一种天然乳胶的改性方法,特别涉及一种氧化普鲁兰多糖-醇溶蛋白改性天然乳胶的方法,属天然高分子材料加工领域。
技术背景
天然乳胶是一种经生物合成、可再生的自然资源,因优异的综合性能而被广泛应用于医用导管、医用手套及避孕套等产品中。但是天然乳胶因含不饱和双键,使其耐油性、耐老化性较差,其中的微量水溶性蛋白引起人体过敏反应。
发明内容
本发明的目的是提供一种制备耐老化性、抗过敏性的天然乳胶的改性方法。
为实现以上目的,本发明的一种氧化普鲁兰多糖-醇溶蛋白改性天然乳胶的方法,步骤为:
(1)氧化普鲁兰多糖-醇溶蛋白复合物的制备:将氧化普鲁兰多糖加水溶解,向溶液中加入醇溶蛋白,混合均匀后冷冻干燥,然后将冻干物置于30℃下加热30min,得到氧化普鲁兰多糖-醇溶蛋白共价复合物备用;
(2)改性乳胶膜的制备:配制氧化普鲁兰多糖-醇溶蛋白共价复合物水溶液,与天然乳胶液混合搅拌均匀,进行乳胶膜硫化处理,待乳液稳定无气泡后,于70℃下浇注成膜,得到改性乳胶膜。
优选的,醇溶蛋白为玉米醇溶蛋白或小麦醇溶蛋白;氧化普鲁兰多糖与醇溶蛋白的质量比为10:1-20:1;氧化普鲁兰多糖-醇溶蛋白共价复合物的加入量为天然乳胶质量的1%-3%。
本发明产生的有益效果为,普鲁兰多糖具有良好的生物相容性及生物可降解性,与人体皮肤具有很好的亲和性。醇溶蛋白具有良好的生物相容性、抗氧化性。利用氧化的普鲁兰多糖与醇溶蛋白分子中的多种活性基团对天然乳胶中的蛋白质交联变性,降低水溶性蛋白溢出量,赋予改性乳胶膜抗过敏性。
实施例
实施例1:
一种氧化普鲁兰多糖-醇溶蛋白改性天然乳胶的方法,步骤为:
(1)氧化普鲁兰多糖-醇溶蛋白蛋白复合物的制备:将20份氧化普鲁兰多糖加水溶解,向溶液中加入2份小麦醇溶蛋白,混合均匀后冷冻干燥,然后将冻干物置于30℃下加热30min,得到氧化普鲁兰多糖-醇溶蛋白共价复合物备用;
(2)改性乳胶膜的制备:将上述氧化普鲁兰多糖-醇溶蛋白共价复合物配制为水溶液,与2000份天然乳胶液混合搅拌均匀,进行乳胶膜硫化处理,待乳液稳定无气泡后,于70℃下浇注成膜,得到改性乳胶膜。以上均为重量份。
实施例2:
一种氧化普鲁兰多糖-醇溶蛋白改性天然乳胶的方法,步骤为:
(1)氧化普鲁兰多糖-醇溶蛋白蛋白复合物的制备:将20份氧化普鲁兰多糖加水溶解,向溶液中加入2份玉米醇溶蛋白,混合均匀后冷冻干燥,然后将冻干物置于30℃下加热30min,得到氧化普鲁兰多糖-醇溶蛋白共价复合物备用;
(2)改性乳胶膜的制备:将上述氧化普鲁兰多糖-醇溶蛋白共价复合物配制为水溶液,与1500份天然乳胶液混合搅拌均匀,进行乳胶膜硫化处理,待乳液稳定无气泡后,于70℃下浇注成膜,得到改性乳胶膜。以上均为重量份。
实施例3:
一种氧化普鲁兰多糖-醇溶蛋白改性天然乳胶的方法,步骤为:
(1)氧化普鲁兰多糖-醇溶蛋白蛋白复合物的制备:将20份氧化普鲁兰多糖加水溶解,向溶液中加入1份玉米醇溶蛋白,混合均匀后冷冻干燥,然后将冻干物置于30℃下加热30min,得到氧化普鲁兰多糖-醇溶蛋白共价复合物备用;
(2)改性乳胶膜的制备:将上述氧化普鲁兰多糖-醇溶蛋白共价复合物配制为水溶液,与800份天然乳胶液混合搅拌均匀,进行乳胶膜硫化处理,待乳液稳定无气泡后,于70℃下浇注成膜,得到改性乳胶膜。以上均为重量份。

Claims (1)

1.一种氧化普鲁兰多糖-醇溶蛋白改性天然乳胶的方法,其特征在于:步骤为:
(1)氧化普鲁兰多糖-醇溶蛋白蛋白复合物的制备:将氧化普鲁兰多糖加水溶解,向溶液中加入醇溶蛋白,混合均匀后冷冻干燥,然后将冻干物置于30℃下加热30min,得到氧化普鲁兰多糖-醇溶蛋白共价复合物备用;
(2)改性乳胶膜的制备:配制氧化普鲁兰多糖-醇溶蛋白共价复合物水溶液,与天然乳胶液混合搅拌均匀,进行乳胶膜硫化处理,待乳液稳定无气泡后,于70℃下浇注成膜,得到改性乳胶膜;
上述醇溶蛋白为玉米醇溶蛋白或小麦醇溶蛋白;
上述氧化普鲁兰多糖与醇溶蛋白的质量比为10︰1-20︰1;
上述氧化普鲁兰多糖-醇溶蛋白共价复合物的加入量为天然乳胶质量的1%-3%。
CN201310546258.7A 2013-11-07 2013-11-07 一种氧化普鲁兰多糖-醇溶蛋白改性天然乳胶的方法 Active CN103642086B (zh)