CN103524954A - 一种含纤维橡胶密封圈 - Google Patents

一种含纤维橡胶密封圈 Download PDF

Info

Publication number
CN103524954A
CN103524954A CN201310430458.6A CN201310430458A CN103524954A CN 103524954 A CN103524954 A CN 103524954A CN 201310430458 A CN201310430458 A CN 201310430458A CN 103524954 A CN103524954 A CN 103524954A
Authority
CN
China
Prior art keywords
parts
add
fibre
raw material
fiber
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201310430458.6A
Other languages
English (en)
Other versions
CN103524954B (zh
Inventor
胡光荣
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Jiangmen City Pengjiang District Hetang Weirun Rubber Co ltd
Original Assignee
TONGLING XINCHUANG FLUID TECHNOLOGY Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by TONGLING XINCHUANG FLUID TECHNOLOGY Co Ltd filed Critical TONGLING XINCHUANG FLUID TECHNOLOGY Co Ltd
Priority to CN201310430458.6A priority Critical patent/CN103524954B/zh
Publication of CN103524954A publication Critical patent/CN103524954A/zh
Application granted granted Critical
Publication of CN103524954B publication Critical patent/CN103524954B/zh
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种含纤维橡胶密封圈,它是由下述重量份的原料组成的:氟橡胶2395-100、石英玻璃纤维10-12、矿棉纤维2-3、硫酸钡粉10-12、轻质碳酸钙10-20、膨润土10-12、PE蜡2-3、聚四氟乙烯纤维3-4、乙撑双硬脂酰胺1-2、苯二甲酸二丁酯3-4、二甲基二巯基乙酸异辛酯锡1-2、异丙基二油酸酰氧基(二辛基磷酸酰氧基)钛酸酯1-2、促进剂DM1-2、硫化剂DCBP0.8-1、改性粒子10-15,本发明生产的密封圈抗拉伸、抗撕裂、耐腐蚀、耐温变性强,加入的各种纤维进一步增强了该密封圈的物理性能,阻燃性等也有很大提高。

Description

一种含纤维橡胶密封圈
技术领域
本发明主要涉及一种密封圈,尤其涉及一种含纤维橡胶密封圈。
背景技术
氟弹性体是以其在优异的阻燃性、优异的气密性、耐高温、耐臭氧、耐气候、耐氧化、耐矿物油、耐燃料油、耐液压油、耐芳香族与许多有机溶剂和化学物的性能著称,用氟橡胶制成的密封圈应用广泛,性能优越。
发明内容
本发明目的就是提供一种含纤维橡胶密封圈。
本发明是通过以下技术方案实现的:
一种含纤维橡胶密封圈,它是由下述重量份的原料组成的:
氟橡胶2395-100、石英玻璃纤维10-12、矿棉纤维2-3、硫酸钡粉10-12、轻质碳酸钙10-20、膨润土10-12、PE蜡2-3、聚四氟乙烯纤维3-4、乙撑双硬脂酰胺1-2、苯二甲酸二丁酯3-4、二甲基二巯基乙酸异辛酯锡1-2、异丙基二油酸酰氧基(二辛基磷酸酰氧基)钛酸酯1-2、促进剂DM1-2、硫化剂DCBP0.8-1、改性粒子10-15;
所述的改性粒子是由下述重量份的原料组成的:
PVC树脂90-100、氮化铝10-15、饱和脂肪醇二羧酸酯2-3、γ-氨丙基三乙氧基硅烷1-2、十溴二苯乙烷1-2、氰尿酸铅0.1-0.2;
将上述PVC树脂封闭研磨,然后加入饱和脂肪醇二羧酸酯、氰尿酸铅,在100-120℃下共混搅拌10-12分钟,降低温度为50-60℃,加入氮化铝、γ-氨丙基三乙氧基硅烷,600-800转/分搅拌分散4-6分钟,加入剩余各原料,充分搅拌,加入双螺杆挤出机挤出造粒,得粒径为2-3μm。
一种含纤维橡胶密封圈的制备方法,包括以下步骤:
将上述石英玻璃纤维、矿棉纤维、聚四氟乙烯纤维混合,加入PE蜡,70-80℃下加热6-10分钟,加入乙撑双硬脂酰胺,充分搅拌后,冷却至常温,加入除了硫化剂DCBP、促进剂DM以外的剩余各原料,混炼,压制成型,加入剩余各原料,进行硫化处理,即得所述含纤维橡胶密封圈。
本发明的优点是:
本发明生产的密封圈抗拉伸、抗撕裂、耐腐蚀、耐温变性强,加入的各种纤维进一步增强了该密封圈的物理性能,阻燃性等也有很大提高。
具体实施方式
实施例1
一种含纤维橡胶密封圈,它是由下述重量份(公斤)的原料组成的:
氟橡胶23100、石英玻璃纤维12、矿棉纤维3、硫酸钡粉12、轻质碳酸钙20、膨润土12、PE蜡2、聚四氟乙烯纤维4、乙撑双硬脂酰胺1、苯二甲酸二丁酯3、二甲基二巯基乙酸异辛酯锡1、异丙基二油酸酰氧基(二辛基磷酸酰氧基)钛酸酯1、促进剂DM1、硫化剂DCBP0.8、改性粒子15;
所述的改性粒子是由下述重量份的原料组成的:
PVC树脂100、氮化铝15、饱和脂肪醇二羧酸酯3、γ-氨丙基三乙氧基硅烷1、十溴二苯乙烷1、氰尿酸铅0.2;
将上述PVC树脂封闭研磨,然后加入饱和脂肪醇二羧酸酯、氰尿酸铅,在120℃下共混搅拌12分钟,降低温度为60℃,加入氮化铝、γ-氨丙基三乙氧基硅烷,800转/分搅拌分散6分钟,加入剩余各原料,充分搅拌,加入双螺杆挤出机挤出造粒,得粒径为3μm。
一种含纤维橡胶密封圈的制备方法,包括以下步骤:
将上述石英玻璃纤维、矿棉纤维、聚四氟乙烯纤维混合,加入PE蜡,80℃下加热10分钟,加入乙撑双硬脂酰胺,充分搅拌后,冷却至常温,加入除了硫化剂DCBP、促进剂DM以外的剩余各原料,混炼,压制成型,加入剩余各原料,进行硫化处理,即得所述含纤维橡胶密封圈。
性能测试:
Figure BDA0000384163710000021

Claims (2)

1.一种含纤维橡胶密封圈,其特征在于它是由下述重量份的原料组成的:
氟橡胶23 95-100、石英玻璃纤维10-12、矿棉纤维2-3、硫酸钡粉10-12、轻质碳酸钙10-20、膨润土10-12、PE蜡2-3、聚四氟乙烯纤维3-4、乙撑双硬脂酰胺1-2、苯二甲酸二丁酯3-4、二甲基二巯基乙酸异辛酯锡1-2、异丙基二油酸酰氧基(二辛基磷酸酰氧基)钛酸酯1-2、促进剂DM1-2、硫化剂DCBP0.8-1、改性粒子10-15;
所述的改性粒子是由下述重量份的原料组成的:
PVC树脂90-100、氮化铝10-15、饱和脂肪醇二羧酸酯2-3、γ-氨丙基三乙氧基硅烷1-2、十溴二苯乙烷1-2、氰尿酸铅0.1-0.2;
将上述PVC树脂封闭研磨,然后加入饱和脂肪醇二羧酸酯、氰尿酸铅,在100-120℃下共混搅拌10-12分钟,降低温度为50-60℃,加入氮化铝、γ-氨丙基三乙氧基硅烷,600-800转/分搅拌分散4-6分钟,加入剩余各原料,充分搅拌,加入双螺杆挤出机挤出造粒,得粒径为2-3μm。
2.一种如权利要求1所述的含纤维橡胶密封圈的制备方法,其特征在于包括以下步骤:
将上述石英玻璃纤维、矿棉纤维、聚四氟乙烯纤维混合,加入PE蜡,70-80℃下加热6-10分钟,加入乙撑双硬脂酰胺,充分搅拌后,冷却至常温,加入除了硫化剂DCBP、促进剂DM以外的剩余各原料,混炼,压制成型,加入剩余各原料,进行硫化处理,即得所述含纤维橡胶密封圈。
CN201310430458.6A 2013-09-18 2013-09-18 一种含纤维橡胶密封圈 Expired - Fee Related CN103524954B (zh)